ID27568A - Metoda-metoda penghambatan korosi dengan menggunakan isomer-isomer dari kloro-metilbenzotriazol - Google Patents
Metoda-metoda penghambatan korosi dengan menggunakan isomer-isomer dari kloro-metilbenzotriazolInfo
- Publication number
- ID27568A ID27568A IDW20010102A ID20010102A ID27568A ID 27568 A ID27568 A ID 27568A ID W20010102 A IDW20010102 A ID W20010102A ID 20010102 A ID20010102 A ID 20010102A ID 27568 A ID27568 A ID 27568A
- Authority
- ID
- Indonesia
- Prior art keywords
- chloro
- isomers
- methylbenzotriazol
- corrosion hazard
- methods
- Prior art date
Links
- 238000005260 corrosion Methods 0.000 title abstract 3
- 230000007797 corrosion Effects 0.000 title abstract 3
- BUOLWKSFADWMOX-UHFFFAOYSA-N 5-chloro-4-methyl-2h-benzotriazole Chemical class CC1=C(Cl)C=CC2=NNN=C12 BUOLWKSFADWMOX-UHFFFAOYSA-N 0.000 title abstract 2
- 238000000034 method Methods 0.000 title 1
- 239000003112 inhibitor Substances 0.000 abstract 2
- CMGDVUCDZOBDNL-UHFFFAOYSA-N 4-methyl-2h-benzotriazole Chemical compound CC1=CC=CC2=NNN=C12 CMGDVUCDZOBDNL-UHFFFAOYSA-N 0.000 abstract 1
- ZAMOUSCENKQFHK-UHFFFAOYSA-N Chlorine atom Chemical compound [Cl] ZAMOUSCENKQFHK-UHFFFAOYSA-N 0.000 abstract 1
- 229910052801 chlorine Inorganic materials 0.000 abstract 1
- 239000000460 chlorine Substances 0.000 abstract 1
Classifications
-
- C—CHEMISTRY; METALLURGY
- C23—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
- C23F—NON-MECHANICAL REMOVAL OF METALLIC MATERIAL FROM SURFACE; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL; MULTI-STEP PROCESSES FOR SURFACE TREATMENT OF METALLIC MATERIAL INVOLVING AT LEAST ONE PROCESS PROVIDED FOR IN CLASS C23 AND AT LEAST ONE PROCESS COVERED BY SUBCLASS C21D OR C22F OR CLASS C25
- C23F11/00—Inhibiting corrosion of metallic material by applying inhibitors to the surface in danger of corrosion or adding them to the corrosive agent
- C23F11/08—Inhibiting corrosion of metallic material by applying inhibitors to the surface in danger of corrosion or adding them to the corrosive agent in other liquids
- C23F11/10—Inhibiting corrosion of metallic material by applying inhibitors to the surface in danger of corrosion or adding them to the corrosive agent in other liquids using organic inhibitors
- C23F11/14—Nitrogen-containing compounds
- C23F11/149—Heterocyclic compounds containing nitrogen as hetero atom
-
- C—CHEMISTRY; METALLURGY
- C07—ORGANIC CHEMISTRY
- C07D—HETEROCYCLIC COMPOUNDS
- C07D249/00—Heterocyclic compounds containing five-membered rings having three nitrogen atoms as the only ring hetero atoms
- C07D249/16—Heterocyclic compounds containing five-membered rings having three nitrogen atoms as the only ring hetero atoms condensed with carbocyclic rings or ring systems
- C07D249/18—Benzotriazoles
-
- C—CHEMISTRY; METALLURGY
- C09—DYES; PAINTS; POLISHES; NATURAL RESINS; ADHESIVES; COMPOSITIONS NOT OTHERWISE PROVIDED FOR; APPLICATIONS OF MATERIALS NOT OTHERWISE PROVIDED FOR
- C09K—MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C09K15/00—Anti-oxidant compositions; Compositions inhibiting chemical change
- C09K15/04—Anti-oxidant compositions; Compositions inhibiting chemical change containing organic compounds
