JP2000282259A - 低摩擦被膜を持つ金属部材の製造方法 - Google Patents
低摩擦被膜を持つ金属部材の製造方法Info
- Publication number
- JP2000282259A JP2000282259A JP8908999A JP8908999A JP2000282259A JP 2000282259 A JP2000282259 A JP 2000282259A JP 8908999 A JP8908999 A JP 8908999A JP 8908999 A JP8908999 A JP 8908999A JP 2000282259 A JP2000282259 A JP 2000282259A
- Authority
- JP
- Japan
- Prior art keywords
- solid lubricant
- metal member
- metal
- soft metal
- powder
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Landscapes
- Other Surface Treatments For Metallic Materials (AREA)
- Application Of Or Painting With Fluid Materials (AREA)
- Coating Apparatus (AREA)
- Lubricants (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP8908999A JP2000282259A (ja) | 1999-03-30 | 1999-03-30 | 低摩擦被膜を持つ金属部材の製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP8908999A JP2000282259A (ja) | 1999-03-30 | 1999-03-30 | 低摩擦被膜を持つ金属部材の製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JP2000282259A true JP2000282259A (ja) | 2000-10-10 |
| JP2000282259A5 JP2000282259A5 (enExample) | 2003-01-15 |
Family
ID=13961162
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP8908999A Pending JP2000282259A (ja) | 1999-03-30 | 1999-03-30 | 低摩擦被膜を持つ金属部材の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JP2000282259A (enExample) |
Cited By (14)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP3357661B2 (ja) | 2000-11-17 | 2002-12-16 | 株式会社不二機販 | 潤滑性被膜の形成方法 |
| GB2401562A (en) * | 2003-06-19 | 2004-11-17 | David Taylor | Leach-preventative coating for a lead sheet |
| RU2247173C2 (ru) * | 2003-04-04 | 2005-02-27 | Ульяновская государственная сельскохозяйственная академия | Способ комбинированной поверхностной обработки деталей |
| WO2006096742A1 (en) * | 2005-03-08 | 2006-09-14 | University Of Florida Research Foundation, Inc. | In-situ lubrication of sliding electrical contacts |
| JP2008051179A (ja) * | 2006-08-23 | 2008-03-06 | Toyota Motor Corp | 摺動部材及び摺動部材の製造方法 |
| JP2009120917A (ja) * | 2007-11-16 | 2009-06-04 | Panasonic Corp | 摺動部材及び流体機械 |
| CN100580067C (zh) * | 2005-11-28 | 2010-01-13 | 日本特殊陶业株式会社 | 抗热接剂、传感器及包括传感器的组件 |
| US7767033B2 (en) | 2006-07-28 | 2010-08-03 | Art Metal Mfg Co., Ltd. | Method for surface treatment of an internal combustion piston and an internal combustion piston |
| KR101170050B1 (ko) | 2003-11-11 | 2012-08-01 | 후지 세이사쿠쇼 가부시키가이샤 | 분사노즐, 그 분사노즐을 구비한 블라스트 가공장치 및블라스트 가공 방법, 그 블라스트 가공 방법에 의한윤활층 형성 방법, 및 그 방법에 의해 윤활층을 형성한접동제품 |
| US8410029B2 (en) | 2008-06-11 | 2013-04-02 | Fuji Kihan Co., Ltd. | Surface-oxide abrasion-resistant lubricant coating and method for forming the same |
| US8430020B2 (en) | 2008-10-08 | 2013-04-30 | Art Metal Mfg Co., Ltd. | Method for surface treatment of a skirt portion of a piston for an internal combustion engine and a piston for an internal combustion engine |
| US8518862B2 (en) | 2005-11-28 | 2013-08-27 | Ngk Spark Plug Co., Ltd. | Anti-seizing agent, sensor and assembly including sensor |
| JP2014152211A (ja) * | 2013-02-06 | 2014-08-25 | Daikin Ind Ltd | 固体粒子、固体潤滑剤及び金属部材 |
| CN117753993A (zh) * | 2023-05-09 | 2024-03-26 | 南阳理工学院 | 一种以SnBiAg和Al2O3为复合润滑剂的微斜孔结构TC16基自润滑材料及其制备方法 |
-
1999
- 1999-03-30 JP JP8908999A patent/JP2000282259A/ja active Pending
Cited By (17)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP3357661B2 (ja) | 2000-11-17 | 2002-12-16 | 株式会社不二機販 | 潤滑性被膜の形成方法 |
| RU2247173C2 (ru) * | 2003-04-04 | 2005-02-27 | Ульяновская государственная сельскохозяйственная академия | Способ комбинированной поверхностной обработки деталей |
| GB2401562A (en) * | 2003-06-19 | 2004-11-17 | David Taylor | Leach-preventative coating for a lead sheet |
| GB2401562B (en) * | 2003-06-19 | 2005-03-30 | David Taylor | Improvement to lead sheet materials |
