JP2007131928A - 製鋼スラグのリサイクル方法 - Google Patents
製鋼スラグのリサイクル方法 Download PDFInfo
- Publication number
- JP2007131928A JP2007131928A JP2005327479A JP2005327479A JP2007131928A JP 2007131928 A JP2007131928 A JP 2007131928A JP 2005327479 A JP2005327479 A JP 2005327479A JP 2005327479 A JP2005327479 A JP 2005327479A JP 2007131928 A JP2007131928 A JP 2007131928A
- Authority
- JP
- Japan
- Prior art keywords
- slag
- steelmaking
- recycling
- reducing
- dephosphorization
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
【解決手段】製鋼工程で発生する燐酸化物を含むスラグを、製銑工程及び/又は製鋼工程にリサイクルする方法の改良である。その方法は、まず、前記スラグを磁力分離して磁着物を除去し、その後に非磁着物と還元性物質とを混合、加熱し、該加熱の際に、別途還元性ガスを非磁着物重量(トン)当たり3〜30リットル(標準状態)/minの流量で添加し、気化脱燐反応を促進して脱燐させてから前記製銑及び/又は製鋼工程にリサイクルするようにした。
【選択図】 図1
Description
(P2O5)+5C=P2(g)+5CO (2)
2Fe+P2(g)=2FeP (3)
製鋼スラグの製銑工程及び製鋼工程へのリサイクルは、スラグ中Fe分の回収、CaO分の回収、再利用が目的であるが、スラグ中に存在する鉄分中にはPが吸収され、高P濃度鉄が形成されており、製鋼で得たままでのスラグのリサイクルは量的に制限せねばならない。
ここでは、還元性ガスとしてプロパンガスを用いたが、H2ガスや他の炭化水素系ガス(CH4、C2H6等)でも同様の結果が得られた。また、ガス化して炭化水素ガスを発生する固体(プラスチック等)の添加でも同様であった。
2 磁力分離器
3 非磁着物
4 磁着物
5 耐熱性容器(容器)
6 カーボン・ルツボ
7 誘導コイル
8 真空ポンプ
9 炭化水素系ガス
10 ペレット
Claims (2)
- 製鋼工程で発生する燐酸化物を含むスラグを、製銑工程及び/又は製鋼工程にリサイクルして再使用するに際し、
まず、前記スラグを磁力分離して磁着物を除去し、その後に非磁着物と還元性物質とを混合、加熱し、該加熱の際に、別途還元性ガスを非磁着物重量(トン)当たり3〜30リットル(標準状態)/minの流量で添加し、気化脱燐反応を促進して脱燐させてから前記製銑及び/又は製鋼工程にリサイクルすることを特徴とする製鋼スラグのリサイクル方法。 - 前記加熱の際の反応容器内雰囲気圧力を0.005〜0.04MPaとすることを特徴とする請求項1の製鋼スラグのリサイクル方法。