- C09K15/30—Anti-oxidant compositions; Compositions inhibiting chemical change containing organic compounds containing heterocyclic ring with at least one nitrogen atom as ring member
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y10—TECHNICAL SUBJECTS COVERED BY FORMER USPC
- Y10S—TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y10S585/00—Chemistry of hydrocarbon compounds
- Y10S585/949—Miscellaneous considerations
- Y10S585/95—Prevention or removal of corrosion or solid deposits
Landscapes
- Chemical & Material Sciences (AREA)
- Organic Chemistry (AREA)
- Engineering & Computer Science (AREA)
- Materials Engineering (AREA)
- Mechanical Engineering (AREA)
- Metallurgy (AREA)
- Preventing Corrosion Or Incrustation Of Metals (AREA)
- Agricultural Chemicals And Associated Chemicals (AREA)
- Low-Molecular Organic Synthesis Reactions Using Catalysts (AREA)
- Heterocyclic Carbon Compounds Containing A Hetero Ring Having Nitrogen And Oxygen As The Only Ring Hetero Atoms (AREA)
- Organic Low-Molecular-Weight Compounds And Preparation Thereof (AREA)
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| US09/103,493 US5968408A (en) | 1998-06-24 | 1998-06-24 | Methods of inhibiting corrosion using isomers of chloro-methylbenzotriazole |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| ID27568A true ID27568A (id) | 2001-04-12 |
Family
ID=22295489
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| IDW20010102A ID27568A (id) | 1998-06-24 | 1999-03-17 | Metoda-metoda penghambatan korosi dengan menggunakan isomer-isomer dari kloro-metilbenzotriazol |
Country Status (18)
| Country | Link |
|---|---|
| US (1) | US5968408A (enExample) |
| EP (1) | EP1089982B1 (enExample) |
| JP (1) | JP2002518484A (enExample) |
| KR (1) | KR100648555B1 (enExample) |
| CN (1) | CN1184210C (enExample) |
| AT (1) | ATE338031T1 (enExample) |
| AU (1) | AU757100B2 (enExample) |
| BR (1) | BR9911464B1 (enExample) |
| CA (1) | CA2335160C (enExample) |
| DE (1) | DE69933030T2 (enExample) |
| ES (1) | ES2272059T3 (enExample) |
| HU (1) | HUP0102259A3 (enExample) |
| ID (1) | ID27568A (enExample) |
| NO (1) | NO20006478D0 (enExample) |
| NZ (1) | NZ508503A (enExample) |
| PL (1) | PL345021A1 (enExample) |
| TW (1) | TW422876B (enExample) |
| WO (1) | WO1999067222A1 (enExample) |
Families Citing this family (12)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CN1047326C (zh) * | 1995-06-14 | 1999-12-15 | 中国石油化工总公司石油化工科学研究院 | 一种铂铼重整催化剂 |
| CA2394440A1 (en) * | 2001-08-02 | 2003-02-02 | Rohm And Haas Company | Process for treating aqueous systems |
| UA66669C2 (en) * | 2003-09-08 | 2006-05-15 | A composition for the prevention of acid microbiological corrosion of water , a method for water treatment and a method for utilization of industrial waters containing ammonium nitrogen | |
| US8105531B1 (en) | 2010-12-21 | 2012-01-31 | Ecolab Usa Inc. | Corrosion inhibition of hypochlorite solutions using polyacrylate and Ca |
| US8114344B1 (en) | 2010-12-21 | 2012-02-14 | Ecolab Usa Inc. | Corrosion inhibition of hypochlorite solutions using sugar acids and Ca |
| US8603392B2 (en) | 2010-12-21 | 2013-12-10 | Ecolab Usa Inc. | Electrolyzed water system |
