GB1252062A - - Google Patents
Info
- Publication number
- GB1252062A GB1252062A GB1252062DA GB1252062A GB 1252062 A GB1252062 A GB 1252062A GB 1252062D A GB1252062D A GB 1252062DA GB 1252062 A GB1252062 A GB 1252062A
- Authority
- GB
- United Kingdom
- Prior art keywords
- electrode
- alloy
- welding
- working surface
- coated
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Abstract
1,252,062. Welding by pressure. CENTRE NATIONAL DE RECHERCHES METALLURGIQUES. 18 March, 1969 [21 March, 1968], No. 14033/69. Heading B3R. An electrode for resistance welding comprises a body of high electrical conductivity alloy, i.e. between 50% and 80% of the conductivity of pure copper, coated on its working surface, with a layer of metal or alloy, different from the alloy of the body, of high melting temperature, i.e. above 1000‹ C. The electrode which is for welding galvanized or lead-coated mild steel may be a spot or roller electrode. The body may be of a copper alloy whose conductivity is between 50% and 80% of that of pure copper and the layer may be tungsten, molybdenum or one of their alloys which may be deposited by a plasma torch. The electrode may be a one-piece spot-welding electrode coated on its working surface or may be as shown in the Figure in two parts 3, 4 held together by a threaded ring 5 with the coating 2 over the working surface which, as shown, extends only across part of the width of the part 4 or which may extend across the wide width of the part 4 which is then curved.
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
LU55729 | 1968-03-21 |
Publications (1)
Publication Number | Publication Date |
---|---|
GB1252062A true GB1252062A (en) | 1971-11-03 |
Family
ID=19725547
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
GB1252062D Expired GB1252062A (en) | 1968-03-21 | 1969-03-18 |
Country Status (5)
Country | Link |
---|---|
BE (1) | BE728322A (en) |
DE (1) | DE1914424A1 (en) |
FR (1) | FR2004395A1 (en) |
GB (1) | GB1252062A (en) |
LU (1) | LU55729A1 (en) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
EP0383060A1 (en) * | 1989-02-13 | 1990-08-22 | Krupp Hoesch Stahl AG | Electrode for the resistance welding of coated steel sheets, and method for its production |
Families Citing this family (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
DE2830534C3 (en) * | 1978-07-12 | 1981-01-22 | Pfaff Industriemaschinen Gmbh, 6750 Kaiserslautern | Thread monitors for sewing, embroidery and tufting machines or the like |
EP0019196B1 (en) * | 1979-05-14 | 1983-09-28 | L. SCHULER GmbH | Device for resistance roller seam welding |
HU181132B (en) * | 1980-05-28 | 1983-06-28 | Csepel Muevek Jarmue | Detector pin for sewing machine of short chain stitch |
DE3501387C2 (en) * | 1984-04-06 | 1986-02-20 | Pfaff Industriemaschinen Gmbh, 6750 Kaiserslautern | Thread monitors for sewing, embroidery and tufting machines or the like. |
DE8410845U1 (en) * | 1984-04-06 | 1984-07-05 | Pfaff Industriemaschinen Gmbh, 6750 Kaiserslautern | THREAD GUARD FOR SEWING, EMBROIDERY AND TUFTING MACHINES OD. DGL. |
-
1968
- 1968-03-21 LU LU55729D patent/LU55729A1/xx unknown
-
1969
- 1969-02-12 BE BE728322D patent/BE728322A/xx unknown
- 1969-03-18 GB GB1252062D patent/GB1252062A/en not_active Expired
- 1969-03-20 FR FR6908015A patent/FR2004395A1/fr not_active Withdrawn
- 1969-03-21 DE DE19691914424 patent/DE1914424A1/en active Pending
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
EP0383060A1 (en) * | 1989-02-13 | 1990-08-22 | Krupp Hoesch Stahl AG | Electrode for the resistance welding of coated steel sheets, and method for its production |
Also Published As
Publication number | Publication date |
---|---|
DE1914424A1 (en) | 1969-11-13 |
LU55729A1 (en) | 1969-10-02 |
BE728322A (en) | 1969-08-12 |
FR2004395A1 (en) | 1969-11-21 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
GB1533044A (en) | Hardfacing by welding | |
GB1252062A (en) | ||
GB1481140A (en) | Consumable wire | |
GB1350193A (en) | Sintered metal electrodes | |
GB867917A (en) | Improvements in joining metals or alloys | |
GB1148321A (en) | Cobalt alloy and welding electrode based upon this alloy | |
GB1218662A (en) | Graphite electrodes having an oxidation-resistant surface coating | |
GB1221024A (en) | Device for plasma arc treatment of materials | |
ES313142A2 (en) | Procedure to join aluminum to a metal different like iron, nickel, chrome, copper, zinc or an alloy of two or more of these. (Machine-translation by Google Translate, not legally binding) | |
GB1118339A (en) | Electrode rods for resistance welding of sheets or plated steel | |
GB900337A (en) | Method of producing alloy weld coatings | |
GB830413A (en) | Improvements in or relating to soldering | |
FR2424093A1 (en) | Composite electrode for electric resistance spot welding - where sintered tungsten- copper pad is welded onto working surface of electrode to provide wear resistance | |
JPS5548479A (en) | Arc welding method | |
JPS58141877A (en) | Electrode for welding and brazing | |
GB983063A (en) | Improvements in and relating to method for resistance welding galvanized materials | |
GB1140025A (en) | Improvements in or relating to consumable metal arc welding | |
US3049610A (en) | Electric arc welding method | |
GB912915A (en) | Electric arc welding | |
GB1496744A (en) | Weld metal | |
US2462002A (en) | Cutting tip for cutting tools | |
FR2314016A1 (en) | Submerged arc deposition welding - using two consumable electrodes connected to obtain high deposition rate but very low dilution | |
JPS55120418A (en) | Manufacture of thin diameter steel pipe with inner surface provided with metallic or alloy protective coat | |
GB1208628A (en) | Wheel-type electrode for welding beryllium metal | |
GB1465535A (en) | Spot welding electrodes |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
PS | Patent sealed | ||
PLNP | Patent lapsed through nonpayment of renewal fees |