| KR101170050B1 (ko) | 2003-11-11 | 2012-08-01 | 후지 세이사쿠쇼 가부시키가이샤 | 분사노즐, 그 분사노즐을 구비한 블라스트 가공장치 및블라스트 가공 방법, 그 블라스트 가공 방법에 의한윤활층 형성 방법, 및 그 방법에 의해 윤활층을 형성한접동제품 |
| US7960317B2 (en) | 2005-03-08 | 2011-06-14 | University Of Florida Research Foundation, Inc. | In-situ lubrication of sliding electrical contacts |
| WO2006096742A1 (en) * | 2005-03-08 | 2006-09-14 | University Of Florida Research Foundation, Inc. | In-situ lubrication of sliding electrical contacts |
| US8518862B2 (en) | 2005-11-28 | 2013-08-27 | Ngk Spark Plug Co., Ltd. | Anti-seizing agent, sensor and assembly including sensor |
| CN100580067C (zh) * | 2005-11-28 | 2010-01-13 | 日本特殊陶业株式会社 | 抗热接剂、传感器及包括传感器的组件 |
| US7767033B2 (en) | 2006-07-28 | 2010-08-03 | Art Metal Mfg Co., Ltd. | Method for surface treatment of an internal combustion piston and an internal combustion piston |
| US8231741B2 (en) | 2006-07-28 | 2012-07-31 | Art Metal Mfg Co., Ltd. | Method for surface treatment of an internal combustion pistion and an internal combustion piston |
| JP2008051179A (ja) * | 2006-08-23 | 2008-03-06 | Toyota Motor Corp | 摺動部材及び摺動部材の製造方法 |
| JP2009120917A (ja) * | 2007-11-16 | 2009-06-04 | Panasonic Corp | 摺動部材及び流体機械 |
| US8410029B2 (en) | 2008-06-11 | 2013-04-02 | Fuji Kihan Co., Ltd. | Surface-oxide abrasion-resistant lubricant coating and method for forming the same |
| US8430020B2 (en) | 2008-10-08 | 2013-04-30 | Art Metal Mfg Co., Ltd. | Method for surface treatment of a skirt portion of a piston for an internal combustion engine and a piston for an internal combustion engine |
| JP2014152211A (ja) * | 2013-02-06 | 2014-08-25 | Daikin Ind Ltd | 固体粒子、固体潤滑剤及び金属部材 |
| CN117753993A (zh) * | 2023-05-09 | 2024-03-26 | 南阳理工学院 | 一种以SnBiAg和Al2O3为复合润滑剂的微斜孔结构TC16基自润滑材料及其制备方法 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP6300843B2 (ja) | 摺動部材 | |
| GB2374640A (en) | Sliding bearing with polybenzimidazole | |
| US5217814A (en) | Sintered sliding material | |
| CN106795640A (zh) | 自润滑复合涂层 | |
| JP2013072535A (ja) | すべり軸受 | |
| Karthik et al. | Tribological studies of Ni-SiC and Ni-Al2O3 composite coatings by pulsed electrodeposition | |
| EP0340257B1 (en) | Mechanically plated coatings containing lubricant particles | |
| JP2015137384A (ja) | 金属皮膜およびその成膜方法 | |
| Roy et al. | Pulse current co-deposition of Ni-WS2 nano-composite film for solid lubrication | |
| EP2507406A2 (en) | Electroless ni-composite plated substrate and method | |
| RU2149218C1 (ru) | Состав для покрытий и способ его нанесения | |
| JPH05302176A5 (enExample) | ||
| JP2877737B2 (ja) | 摺動材料 | |
| Çuvalcı et al. | Investigation of the abrasive wear behaviour of ZA-27 alloy and CuSn10 bronze | |
| Zuo et al. | Effect of activators on the properties of nickel coated diamond composite powders | |
| JP4977599B2 (ja) | 基材の表面にフッ素樹脂潤滑皮膜を形成する方法 | |
| JP2923440B2 (ja) | 可撓性ダイヤモンド塗装研磨物体 | |
| CN116328026B (zh) | 一种具有自润滑功能的TiN/GO复合陶瓷涂层及其制备方法 | |
| JPS6479417A (ja) | 摺動材料ならびにその製造方法 | |
| JP5568147B1 (ja) | 摺動接触部材 | |
| KR101841471B1 (ko) | 복합 표면 처리방법을 이용한 다층구조 금속 제조방법 및 이에 의하여 제조된 다층구조 금속 | |
| CN114717512B (zh) | 一种自适应长效润滑性能金/碳复合薄膜的制备方法 | |
| JP2004018979A (ja) | 複合めっき皮膜 | |
| JP3513273B2 (ja) | 気体軸受けユニット | |
| JP2014157826A (ja) | 電気接点部材 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| A977 | Report on retrieval |
Free format text: JAPANESE INTERMEDIATE CODE: A971007 Effective date: 20040622 |
|
| A131 | Notification of reasons for refusal |
Effective date: 20050708 Free format text: JAPANESE INTERMEDIATE CODE: A131 |
|
| A521 | Written amendment |
Free format text: JAPANESE INTERMEDIATE CODE: A523 Effective date: 20050902 |
|
| A02 | Decision of refusal |
Effective date: 20060317 Free format text: JAPANESE INTERMEDIATE CODE: A02 |