| US8114343B1 (en) | 2010-12-21 | 2012-02-14 | Ecolab USA, Inc. | Corrosion inhibition of hypochlorite solutions using Zn and Ca |
| US8557178B2 (en) | 2010-12-21 | 2013-10-15 | Ecolab Usa Inc. | Corrosion inhibition of hypochlorite solutions in saturated wipes |
| BR112018075447B1 (pt) * | 2016-06-09 | 2023-01-10 | Chemtreat, Inc | Métodos para medir, monitorar e controlar a concentração de um composto triazólico halogenado ex situ na água de um sistema de água |
| CA3087518A1 (en) | 2018-01-03 | 2019-07-11 | Ecolab Usa Inc. | Process and method for reducing metal corrosion in water |
| JP7209004B2 (ja) * | 2018-03-28 | 2023-01-19 | フジフイルム エレクトロニック マテリアルズ ユー.エス.エー., インコーポレイテッド | ルテニウムバリアの化学機械研磨スラリー |
| CN110205633A (zh) * | 2019-07-08 | 2019-09-06 | 威海翔泽新材料科技有限公司 | 一种耐卤素铜缓蚀剂及其制备方法 |
Family Cites Families (9)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| GB1065995A (en) * | 1963-12-06 | 1967-04-19 | Geigy Uk Ltd | Benzotriazoles and their production |
| US3985503A (en) * | 1975-03-17 | 1976-10-12 | The Sherwin-Williams Company | Process for inhibiting metal corrosion |
| US4107060A (en) * | 1975-06-17 | 1978-08-15 | Mobil Oil Corporation | Lubricant compositions containing biocidal, antirust additives |
| JPS5318432A (en) * | 1976-08-03 | 1978-02-20 | Nippon Musical Instruments Mfg | Degreasing and cleaning solution |
| US4642221A (en) * | 1983-07-05 | 1987-02-10 | Atlantic Richfield Company | Method and composition for inhibiting corrosion in aqueous heat transfer systems |
| US4744950A (en) * | 1984-06-26 | 1988-05-17 | Betz Laboratories, Inc. | Method of inhibiting the corrosion of copper in aqueous mediums |
| US5411677A (en) * | 1993-04-26 | 1995-05-02 | The Penn State Research Foundation | Method and composition for preventing copper corrosion |
| US5773627A (en) * | 1995-03-21 | 1998-06-30 | Betzdearborn Inc. | Methods of inhibiting corrosion using halo-benzotriazoles |
| MY129257A (en) * | 1995-03-21 | 2007-03-30 | Betz Laboratories | Methods of inhibiting corrosion using halo-benzotriazoles |
-
1998
- 1998-06-24 US US09/103,493 patent/US5968408A/en not_active Expired - Lifetime
-
1999
- 1999-03-12 TW TW088103798A patent/TW422876B/zh not_active IP Right Cessation
- 1999-03-17 CN CNB998077844A patent/CN1184210C/zh not_active Expired - Lifetime
- 1999-03-17 PL PL99345021A patent/PL345021A1/xx unknown
- 1999-03-17 AU AU30944/99A patent/AU757100B2/en not_active Expired
- 1999-03-17 EP EP99912602A patent/EP1089982B1/en not_active Expired - Lifetime
- 1999-03-17 KR KR1020007014717A patent/KR100648555B1/ko not_active Expired - Lifetime
- 1999-03-17 JP JP2000555876A patent/JP2002518484A/ja active Pending
- 1999-03-17 CA CA002335160A patent/CA2335160C/en not_active Expired - Lifetime
- 1999-03-17 WO PCT/US1999/005785 patent/WO1999067222A1/en not_active Ceased
- 1999-03-17 DE DE69933030T patent/DE69933030T2/de not_active Expired - Lifetime
- 1999-03-17 ES ES99912602T patent/ES2272059T3/es not_active Expired - Lifetime
- 1999-03-17 ID IDW20010102A patent/ID27568A/id unknown
- 1999-03-17 NZ NZ508503A patent/NZ508503A/xx not_active IP Right Cessation
