JP2004526286A5 - - Google Patents

Download PDF

Info

Publication number
JP2004526286A5
JP2004526286A5 JP2002574138A JP2002574138A JP2004526286A5 JP 2004526286 A5 JP2004526286 A5 JP 2004526286A5 JP 2002574138 A JP2002574138 A JP 2002574138A JP 2002574138 A JP2002574138 A JP 2002574138A JP 2004526286 A5 JP2004526286 A5 JP 2004526286A5
Authority
JP
Japan
Prior art keywords
oxide
zinc
mixture
aqueous
paste
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP2002574138A
Other languages
English (en)
Japanese (ja)
Other versions
JP2004526286A (ja
Filing date
Publication date
Application filed filed Critical
Priority claimed from PCT/CA2002/000352 external-priority patent/WO2002075825A2/en
Publication of JP2004526286A publication Critical patent/JP2004526286A/ja
Publication of JP2004526286A5 publication Critical patent/JP2004526286A5/ja
Pending legal-status Critical Current

Links

JP2002574138A 2001-03-15 2002-03-15 アルカリ電池のための酸化亜鉛電極の製造方法 Pending JP2004526286A (ja)

Applications Claiming Priority (2)

Application Number Priority Date Filing Date Title
US27634401P 2001-03-15 2001-03-15
PCT/CA2002/000352 WO2002075825A2 (en) 2001-03-15 2002-03-15 Methods for production of zinc oxide electrodes for alkaline batteries

Publications (2)

Publication Number Publication Date
JP2004526286A JP2004526286A (ja) 2004-08-26
JP2004526286A5 true JP2004526286A5 (enExample) 2005-07-21

Family

ID=23056271

Family Applications (1)

Application Number Title Priority Date Filing Date
JP2002574138A Pending JP2004526286A (ja) 2001-03-15 2002-03-15 アルカリ電池のための酸化亜鉛電極の製造方法

Country Status (5)

Country Link
US (2) US7255720B2 (enExample)
EP (1) EP1371103A2 (enExample)
JP (1) JP2004526286A (enExample)
AU (1) AU2002242530A1 (enExample)
WO (1) WO2002075825A2 (enExample)

Families Citing this family (17)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US7829221B2 (en) * 2000-11-10 2010-11-09 Powergenix Systems, Inc. Cobalt containing positive electrode formulation for a nickel-zinc cell
US7118726B2 (en) 2002-12-13 2006-10-10 Clark Manufacturing, Llc Method for making oxide compounds
CN100521302C (zh) * 2003-08-18 2009-07-29 鲍尔热尼系统公司 制造镍锌电池的方法
US8586244B2 (en) * 2007-04-02 2013-11-19 Eveready Battery Co., Inc. Alkaline electrochemical cell having a negative electrode with solid zinc oxide and a surfactant
US8048566B2 (en) * 2008-02-07 2011-11-01 Powergenix Systems, Inc. Nickel hydroxide electrode for rechargeable batteries
US8043748B2 (en) * 2008-02-07 2011-10-25 Powergenix Systems, Inc. Pasted nickel hydroxide electrode for rechargeable nickel-zinc batteries
CA2720078A1 (en) 2008-04-02 2009-10-08 Powergenix Systems, Inc. Cylindrical nickel-zinc cell with negative can
CN102210052A (zh) * 2008-12-12 2011-10-05 松下电器产业株式会社 碱性干电池
KR101822666B1 (ko) * 2009-08-07 2018-03-08 파워지닉스 시스템즈, 인코포레이티드 탄소 섬유 아연 음극
CN103748710B (zh) 2011-08-23 2018-11-27 株式会社日本触媒 负极合剂或凝胶电解质以及使用了该负极合剂或凝胶电解质的电池
US9337483B2 (en) 2013-01-14 2016-05-10 Powergenix Systems, Inc. Pasted nickel hydroxide electrode and additives for rechargeable alkaline batteries
JP6368097B2 (ja) * 2013-02-01 2018-08-01 株式会社日本触媒 亜鉛負極及び電池
WO2014119663A1 (ja) 2013-02-01 2014-08-07 株式会社日本触媒 電極前駆体、電極、及び、電池
JP6967080B2 (ja) * 2017-11-08 2021-11-17 シャープ株式会社 電池用負極、電池および電池の製造方法
CN112824323A (zh) * 2019-11-21 2021-05-21 中国科学院大连化学物理研究所 一种铟掺杂氧化锌复合还原氧化石墨烯材料及制备和应用
CN111082008B (zh) * 2019-12-14 2021-07-23 莒南凯佳化工有限公司 一种电化学储能用纳米纤维素/氧化锌复合物制备方法
CN115241405B (zh) * 2022-07-12 2025-06-06 山东合泰新能源有限公司 一种锌镍电池负极材料及制备方法和负极

