GB1274913A - A method of treating steel - Google Patents
A method of treating steelInfo
- Publication number
- GB1274913A GB1274913A GB2442669A GB2442669A GB1274913A GB 1274913 A GB1274913 A GB 1274913A GB 2442669 A GB2442669 A GB 2442669A GB 2442669 A GB2442669 A GB 2442669A GB 1274913 A GB1274913 A GB 1274913A
- Authority
- GB
- United Kingdom
- Prior art keywords
- ladle
- steel
- oxidizing
- gas
- refractory
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Classifications
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B22—CASTING; POWDER METALLURGY
- B22D—CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES
- B22D1/00—Treatment of fused masses in the ladle or the supply runners before casting
- B22D1/002—Treatment with gases
- B22D1/005—Injection assemblies therefor
Landscapes
- Engineering & Computer Science (AREA)
- Mechanical Engineering (AREA)
- Treatment Of Steel In Its Molten State (AREA)
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP3165468 | 1968-05-13 |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| GB1274913A true GB1274913A (en) | 1972-05-17 |
Family
ID=12337138
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| GB2442669A Expired GB1274913A (en) | 1968-05-13 | 1969-05-13 | A method of treating steel |
Country Status (8)
| Country | Link |
|---|---|
| AT (1) | ATA456169A (enrdf_load_stackoverflow) |
| BE (1) | BE733287A (enrdf_load_stackoverflow) |
| CA (1) | CA941617A (enrdf_load_stackoverflow) |
| DE (1) | DE1924403A1 (enrdf_load_stackoverflow) |
| FR (1) | FR2008406B1 (enrdf_load_stackoverflow) |
| GB (1) | GB1274913A (enrdf_load_stackoverflow) |
| NL (1) | NL6907313A (enrdf_load_stackoverflow) |
| SE (1) | SE391193B (enrdf_load_stackoverflow) |
Family Cites Families (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| BE555593A (enrdf_load_stackoverflow) * | ||||
| FR1129149A (fr) * | 1955-07-18 | 1957-01-16 | Neyrpic Ets | Perfectionnements aux procédés d'insufflation de gaz dans une matière liquide ou dans un mélange de matière liquide et de matière solide |
-
1969
- 1969-05-12 CA CA051,325A patent/CA941617A/en not_active Expired
- 1969-05-13 GB GB2442669A patent/GB1274913A/en not_active Expired
- 1969-05-13 SE SE675869A patent/SE391193B/xx unknown
- 1969-05-13 FR FR6915429A patent/FR2008406B1/fr not_active Expired
- 1969-05-13 DE DE19691924403 patent/DE1924403A1/de active Pending
- 1969-05-13 AT AT456169A patent/ATA456169A/de not_active Application Discontinuation
- 1969-05-13 NL NL6907313A patent/NL6907313A/xx unknown
- 1969-05-20 BE BE733287A patent/BE733287A/xx unknown
Also Published As
| Publication number | Publication date |
|---|---|
| NL6907313A (enrdf_load_stackoverflow) | 1969-11-17 |
| ATA456169A (de) | 1975-04-15 |
| FR2008406A1 (enrdf_load_stackoverflow) | 1970-01-23 |
| DE1924403A1 (de) | 1971-02-04 |
| FR2008406B1 (enrdf_load_stackoverflow) | 1973-05-25 |
| BE733287A (enrdf_load_stackoverflow) | 1969-11-03 |
| CA941617A (en) | 1974-02-12 |
| SE391193B (sv) | 1977-02-07 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| GB1435189A (en) | Process and equipment for blowing fine-grain reagents into steel melts | |
| GB1206062A (en) | Deoxidation method | |
| GB1368881A (en) | Method of treating molten metal | |
| GB1208332A (en) | Method of treating nodular cast iron | |
| GB1389430A (en) | Process for continuous casting of metal bars | |
| FR2045771A7 (en) | Corrosion resistant steel | |
| GB1274913A (en) | A method of treating steel | |
| ES383931A1 (es) | Dispositivo de colada con tubos de colada en instalaciones de colada continua de acero. | |
| GB1268706A (en) | Process for the production of a pig iron with vermicular graphite | |
| ES402610A1 (es) | Procedimiento para la colada continua de un metal fundido. | |
| GB1221618A (en) | Steel refining agent | |
| US2544837A (en) | Apparatus for the continuous formation of metal in sheets | |
| SE8605428L (sv) | Forfarande for efterbehandling av en gjutjernsmelta | |
| Gorobets | Investigation into the Thermodynamics of the De-Oxidation of Iron by a Magnesium Solution | |
| GB1104563A (en) | Improvements in or relating to centrifugal casting of tubular members | |
| FR2086293A1 (fr) | Procede et appareil pour le degazage et la purification de masses metalliques fondues | |
| FR2150591A1 (en) | Cooling of molten metal - by addition of particles of the same metal(s) at a considerably lower temp | |
| GB1362637A (en) | Treating steel in the ladle | |
| GB1258451A (enrdf_load_stackoverflow) | ||
| SU880618A1 (ru) | Промежуточный ковш дл разливки металлов | |
| GB1259702A (en) | Method and apparatus for refining molten iron or molten iron alloys | |
| GB1278624A (en) | Apparatus for the continuous casting of metal | |
| Grevillius et al. | Operational Experience of the ASEA-SKF Ladle Furnace Process at Bofors Steelworks.(Retroactive Coverage) | |
| SU440422A2 (ru) | Способ обработки металлов в вакууме и столбе синтетического шлака | |
| FR2060309A1 (en) | Introduction of additions during steel - casting |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| PS | Patent sealed | ||
| 433D | Application made for revocation (sect. 33/1949) | ||
| 433A | Case decided by the comptroller ** patent amended (sect. 33/1949) | ||
| SPA | Amended specification published | ||
| PCNP | Patent ceased through non-payment of renewal fee |