GB1418807A - Methods of increasing the wear resistance of the working surfaces of extrusion dies - Google Patents
Methods of increasing the wear resistance of the working surfaces of extrusion diesInfo
- Publication number
- GB1418807A GB1418807A GB703273A GB703273A GB1418807A GB 1418807 A GB1418807 A GB 1418807A GB 703273 A GB703273 A GB 703273A GB 703273 A GB703273 A GB 703273A GB 1418807 A GB1418807 A GB 1418807A
- Authority
- GB
- United Kingdom
- Prior art keywords
- coating
- increasing
- wear resistance
- binder
- die
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C23—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
- C23C—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL
- C23C8/00—Solid state diffusion of only non-metal elements into metallic material surfaces; Chemical surface treatment of metallic material by reaction of the surface with a reactive gas, leaving reaction products of surface material in the coating, e.g. conversion coatings, passivation of metals
- C23C8/80—After-treatment
Landscapes
- Chemical & Material Sciences (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Engineering & Computer Science (AREA)
- Materials Engineering (AREA)
- Mechanical Engineering (AREA)
- Metallurgy (AREA)
- Organic Chemistry (AREA)
- Mounting, Exchange, And Manufacturing Of Dies (AREA)
- Forging (AREA)
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| CH210172A CH578623A5 (enExample) | 1972-02-14 | 1972-02-14 |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| GB1418807A true GB1418807A (en) | 1975-12-24 |
Family
ID=4225894
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| GB703273A Expired GB1418807A (en) | 1972-02-14 | 1973-02-13 | Methods of increasing the wear resistance of the working surfaces of extrusion dies |
Country Status (11)
| Country | Link |
|---|---|
| JP (1) | JPS5621834B2 (enExample) |
| AT (1) | AT320374B (enExample) |
| AU (1) | AU5196373A (enExample) |
| BE (1) | BE795415A (enExample) |
| CH (1) | CH578623A5 (enExample) |
| DE (1) | DE2303632C3 (enExample) |
| DK (1) | DK143862C (enExample) |
| FR (1) | FR2172236B1 (enExample) |
| GB (1) | GB1418807A (enExample) |
| IT (1) | IT979121B (enExample) |
| NL (1) | NL7301883A (enExample) |
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US5100701A (en) * | 1987-04-29 | 1992-03-31 | Siemens Aktiengesellschaft | Solder-repelling coating for tools |
| WO2010145674A1 (en) * | 2009-06-15 | 2010-12-23 | Statoil Asa | Wellbore tubing expansion cone |
Families Citing this family (6)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS51101736A (ja) * | 1975-03-06 | 1976-09-08 | Tokyo Juki Industrial Co Ltd | Tetsukeikinzokunohyomenshorihoho |
| FR2428682A1 (fr) * | 1978-06-16 | 1980-01-11 | Stephanois Rech Meca Hydr Cent | Procede de conditionnement de surface d'une piece metallique et surface obtenue |
| FR2441444A1 (fr) * | 1978-11-20 | 1980-06-13 | Bar Lorforge | Procede de traitement a chaud de masse metallique comportant une mise en forme de celle-ci avec un appareil de formage, permettant d'ameliorer notamment la duree de vie de ce dernier |
| WO1987006273A2 (en) * | 1986-04-10 | 1987-10-22 | MTU MOTOREN- UND TURBINEN-UNION MüNCHEN GMBH | Coating to protect against wear and fretting corrosion of, in particular, metal mechanical components held together by frictional adherence |
| US4692385A (en) * | 1986-04-14 | 1987-09-08 | Materials Development Corporation | Triplex article |
| US4864676A (en) * | 1986-06-04 | 1989-09-12 | Heinrich Schaiper | Tooth brush |
Family Cites Families (7)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| DE540528C (de) * | 1929-01-11 | 1931-12-21 | I G Farbenindustrie Akt Ges | Verwendung von stickstoffgehaertetem Stahl fuer Strangpressen |
| US2622993A (en) * | 1949-08-03 | 1952-12-23 | Deering Milliken Res Trust | Process of lubricating metal surface and article resulting therefrom |
| CH365921A (de) * | 1958-11-04 | 1962-11-30 | Berghaus Elektrophysik Anst | Verfahren zur Behandlung der Oberfläche von Metallkörpern |
| CH397377A (de) * | 1959-01-23 | 1965-08-15 | Berghaus Elektrophysik Anst | Verfahren zur Oberflächenbehandlung von Metallkörpern |
| DE1267055B (de) * | 1965-07-06 | 1968-04-25 | Berghaus Elektrophysik Anst | ? mit extrem verschleissfester Oberflaeche |
| DE1521325C3 (de) * | 1966-04-13 | 1975-06-26 | Elektrophysikalische Anstalt Bernhard Berghaus, Vaduz | Verfahren zur Gewinnung von verschleißfesten Gleitflächen mit guten Einlaufeigenschaften auf Werkstücken aus Elsen und Stahl |