Family Cites Families (23)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS4813775B1 (enExample) * 1970-04-17 1973-04-28
US3645793A (en) * 1970-06-01 1972-02-29 Esb Inc Method for producing porous metal battery electrode structure
JPS549696B2 (enExample) * 1973-01-31 1979-04-26
JPS5461B2 (enExample) * 1973-11-21 1979-01-05
US4118551A (en) * 1977-10-31 1978-10-03 Yardney Electric Corporation Mercury-free zinc electrode
US4224391A (en) * 1979-09-14 1980-09-23 Electrochimica Corporation Electrolyte for zinc anode batteries and method of making same
EP0028879B1 (en) * 1979-10-30 1990-03-28 General Motors Corporation Zinc electrodes for nickel-zinc accumulators
US4358517A (en) * 1979-10-30 1982-11-09 General Motors Corporation Nickel-zinc cell
US4260669A (en) * 1980-03-14 1981-04-07 Union Carbide Corporation Alkaline-MnO2 cell having a zinc powder-gel anode containing starch graft copolymer
JPS60208053A (ja) * 1984-03-31 1985-10-19 Furukawa Battery Co Ltd:The アルカリ蓄電池用亜鉛極
JP2557683B2 (ja) * 1988-05-16 1996-11-27 三洋電機株式会社 アルカリ蓄電池用亜鉛活物質及びその製造方法並びにその活物質を用いた亜鉛極
JPH02215047A (ja) * 1989-02-16 1990-08-28 Sanyo Electric Co Ltd アルカリ蓄電池用亜鉛極の製造方法
US5378329A (en) * 1990-12-31 1995-01-03 Electric Fuel (E.F.L.) Ltd. Process for the preparation of an alkaline-zinc slurry for use in batteries
US5215836A (en) * 1991-07-18 1993-06-01 Electrochimica Corporation Alkaline galvanic cells
US5302475A (en) * 1991-11-12 1994-04-12 The Regents Of The University Of California Rechargeable zinc cell with alkaline electrolyte which inhibits shape change in zinc electrode
JP3018715B2 (ja) * 1992-02-26 2000-03-13 松下電器産業株式会社 亜鉛アルカリ電池の製造法
US5424145A (en) * 1992-03-18 1995-06-13 Battery Technologies Inc. High capacity rechargeable cell having manganese dioxide electrode
US5401590A (en) * 1992-12-07 1995-03-28 Duracell Inc. Additives for electrochemical cells having zinc anodes
JP3257876B2 (ja) * 1993-09-27 2002-02-18 富士写真フイルム株式会社 シート状極板の製造方法および化学電池
US5863676A (en) * 1997-03-27 1999-01-26 Energy Research Corporation Calcium-zincate electrode for alkaline batteries and method for making same
GB9713683D0 (en) * 1997-06-27 1997-09-03 Battery Technologies Inc Additives for rechargeable alkaline manganese dioxide cells
JP3653410B2 (ja) * 1998-03-24 2005-05-25 三洋電機株式会社 密閉型アルカリ亜鉛蓄電池
FR2778498B1 (fr) * 1998-05-07 2000-06-09 Alsthom Cge Alcatel Accumulateur a electrolyte alcalin contenant une electrode negative au zinc

Similar Documents

Publication Publication Date Title
US7816035B2 (en) Methods for production of zinc oxide electrodes for alkaline batteries
CN101898799A (zh) 一种锰酸锂空心球材料的制备方法
WO2018163485A1 (ja) アルカリ乾電池
CN115784325A (zh) 一种适合储能应用的钠离子电池正极材料的制备方法
CN102088084A (zh) 一种锂电池复合电极活性材料及其制备方法
EP0212318A1 (fr) Procédé de fabrication d'une électrode au cadmium consolidée par polymère pour accumulateur alcalin et électrode obtenue par ce procédé
JP2002056844A (ja) アルカリ蓄電池用正極活物質の製造方法およびこの正極活物質を用いたニッケル電極ならびにこのニッケル電極を用いたアルカリ蓄電池
JPH0350384B2 (enExample)
JP3736842B2 (ja) アルカリ電解液電池用電極およびそれを用いたアルカリ電解液電池
JP2001185138A (ja) アルカリ蓄電池用正極活物質及びその製法
CN102306763A (zh) 一种圆柱形碱性锌锰电池正极粉及其制备方法
JP2004339601A (ja) ニッケル粉末の製造方法
CN105330265A (zh) 一种适于量产β”-Al2O3隔膜的方法
JPS60170167A (ja) アルカリ電池用電極の製造方法
JPH0514382B2 (enExample)
JP4305029B2 (ja) 非焼結式ニッケル正極を備えたアルカリ蓄電池
JP3369783B2 (ja) アルカリ蓄電池用水酸化ニッケル電極の製造方法及びアルカリ蓄電池
JPH0569264B2 (enExample)
JPH01187768A (ja) アルカリ電池用ニッケル極
JPS61203566A (ja) アルカリ蓄電池用カドミウム負極板の製造法
JP2022084052A (ja) 負極活物質の製造方法
JPH041992B2 (enExample)
JPS61239564A (ja) アルカリ蓄電池用陽極の製造方法
JPS59186265A (ja) 電池用ガス拡散電極の製造法
JPH07120530B2 (ja) アルカリ電池用焼結式ニッケル基板の製造方法