JP2003173772A - 電極用水素吸蔵合金粉末およびその製造方法 - Google Patents
電極用水素吸蔵合金粉末およびその製造方法Info
- Publication number
- JP2003173772A JP2003173772A JP2001370468A JP2001370468A JP2003173772A JP 2003173772 A JP2003173772 A JP 2003173772A JP 2001370468 A JP2001370468 A JP 2001370468A JP 2001370468 A JP2001370468 A JP 2001370468A JP 2003173772 A JP2003173772 A JP 2003173772A
- Authority
- JP
- Japan
- Prior art keywords
- hydrogen storage
- alloy powder
- storage alloy
- electrode
- hydrogen
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Withdrawn
Links
Classifications
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E60/00—Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
- Y02E60/10—Energy storage using batteries
Landscapes
- Powder Metallurgy (AREA)
- Secondary Cells (AREA)
- Battery Electrode And Active Subsutance (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP2001370468A JP2003173772A (ja) | 2001-12-04 | 2001-12-04 | 電極用水素吸蔵合金粉末およびその製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP2001370468A JP2003173772A (ja) | 2001-12-04 | 2001-12-04 | 電極用水素吸蔵合金粉末およびその製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JP2003173772A true JP2003173772A (ja) | 2003-06-20 |
| JP2003173772A5 JP2003173772A5 (enExample) | 2005-04-14 |
Family
ID=19179689
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP2001370468A Withdrawn JP2003173772A (ja) | 2001-12-04 | 2001-12-04 | 電極用水素吸蔵合金粉末およびその製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JP2003173772A (enExample) |
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2005279418A (ja) * | 2004-03-29 | 2005-10-13 | Taiheiyo Cement Corp | 水素貯蔵材料の製造装置および水素貯蔵材料の製造方法ならびに水素貯蔵材料 |
| CN100438148C (zh) * | 2005-09-21 | 2008-11-26 | 比亚迪股份有限公司 | 一种合金粉的表面处理方法 |
| JP2009287044A (ja) * | 2008-05-27 | 2009-12-10 | Mitsui Mining & Smelting Co Ltd | 金属微粒子及び金属微粒子の製造方法 |
-
2001
- 2001-12-04 JP JP2001370468A patent/JP2003173772A/ja not_active Withdrawn
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2005279418A (ja) * | 2004-03-29 | 2005-10-13 | Taiheiyo Cement Corp | 水素貯蔵材料の製造装置および水素貯蔵材料の製造方法ならびに水素貯蔵材料 |
| CN100438148C (zh) * | 2005-09-21 | 2008-11-26 | 比亚迪股份有限公司 | 一种合金粉的表面处理方法 |
| JP2009287044A (ja) * | 2008-05-27 | 2009-12-10 | Mitsui Mining & Smelting Co Ltd | 金属微粒子及び金属微粒子の製造方法 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP5743780B2 (ja) | 円筒型ニッケル−水素蓄電池 | |
| JP4678130B2 (ja) | 密閉型ニッケル水素蓄電池とその製造法 | |
| JP2988479B1 (ja) | アルカリ蓄電池と水素吸蔵合金電極及びその製造法 | |
| JP5119577B2 (ja) | ニッケル水素電池 | |
| JP3835993B2 (ja) | 電極用合金粉末およびその製造法 | |
| US6790558B2 (en) | Electrode alloy powder and method of producing the same | |
| JP5465478B2 (ja) | アルカリ蓄電池用負極、アルカリ蓄電池及びアルカリ蓄電池の製造方法 | |
| EP0944124B1 (en) | Hydrogen-absorbing alloy for battery, method for producing the same, and alkaline storage battery using the same | |
| JP5142428B2 (ja) | ニッケル水素蓄電池用水素吸蔵合金電極の製造方法 | |
| JP3553750B2 (ja) | アルカリ蓄電池用水素吸蔵合金の製造方法 | |
| JP4743997B2 (ja) | 水素吸蔵合金電極 | |
| JP2003173772A (ja) | 電極用水素吸蔵合金粉末およびその製造方法 | |
| JP2003533854A (ja) | NiMH電池用の合金粉末の特性を改善する方法 | |
| JP2004124132A (ja) | 水素吸蔵合金粉末、水素吸蔵合金電極およびそれを用いたニッケル水素蓄電池。 | |
| JP3547920B2 (ja) | 水素吸蔵合金電極の製造方法 | |
| JP2001135311A (ja) | アルカリ蓄電池 | |
| JP3387314B2 (ja) | 水素吸蔵合金電極の製造方法 | |
| JP4115367B2 (ja) | アルカリ蓄電池用水素吸蔵合金及びその製造方法並びにアルカリ蓄電池 | |
| JP3568337B2 (ja) | 水素吸蔵合金電極及び金属水素化物蓄電池 | |
| JP2008269888A (ja) | ニッケル水素蓄電池 | |
| JP3651324B2 (ja) | アルカリ蓄電池とそれに用いる水素吸蔵合金粉末およびその製造法 | |
| JPH10149824A (ja) | 水素吸蔵合金電極の製造方法 | |
| JP3414172B2 (ja) | 電池用水素吸蔵合金の製造法 | |
| JP3322449B2 (ja) | 金属水素化物電極の製造方法 | |
| JP3553752B2 (ja) | 水素吸蔵合金電極の製造方法 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| A521 | Request for written amendment filed |
Free format text: JAPANESE INTERMEDIATE CODE: A523 Effective date: 20040609 |
|
| A621 | Written request for application examination |
Free format text: JAPANESE INTERMEDIATE CODE: A621 Effective date: 20040609 |
|
| A977 | Report on retrieval |
Free format text: JAPANESE INTERMEDIATE CODE: A971007 Effective date: 20050927 |
|
| A761 | Written withdrawal of application |
Free format text: JAPANESE INTERMEDIATE CODE: A761 Effective date: 20070704 |