JP2004189833A5 - - Google Patents

Download PDF

Info

Publication number
JP2004189833A5
JP2004189833A5 JP2002358058A JP2002358058A JP2004189833A5 JP 2004189833 A5 JP2004189833 A5 JP 2004189833A5 JP 2002358058 A JP2002358058 A JP 2002358058A JP 2002358058 A JP2002358058 A JP 2002358058A JP 2004189833 A5 JP2004189833 A5 JP 2004189833A5
Authority
JP
Japan
Prior art keywords
heat
polylactic acid
heat resistance
crystallization
treated
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP2002358058A
Other languages
English (en)
Other versions
JP2004189833A (ja
Filing date
Publication date
Application filed filed Critical
Priority to JP2002358058A priority Critical patent/JP2004189833A/ja
Priority claimed from JP2002358058A external-priority patent/JP2004189833A/ja
Publication of JP2004189833A publication Critical patent/JP2004189833A/ja
Publication of JP2004189833A5 publication Critical patent/JP2004189833A5/ja
Pending legal-status Critical Current

Description

このため、ポリ乳酸からなる成形品の耐熱性を向上させるため、成形品を熱処理して結晶化させる(特開平9−12748)、あるいは、延伸配向結晶化させる(特開平8−73628)方法が提案されているが、ポリ乳酸は結晶化速度が遅く、成形品を熱処理すると不透明になってしまうという問題があり、また延伸配向結晶化による方法では、透明で耐熱性のあるシートができるが、十分な耐熱性を発現させるためには、縦方向と横方向に少なくとも2倍以上延伸する必要があり、大がかりで高価な設備が必要であるばかりでなく、350μm以上の厚いシートの製造が難しい。さらに、ポリ乳酸は結晶化速度が遅いため、延伸倍率高いと、その後ヒートセットを十分に行っても、延伸による歪みが解消されず、Tg以上に加熱すると歪みの解放による変形が生じてしまう。
ΔPが0.03を超えると、シートの延伸歪みが大きくなり、Tgを超える高温状態で、延伸歪みの解放による変形が生じやすくなり、耐熱性が低下する。ΔPの好ましい範囲は0〜0.02であり、特に好ましく0.0001〜0.01、さらに好ましくは0.001〜0.005である。
JP2002358058A 2002-12-10 2002-12-10 ポリ乳酸よりなるシート及びその製造方法 Pending JP2004189833A (ja)