FR2337606A1 - Arc welding under water or at elevated pressure - in an atmosphere of controlled composition to produce high quality welds - Google Patents
Arc welding under water or at elevated pressure - in an atmosphere of controlled composition to produce high quality weldsInfo
- Publication number
- FR2337606A1 FR2337606A1 FR7700595A FR7700595A FR2337606A1 FR 2337606 A1 FR2337606 A1 FR 2337606A1 FR 7700595 A FR7700595 A FR 7700595A FR 7700595 A FR7700595 A FR 7700595A FR 2337606 A1 FR2337606 A1 FR 2337606A1
- Authority
- FR
- France
- Prior art keywords
- under water
- atmosphere
- arc welding
- high quality
- produce high
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Withdrawn
Abstract
In the welding process, a chamber around the workpiece is filled with gas, and a welding rod with a flux core with >=1 strong de-oxidiser is used. An arc zone between the rod and the workpiece is screened by a gas mixt. with >=1 inert gas and oxygen and/or an oxygen-contg. gas. This is split to form free oxygen in the arc or reacts with the de-oxidiser. Method is used for arc welding under water or where the pressure is higher than atmospheric. The weld quantity is good and the weld is clearly visible during the work.
Applications Claiming Priority (2)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
GB107876 | 1976-01-12 | ||
GB9245/76A GB1539917A (en) | 1976-03-08 | 1976-03-08 | Methods of arc welding in a super-atmospheric environment |
Publications (1)
Publication Number | Publication Date |
---|---|
FR2337606A1 true FR2337606A1 (en) | 1977-08-05 |
Family
ID=26236433
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
FR7700595A Withdrawn FR2337606A1 (en) | 1976-01-12 | 1977-01-11 | Arc welding under water or at elevated pressure - in an atmosphere of controlled composition to produce high quality welds |
Country Status (15)
Country | Link |
---|---|
JP (1) | JPS52151649A (en) |
AU (1) | AU510031B2 (en) |
BR (1) | BR7700175A (en) |
DK (1) | DK9677A (en) |
EG (1) | EG13307A (en) |
ES (1) | ES454942A1 (en) |
FR (1) | FR2337606A1 (en) |
IE (1) | IE44577B1 (en) |
IN (1) | IN146110B (en) |
IT (1) | IT1075055B (en) |
MX (1) | MX144601A (en) |
NL (1) | NL7700275A (en) |
NO (1) | NO144874C (en) |
NZ (1) | NZ182982A (en) |
OA (1) | OA05543A (en) |
Cited By (7)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
FR2382968A2 (en) * | 1977-03-07 | 1978-10-06 | Boc Ltd | PROCESS OF ARC WELDING UNDER WATER OR UNDER PRESSURE EXCEEDING THAN ATMOSPHERE |
DE2836983A1 (en) * | 1977-04-05 | 1980-03-13 | Welding Inst | METHOD AND DEVICE FOR WELDING UNDER PRESSURE |
FR2434000A1 (en) * | 1977-04-05 | 1980-03-21 | Welding Inst | MIG welding at high pressure with electrode negative w.r.t. workpiece - e.g. underwater pipeline, using small dia. electrode wire and increased power supply slope |
WO2001007753A1 (en) * | 1999-07-27 | 2001-02-01 | Shell Internationale Research Maatschappij B.V. | Method of creating a weld in a wellbore |
US6460618B1 (en) | 1999-11-29 | 2002-10-08 | Shell Oil Company | Method and apparatus for improving the permeability in an earth formation utilizing shock waves |
AU763587B2 (en) * | 1999-07-27 | 2003-07-24 | Shell Internationale Research Maatschappij B.V. | Method of creating a weld in a wellbore |
WO2024153623A1 (en) * | 2023-01-17 | 2024-07-25 | Fronius International Gmbh | Method and device for welding workpieces in a protective gas chamber |
Families Citing this family (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
NZ182982A (en) * | 1976-01-12 | 1979-10-25 | Boc Ltd | Arc welding under water |
JPS5628806U (en) * | 1979-08-07 | 1981-03-18 | ||
JPS5636374A (en) * | 1979-08-29 | 1981-04-09 | Kawasaki Heavy Ind Ltd | Underwater dry type welding equipment |
JP2013230486A (en) * | 2012-04-27 | 2013-11-14 | Mitsubishi Heavy Ind Ltd | Welding device |
Citations (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
FR2164966A5 (en) * | 1971-12-13 | 1973-08-03 | Anna Welding Corp | Underwater arc welding - high pressure gas envelope for preventing water entering arc and weld |
US3794804A (en) * | 1969-11-13 | 1974-02-26 | Anna Welding Corp | Method for underwater arc welding |
NL7611234A (en) * | 1975-10-10 | 1977-04-13 | British Oxygen Co Ltd | PROCEDURE FOR ARC WELDING UNDER WATER. |
NL7700275A (en) * | 1976-01-12 | 1977-07-14 | British Oxygen Co Ltd | WELDING METHOD. |
Family Cites Families (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5038372B2 (en) * | 1972-03-15 | 1975-12-09 | ||
US3876852A (en) * | 1973-04-25 | 1975-04-08 | Hydro Tech International Inc | Method and apparatus for underwater welding |
-
1976
- 1976-12-23 NZ NZ182982A patent/NZ182982A/en unknown
- 1976-12-24 IN IN2262/CAL/76A patent/IN146110B/en unknown
-
1977
- 1977-01-05 EG EG6/77A patent/EG13307A/en active
- 1977-01-06 AU AU21092/77A patent/AU510031B2/en not_active Expired
- 1977-01-07 NO NO770054A patent/NO144874C/en unknown