- 1999-03-17 AT AT99912602T patent/ATE338031T1/de not_active IP Right Cessation
- 1999-03-17 BR BRPI9911464-0A patent/BR9911464B1/pt not_active IP Right Cessation
- 1999-03-17 HU HU0102259A patent/HUP0102259A3/hu unknown
-
2000
- 2000-12-19 NO NO20006478A patent/NO20006478D0/no not_active Application Discontinuation
Also Published As
| Publication number | Publication date |
|---|---|
| DE69933030T2 (de) | 2007-04-12 |
| DE69933030D1 (de) | 2006-10-12 |
| EP1089982B1 (en) | 2006-08-30 |
| JP2002518484A (ja) | 2002-06-25 |
| AU757100B2 (en) | 2003-01-30 |
| CA2335160A1 (en) | 1999-12-29 |
| PL345021A1 (en) | 2001-11-19 |
| CN1184210C (zh) | 2005-01-12 |
| EP1089982A1 (en) | 2001-04-11 |
| BR9911464B1 (pt) | 2010-09-08 |
| WO1999067222A1 (en) | 1999-12-29 |
| HUP0102259A2 (hu) | 2001-09-28 |
| NO20006478L (no) | 2000-12-19 |
| ATE338031T1 (de) | 2006-09-15 |
| CN1306517A (zh) | 2001-08-01 |
| BR9911464A (pt) | 2001-09-18 |
| HUP0102259A3 (en) | 2002-06-28 |
| ES2272059T3 (es) | 2007-04-16 |
| US5968408A (en) | 1999-10-19 |
| NZ508503A (en) | 2003-03-28 |
| AU3094499A (en) | 2000-01-10 |
| EP1089982A4 (en) | 2005-04-06 |
| KR20010053155A (ko) | 2001-06-25 |
| KR100648555B1 (ko) | 2006-11-24 |
| TW422876B (en) | 2001-02-21 |
| NO20006478D0 (no) | 2000-12-19 |
| CA2335160C (en) | 2006-01-03 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| MY129257A (en) | Methods of inhibiting corrosion using halo-benzotriazoles | |
| DE69609193D1 (de) | Neosäure als korrosinsinhibitoren | |
| DE60320251D1 (de) | Wässriges gel und herstellungsverfahren und verwendung des wässrigen gels | |
| DE60123392D1 (de) | Verbessertes enteisungs- und befeuchtungsmittel | |
| PL345021A1 (en) | Methods of inhibiting corrosion using isomers of chloro-methylbenzotriazole | |
| DE69317764D1 (de) | Aminoacetylmercaptoacetylamid derivate mit enkephalinase- und ace-hemmwirkung | |
| EA200000251A1 (ru) | Производные резорцинола | |
| MXPA01009299A (es) | Aditivo inhibidor de corrosion no carcinogenico. | |
| YU19299A (sh) | Supstituisani tricikli | |
| ATE326209T1 (de) | Verminderung des haarwuchses | |
| AU1930900A (en) | Use of protease inhibitors to modulate cellular pathways, immunity and therapiesassociated therewith | |
| DE60020377D1 (de) | Verfahren zur korrsosionsinhibierung geeignet zur verwendung in trinkwasser | |
| DK1274883T3 (da) | Korrosionsinhibitor | |
| BG100248A (bg) | Инхибитори на скваленсинтетаза | |
| EA200300468A1 (ru) | Подавление зависимости опухолевых клеток от фактора роста | |
| EA200100853A1 (ru) | Резорциновая композиция | |
| DE60018802D1 (de) | Emulgiertes gel | |
| DE69910432D1 (de) | Substituierte pyrroloindole | |
| CA2238082A1 (en) | Methods of inhibiting corrosion using halo-benzotriazoles | |
| DK1252118T3 (da) | Kaliummonofluorphosphat som en korrosionshæmmer | |
| ATE256661T1 (de) | Bispiperidine mit antithrombotischer wirkung | |
| SE9900301D0 (sv) | Absorptionskylapparat beskaffad att hindra korrosion i densamma | |
| ATE263750T1 (de) | Neues verfahren | |
| RU96106768A (ru) | Устройство для защиты металлов от коррозии в водной среде | |
| MD1690C2 (ro) | Soluţie pentru conservarea suprafeţei interioare a cazanelor de abur |