GB1289975A - - Google Patents
Info
- Publication number
- GB1289975A GB1289975A GB6076469A GB1289975DA GB1289975A GB 1289975 A GB1289975 A GB 1289975A GB 6076469 A GB6076469 A GB 6076469A GB 1289975D A GB1289975D A GB 1289975DA GB 1289975 A GB1289975 A GB 1289975A
- Authority
- GB
- United Kingdom
- Prior art keywords
- dec
- electrodes
- acid
- headings
- hrs
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C23—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
- C23G—CLEANING OR DE-GREASING OF METALLIC MATERIAL BY CHEMICAL METHODS OTHER THAN ELECTROLYSIS
- C23G1/00—Cleaning or pickling metallic material with solutions or molten salts
- C23G1/14—Cleaning or pickling metallic material with solutions or molten salts with alkaline solutions
- C23G1/20—Other heavy metals
- C23G1/205—Other heavy metals refractory metals
-
- C—CHEMISTRY; METALLURGY
- C23—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
- C23G—CLEANING OR DE-GREASING OF METALLIC MATERIAL BY CHEMICAL METHODS OTHER THAN ELECTROLYSIS
- C23G1/00—Cleaning or pickling metallic material with solutions or molten salts
- C23G1/02—Cleaning or pickling metallic material with solutions or molten salts with acid solutions
- C23G1/10—Other heavy metals
- C23G1/106—Other heavy metals refractory metals
-
- C—CHEMISTRY; METALLURGY
- C25—ELECTROLYTIC OR ELECTROPHORETIC PROCESSES; APPARATUS THEREFOR
- C25B—ELECTROLYTIC OR ELECTROPHORETIC PROCESSES FOR THE PRODUCTION OF COMPOUNDS OR NON-METALS; APPARATUS THEREFOR
- C25B11/00—Electrodes; Manufacture thereof not otherwise provided for
Landscapes
- Chemical & Material Sciences (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Engineering & Computer Science (AREA)
- Materials Engineering (AREA)
- Metallurgy (AREA)
- Organic Chemistry (AREA)
- General Chemical & Material Sciences (AREA)
- Mechanical Engineering (AREA)
- Electrochemistry (AREA)
- Inorganic Compounds Of Heavy Metals (AREA)
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| GB6076469 | 1969-12-12 |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| GB1289975A true GB1289975A (enExample) | 1972-09-20 |
Family
ID=10486039
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| GB6076469A Expired GB1289975A (enExample) | 1969-12-12 | 1969-12-12 |
Country Status (5)
| Country | Link |
|---|---|
| AU (1) | AU2337970A (enExample) |
| BE (1) | BE760193A (enExample) |
| FR (1) | FR2075006A5 (enExample) |
| GB (1) | GB1289975A (enExample) |
| ZA (1) | ZA708398B (enExample) |
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| GB2200136A (en) * | 1987-01-12 | 1988-07-27 | Nihon Parkerizing | Cleaning of aluminium surfaces |
-
1969
- 1969-12-12 GB GB6076469A patent/GB1289975A/en not_active Expired
-
1970
- 1970-12-11 ZA ZA708398A patent/ZA708398B/xx unknown
- 1970-12-11 FR FR7044851A patent/FR2075006A5/fr not_active Expired
- 1970-12-11 BE BE760193A patent/BE760193A/xx unknown
- 1970-12-15 AU AU23379/70A patent/AU2337970A/en not_active Expired
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| GB2200136A (en) * | 1987-01-12 | 1988-07-27 | Nihon Parkerizing | Cleaning of aluminium surfaces |
| GB2200136B (en) * | 1987-01-12 | 1991-05-22 | Nihon Parkerizing | Cleaning of aluminium surfaces |
Also Published As
| Publication number | Publication date |
|---|---|
| FR2075006A5 (enExample) | 1971-10-08 |
| AU2337970A (en) | 1972-06-22 |
| BE760193A (fr) | 1971-06-11 |
| ZA708398B (en) | 1972-07-26 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| SE7703909L (sv) | Sura, vattenhaltiga kemisk omvandling asadkomma beleggningslosningar samt forfarande for att dermed bilda fastsittande korrosionsbestendiga beleggningar pa aluminiumytor | |
| ES460628A1 (es) | Procedimiento para la preparacion de aglutinantes auto-reti-culables para lacas de electro-inmersion depositables cato- dicamente. | |
| GB1449080A (en) | Electrolyte for applying barrier anodic coatings | |
| NL168276C (nl) | Anode voor de elektrolyse van zoutoplossingen, omvattende een substraat van titaan of titaanlegering en een dunne hechtende bekledingslaag van rutheniumoxyde. | |
| GB1290752A (enExample) | ||
| SE7710315L (sv) | Bad for elektropletering av stal | |
| GB1289975A (enExample) | ||
| GB1050172A (enExample) | ||
| IT1078966B (it) | Rivestimenti per conversione di cromo | |
| GB1312375A (en) | Stripping of coated titanium electrodes for re-coating | |
| JPS56166386A (en) | Regeneration method for electrode coated with lead dioxide | |
| GB810818A (en) | Improvements in or relating to processes for electrolytically coating metals with a platinum layer | |
| GB1399500A (en) | Electrolytic deposit of platinum iridium and alloys thereof | |
| GB1470484A (en) | Barrier coated cellulosic substrates | |
| Ohta | Electrophoretic Coating of Boehmite-Coated Aluminum | |
| Ohta | Aluminum Substrates Coating--Electro-Oxidized Substrates Coated With Resins by Electrophoresis | |
| SU827613A1 (ru) | Способ пассивировани цинковой по-ВЕРХНОСТи | |
| GB835091A (en) | Improved method of manufacture of capacitors | |
| Grishchenko et al. | Alumina Coatings Stripping | |
| Semina et al. | Electrochemical and Chemical Behaviour of Zn in HNO sub 3 Solutions: Influence of H exp+ and NO sub 3 exp- Concentrations | |
| GB1068732A (en) | Electrode boiler | |
| ES403824A1 (es) | Procedimiento para aplicar un recubrimiento de un material formador de pelicula sobre la superficie de un metal suscep-tible de ser corroido por acido. | |
| Ohta | Coating Aluminum With Anticorrosive Resin | |
| Brinzoi et al. | Effect of Water Content on the Corrosion of Aluminum and Zirconium in Methanol Solutions | |
| Yakhvarov | The Electrochemical Behaviour of Zirconium in Aqueous and Ethylene Glycol Solutions of Certain Salts\ Halides and Perchlorates\ |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| PS | Patent sealed | ||
| PCNP | Patent ceased through non-payment of renewal fee |