- 1977-01-07 MX MX167624A patent/MX144601A/en unknown
- 1977-01-11 DK DK9677A patent/DK9677A/en not_active Application Discontinuation
- 1977-01-11 FR FR7700595A patent/FR2337606A1/en not_active Withdrawn
- 1977-01-11 IT IT19167/77A patent/IT1075055B/en active
- 1977-01-11 BR BR7700175A patent/BR7700175A/en unknown
- 1977-01-11 ES ES454942A patent/ES454942A1/en not_active Expired
- 1977-01-11 JP JP185077A patent/JPS52151649A/en active Pending
- 1977-01-12 OA OA56045A patent/OA05543A/en unknown
- 1977-01-12 IE IE56/77A patent/IE44577B1/en unknown
- 1977-01-12 NL NL7700275A patent/NL7700275A/en not_active Application Discontinuation
Patent Citations (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US3794804A (en) * | 1969-11-13 | 1974-02-26 | Anna Welding Corp | Method for underwater arc welding |
FR2164966A5 (en) * | 1971-12-13 | 1973-08-03 | Anna Welding Corp | Underwater arc welding - high pressure gas envelope for preventing water entering arc and weld |
NL7611234A (en) * | 1975-10-10 | 1977-04-13 | British Oxygen Co Ltd | PROCEDURE FOR ARC WELDING UNDER WATER. |
NL7700275A (en) * | 1976-01-12 | 1977-07-14 | British Oxygen Co Ltd | WELDING METHOD. |
Cited By (7)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
FR2382968A2 (en) * | 1977-03-07 | 1978-10-06 | Boc Ltd | PROCESS OF ARC WELDING UNDER WATER OR UNDER PRESSURE EXCEEDING THAN ATMOSPHERE |
DE2836983A1 (en) * | 1977-04-05 | 1980-03-13 | Welding Inst | METHOD AND DEVICE FOR WELDING UNDER PRESSURE |
FR2434000A1 (en) * | 1977-04-05 | 1980-03-21 | Welding Inst | MIG welding at high pressure with electrode negative w.r.t. workpiece - e.g. underwater pipeline, using small dia. electrode wire and increased power supply slope |
WO2001007753A1 (en) * | 1999-07-27 | 2001-02-01 | Shell Internationale Research Maatschappij B.V. | Method of creating a weld in a wellbore |
AU763587B2 (en) * | 1999-07-27 | 2003-07-24 | Shell Internationale Research Maatschappij B.V. | Method of creating a weld in a wellbore |
US6460618B1 (en) | 1999-11-29 | 2002-10-08 | Shell Oil Company | Method and apparatus for improving the permeability in an earth formation utilizing shock waves |
WO2024153623A1 (en) * | 2023-01-17 | 2024-07-25 | Fronius International Gmbh | Method and device for welding workpieces in a protective gas chamber |
Also Published As
Publication number | Publication date |
---|---|
BR7700175A (en) | 1977-09-06 |
OA05543A (en) | 1981-04-30 |
MX144601A (en) | 1981-10-29 |
AU510031B2 (en) | 1980-06-05 |
NL7700275A (en) | 1977-07-14 |
NO144874C (en) | 1981-12-02 |
JPS52151649A (en) | 1977-12-16 |
NO770054L (en) | 1977-07-13 |
EG13307A (en) | 1982-03-31 |
ES454942A1 (en) | 1977-12-01 |
NO144874B (en) | 1981-08-24 |
IN146110B (en) | 1979-02-24 |
IE44577B1 (en) | 1982-01-13 |
AU2109277A (en) | 1978-07-13 |
IT1075055B (en) | 1985-04-22 |
NZ182982A (en) | 1979-10-25 |
DK9677A (en) | 1977-07-13 |
IE44577L (en) | 1977-07-12 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS558308A (en) | Welding method for forming thick walled steel pipe | |
NZ511355A (en) | Laser/arc hybrid welding process with an argon/helium gas mixture | |
FR2337606A1 (en) | Arc welding under water or at elevated pressure - in an atmosphere of controlled composition to produce high quality welds | |
SE8304232D0 (en) | WELDING METHOD | |
KR940003652A (en) | Shielding gas for arc welding | |
JPS5527417A (en) | Vertical downward build-up welding method | |
GB1460140A (en) | Weld shielding gas containing sulphur hexafluoride | |
US4929812A (en) | Method for electrical arc spot welding with consumable electrode | |
JPS53113734A (en) | One-side arc welding method for 9% ni steel | |
JPS53130241A (en) | Welding method for manufacture of thick walled steel pipe | |
JPS5577992A (en) | Electrogas arc welding method | |
JPS5781995A (en) | Steel wire for gas shielded arc welding | |
JPS6462277A (en) | Method for welding metal chromium | |
JPS53106361A (en) | Submerged arc welding method for steel plate | |
JPS53137043A (en) | Inert gas arc welding method for steel for low temperature use | |
Kuwana et al. | Nitrogen Absorption of Iron Weld Metal in Gas Tungsten Arc Welding | |
JPS56158295A (en) | Electrode for welding excellent in arc stability | |
JPS54133445A (en) | Arc welding method for high tension steel | |
JPS57209778A (en) | Gas shielded arc welding method | |
JPS5471739A (en) | Crater treating method for inert-gas arc welding | |
JPS6457979A (en) | Mag welding method | |
FR2434000A1 (en) | MIG welding at high pressure with electrode negative w.r.t. workpiece - e.g. underwater pipeline, using small dia. electrode wire and increased power supply slope | |
JPS5395850A (en) | Multiple wire submerged arc welding method | |
GB751558A (en) | Improvements in electric arc welding | |
GB2002276A (en) | Welding at pressures greater than atmospheric pressures |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
ST | Notification of lapse |