FR2382969A1 - Procede pour eviter les defauts d'extremite des joints de soudure de tubes - Google Patents
Procede pour eviter les defauts d'extremite des joints de soudure de tubesInfo
- Publication number
- FR2382969A1 FR2382969A1 FR7806767A FR7806767A FR2382969A1 FR 2382969 A1 FR2382969 A1 FR 2382969A1 FR 7806767 A FR7806767 A FR 7806767A FR 7806767 A FR7806767 A FR 7806767A FR 2382969 A1 FR2382969 A1 FR 2382969A1
- Authority
- FR
- France
- Prior art keywords
- procedure
- avoiding end
- end defects
- tube welding
- welding
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
Procédé pour éviter les défauts d'extrémité des joints de soudure de tubes, réalisés au moyen de plusieurs électrodes, notamment sous poudre protectrice, et en particulier à des vitesses de soudure élevées et avec utilisation de pièces de prolongement du joint rapportées avant cintrage. Selon l'invention, ce procédé est caractérisé en ce que, pendant la phase de démarrage de la soudure, la vitesse de soudure est augmentée de façon uniforme ou par paliers de zéro à la valeur nominale, de sorte que la géometrie définitive du joint de soudure soit obtenue avant la transition entre les pièces auxiliaires rapportées et le tuyau. Fabrication de tubes par roulage de tôle et soudage
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
DE2710713A DE2710713C3 (de) | 1977-03-09 | 1977-03-09 | Verfahren zur Vermeidung von Anfangsfehlern beim Mehrdraht-Längsnahtschweißen von Rohren |
Publications (2)
Publication Number | Publication Date |
---|---|
FR2382969A1 true FR2382969A1 (fr) | 1978-10-06 |
FR2382969B1 FR2382969B1 (fr) | 1982-02-19 |
Family
ID=6003407
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
FR7806767A Granted FR2382969A1 (fr) | 1977-03-09 | 1978-03-09 | Procede pour eviter les defauts d'extremite des joints de soudure de tubes |
Country Status (5)
Country | Link |
---|---|
JP (1) | JPS53110950A (fr) |
DE (1) | DE2710713C3 (fr) |
FR (1) | FR2382969A1 (fr) |
GB (1) | GB1597042A (fr) |
IT (1) | IT1093200B (fr) |
Families Citing this family (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS62230478A (ja) * | 1986-03-31 | 1987-10-09 | Sumitomo Metal Ind Ltd | タブ板自動溶接装置 |
US6568077B1 (en) * | 2000-05-11 | 2003-05-27 | General Electric Company | Blisk weld repair |
Citations (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US2564396A (en) * | 1949-11-01 | 1951-08-14 | Republic Steel Corp | Seam welding procedure for pipe manufacture |
DE2609201A1 (de) * | 1976-03-05 | 1977-09-15 | Kobe Steel Ltd | Verfahren zur verhinderung der rissbildung am ende des grundmetalls beim lichtbogenschweissen und dafuer verwendbares endstueck |
-
1977
- 1977-03-09 DE DE2710713A patent/DE2710713C3/de not_active Expired
-
1978
- 1978-02-06 JP JP1224778A patent/JPS53110950A/ja active Pending
- 1978-02-21 GB GB6894/78A patent/GB1597042A/en not_active Expired
- 1978-03-09 IT IT20987/78A patent/IT1093200B/it active
- 1978-03-09 FR FR7806767A patent/FR2382969A1/fr active Granted
Patent Citations (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US2564396A (en) * | 1949-11-01 | 1951-08-14 | Republic Steel Corp | Seam welding procedure for pipe manufacture |
DE2609201A1 (de) * | 1976-03-05 | 1977-09-15 | Kobe Steel Ltd | Verfahren zur verhinderung der rissbildung am ende des grundmetalls beim lichtbogenschweissen und dafuer verwendbares endstueck |
Also Published As
Publication number | Publication date |
---|---|
DE2710713C3 (de) | 1980-12-04 |
GB1597042A (en) | 1981-09-03 |
DE2710713B2 (de) | 1980-03-13 |
JPS53110950A (en) | 1978-09-28 |
FR2382969B1 (fr) | 1982-02-19 |
DE2710713A1 (de) | 1978-09-14 |
IT1093200B (it) | 1985-07-19 |
IT7820987A0 (it) | 1978-03-09 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
NO953752D0 (no) | Fremstilling av metallrör med langsgående sveisesöm | |
FR2382969A1 (fr) | Procede pour eviter les defauts d'extremite des joints de soudure de tubes | |
JPS522825A (en) | Method of manufacturing high tensile seam welded steel tube | |
FR2381589A1 (fr) | Procede pour eliminer les defauts d'extremites dans le soudage a fils multiples du joint longitudinal des tubes | |
US4521669A (en) | Tube-welding auxiliary | |
JPS56151192A (en) | V-groove welded tube | |
JPS5573468A (en) | Butt-welded structure of thin-wall tubular body and welding method thereof | |
JPS53130242A (en) | Welding method for manufacture of thick-walled large diameter welded steel pipe | |
SU841852A1 (ru) | Способ аргонодуговой сварки | |
JPS571596A (en) | Welding method of pipe and welding fitting used therefor | |
SU479578A1 (ru) | Способ заварки кратеров при дуговой сварке изделий конечной длины | |
JPS5545572A (en) | Welding method | |
JPH01192476A (ja) | 溶接鋼管の製造方法 | |
JPS5478340A (en) | Butt welding method for aluminum clad steel | |
CA2185996A1 (fr) | Procede d'attenuation des contraintes residuelles des composants metalliques soudes grace a un deplacement rapide de la torche de soudure | |
SU105861A1 (ru) | Способ сварки продольного шва труб | |
GB819390A (en) | Welded joint for steel tubes | |
SU1464617A2 (ru) | Способ нанесени покрыти на внутреннюю поверхность трубы | |
SU1729715A1 (ru) | Способ контактной стыковой сварки оплавлением | |
GB190922078A (en) | Improvements in the Manufacture of Metallic Tubes. | |
Sato et al. | Size Effects of Tensile Specimen on Strength of Butt-Welded Joints Having Soft Weld Metal | |
JPH0947878A (ja) | ステンレス鋼管の仮付け溶接方法 | |
JPS53116264A (en) | Tack welding method for seam of steel pipe | |
JPS5493652A (en) | Method and apparatus for manufacture of crossed pipe parts | |
RU1812026C (ru) | Способ производства сварных пр мошовных труб большого диаметра |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
ST | Notification of lapse |