| GB1227452A (enExample) * | 1967-08-07 | 1971-04-07 |
-
0
- BE BE795415D patent/BE795415A/xx unknown
-
1972
- 1972-02-14 CH CH210172A patent/CH578623A5/xx not_active IP Right Cessation
-
1973
- 1973-01-25 DE DE19732303632 patent/DE2303632C3/de not_active Expired
- 1973-02-08 AU AU51963/73A patent/AU5196373A/en not_active Expired
- 1973-02-09 NL NL7301883A patent/NL7301883A/xx not_active Application Discontinuation
- 1973-02-13 GB GB703273A patent/GB1418807A/en not_active Expired
- 1973-02-14 FR FR7305206A patent/FR2172236B1/fr not_active Expired
- 1973-02-14 DK DK78673A patent/DK143862C/da not_active Application Discontinuation
- 1973-02-14 AT AT130473A patent/AT320374B/de active
- 1973-02-14 JP JP1759273A patent/JPS5621834B2/ja not_active Expired
- 1973-02-14 IT IT2040573A patent/IT979121B/it active
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US5100701A (en) * | 1987-04-29 | 1992-03-31 | Siemens Aktiengesellschaft | Solder-repelling coating for tools |
| WO2010145674A1 (en) * | 2009-06-15 | 2010-12-23 | Statoil Asa | Wellbore tubing expansion cone |
Also Published As
| Publication number | Publication date |
|---|---|
| IT979121B (it) | 1974-09-30 |
| CH578623A5 (enExample) | 1976-08-13 |
| DE2303632C3 (de) | 1982-05-06 |
| DE2303632A1 (de) | 1973-08-30 |
| FR2172236A1 (enExample) | 1973-09-28 |
| DK143862B (da) | 1981-10-19 |
| BE795415A (fr) | 1973-05-29 |
| NL7301883A (enExample) | 1973-08-16 |
| AU5196373A (en) | 1974-08-08 |
| JPS4889841A (enExample) | 1973-11-24 |
| DK143862C (da) | 1982-04-05 |
| FR2172236B1 (enExample) | 1978-09-29 |
| JPS5621834B2 (enExample) | 1981-05-21 |
| AT320374B (de) | 1975-02-10 |
| DE2303632B2 (de) | 1981-06-11 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| ES413006A1 (es) | Un metodo de guarnecer la superficie de molde para la cola-da continua de un metal fundido. | |
| US2299192A (en) | Method of making sintered articles | |
| FR2399487A1 (fr) | Procede de realisation de revetement metallique resistant a la corrosion a temperature elevee | |
| GB1418807A (en) | Methods of increasing the wear resistance of the working surfaces of extrusion dies | |
| GB1400642A (en) | Extrusion dies | |
| ES8302254A1 (es) | "procedimiento para el tratamiento superficial de roscas en tubos de acero". | |
| FI865209A0 (fi) | Foerfarande och anordning foer utbredning av vaetskeformiga korrosionsskyddsaemnen pao korrosionsutsatta platser ur en foerpackningsbehaollare eller - behaollardelar. | |
| JPH06294427A (ja) | クラツチ又はブレーキ用摩擦リングの製造方法 | |
| ES2103713T3 (es) | Instalacion y procedimiento para la fabricacion de piezas planas y recubiertas con capas de polvo, en especial piezas de chapa planas. | |
| FR2103432A1 (fr) | Moules a compression pour le formage de matieres plastiques | |
| GB1308374A (en) | Method for producing a die or mould | |
| ES407627A1 (es) | Procedimiento para el tratamiento previo de superficies me-talicas. | |
| ES2071694T3 (es) | Procedimiento para la obtencion de capas de gran dureza sobre materiales de titanio asi como sus aleaciones. | |
| ES360555A1 (es) | Procedimiento para la lubricacion en seco de organos meca- nicos. | |
| GB1479194A (en) | Method for the coating of a shaped article of hardenable plastics material | |
| DE59303156D1 (de) | Verfahren zum herstellen von schleifkörpern fur elektrische kollektoren od.dgl. | |
| GB1141618A (en) | Improvements in and relating to self-lubricating coatings on metal surfaces | |
| CA958312A (en) | Method of coating sintered hard metal bodies with surface layer of carbide | |
| SU1730784A1 (ru) | Способ получения твердосплавного материала с износостойким покрытием | |
| SU1352103A1 (ru) | Способ изготовлени упругодемпфирующего антифрикционного покрыти подп тника | |
| ES423948A1 (es) | Metodo para transformar continuamente metal fundido en un producto solidificado. | |
| GB1500174A (en) | Method for the production of forming tools for deep drawing moulding extruding and the like | |
| GB692190A (en) | Improvements in or relating to plain bearings and the manufacture thereof | |
| ES360901A2 (es) | Perfeccionamiento de tratamiento de superficies metalicas para formar sobre las mismas un revestimiento de lubrifican-te utilizablee para una operacion de conformacion de un me- tal. | |
| SU375169A1 (ru) | ВСЕСОЮЗНАЯ I ..^птиплр^ии""; Н^В: |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| PS | Patent sealed | ||
| PCNP | Patent ceased through non-payment of renewal fee |