JP2008280597A5 - - Google Patents
Download PDFInfo
- Publication number
- JP2008280597A5 JP2008280597A5 JP2007127883A JP2007127883A JP2008280597A5 JP 2008280597 A5 JP2008280597 A5 JP 2008280597A5 JP 2007127883 A JP2007127883 A JP 2007127883A JP 2007127883 A JP2007127883 A JP 2007127883A JP 2008280597 A5 JP2008280597 A5 JP 2008280597A5
- Authority
- JP
- Japan
- Prior art keywords
- iridium
- alloy
- oxidation
- resistant
- iridium alloy
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Images
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP2007127883A JP5224720B2 (ja) | 2007-05-14 | 2007-05-14 | 耐酸化性イリジウム合金及びその製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP2007127883A JP5224720B2 (ja) | 2007-05-14 | 2007-05-14 | 耐酸化性イリジウム合金及びその製造方法 |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JP2008280597A JP2008280597A (ja) | 2008-11-20 |
| JP2008280597A5 true JP2008280597A5 (enExample) | 2010-07-01 |
| JP5224720B2 JP5224720B2 (ja) | 2013-07-03 |
Family
ID=40141666
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP2007127883A Expired - Fee Related JP5224720B2 (ja) | 2007-05-14 | 2007-05-14 | 耐酸化性イリジウム合金及びその製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JP5224720B2 (enExample) |
Families Citing this family (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP7620297B2 (ja) | 2018-05-22 | 2025-01-23 | 国立大学法人 名古屋工業大学 | 構造部材及びその製造方法 |
Family Cites Families (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP4255519B2 (ja) * | 1995-06-12 | 2009-04-15 | 株式会社デンソー | 内燃機関用スパークプラグ及びその製造方法 |
| JP4847814B2 (ja) * | 2006-07-25 | 2011-12-28 | 田中貴金属工業株式会社 | スパークプラグ用の貴金属合金チップ及びその製造方法 |
-
2007
- 2007-05-14 JP JP2007127883A patent/JP5224720B2/ja not_active Expired - Fee Related
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| EP2692703B1 (en) | Molten glass holding refractory, glass manufacturing apparatus using molten glass holding refractory and method for manufacturing glass using glass manufacturing apparatus | |
| CN1665960A (zh) | 高耐氧化部件 | |
| WO2011136294A1 (ja) | 温度センサ素子及びその製造方法、並びに、温度センサ | |
| JP3927574B2 (ja) | NiCoCrAl薄膜 | |
| CN1639388A (zh) | 具有良好耐高温氧化性的Ni合金耐热材料 | |
| EP2631324A1 (en) | Ni-based superalloy member having heat-resistant bond coat layer formed therein | |
| JP2010138418A (ja) | 白金イリジウム合金及びその製造方法 | |
| KR100611723B1 (ko) | 내고온 부식성, 내산화성이 우수한 내열성 티타늄합금재료 및 그 제조방법 | |
| CN108048839A (zh) | 一种钨铼热电偶高温抗氧化涂层及其应用 | |
| CN113322395B (zh) | 一种Pt-Ru-Ir合金火花塞电极材料及其制备方法和应用的火花塞 | |
| JP2012132099A (ja) | ニオブ基合金の耐熱材料 | |
| JP2007186788A (ja) | 拡散障壁コーティングおよびタービンエンジン部品 | |
| JP5105990B2 (ja) | 耐熱PtRh合金 | |
| WO2010084755A1 (ja) | スパークプラグ | |
| JP5618445B2 (ja) | 高耐久性Pt線 | |
| JP5224720B2 (ja) | 耐酸化性イリジウム合金及びその製造方法 | |
| JP5826182B2 (ja) | 改善された電極材料から製造されたスパークプラグ電極 | |
| JP2008280597A5 (enExample) | ||
| EP1542505A1 (en) | Metal based resistance heating element and method for preparation thereof | |
| RU2232206C1 (ru) | Способ получения защитного покрытия на сплавах | |
| JP5610299B2 (ja) | 耐酸化消耗性白金合金、耐酸化消耗性白金合金皮膜および耐酸化消耗性金属部材 | |
| JP2022060168A (ja) | 温度センサを接触させるための白金組成物のワイヤ | |
| JP2005048283A (ja) | 遮熱コーティング部材およびその製造方法 | |
| JP2004250788A (ja) | 皮膜形成方法 | |
| JP2005281032A (ja) | 焼結用グラファイトトレー |