DE68927974T2 - Verfahren zur Unterdrückung der Bildung von Polymerkrusten - Google Patents
Verfahren zur Unterdrückung der Bildung von PolymerkrustenInfo
- Publication number
- DE68927974T2 DE68927974T2 DE68927974T DE68927974T DE68927974T2 DE 68927974 T2 DE68927974 T2 DE 68927974T2 DE 68927974 T DE68927974 T DE 68927974T DE 68927974 T DE68927974 T DE 68927974T DE 68927974 T2 DE68927974 T2 DE 68927974T2
- Authority
- DE
- Germany
- Prior art keywords
- suppressing
- formation
- polymer crusts
- crusts
- polymer
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C08—ORGANIC MACROMOLECULAR COMPOUNDS; THEIR PREPARATION OR CHEMICAL WORKING-UP; COMPOSITIONS BASED THEREON
- C08F—MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08F2/00—Processes of polymerisation
- C08F2/002—Scale prevention in a polymerisation reactor or its auxiliary parts
- C08F2/004—Scale prevention in a polymerisation reactor or its auxiliary parts by a prior coating on the reactor walls
Landscapes
- Chemical & Material Sciences (AREA)
- Health & Medical Sciences (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Medicinal Chemistry (AREA)
- Polymers & Plastics (AREA)
- Organic Chemistry (AREA)
- Polymerisation Methods In General (AREA)
Applications Claiming Priority (3)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP30941588A JPH0617366B2 (ja) | 1988-12-07 | 1988-12-07 | 重合体スケールの付着防止方法 |
JP31160188A JPH0617367B2 (ja) | 1988-12-09 | 1988-12-09 | 重合体スケールの付着防止方法 |
JP63311602A JPH0676443B2 (ja) | 1988-12-09 | 1988-12-09 | 重合体スケールの付着防止方法 |
Publications (2)
Publication Number | Publication Date |
---|---|
DE68927974D1 DE68927974D1 (de) | 1997-05-22 |
DE68927974T2 true DE68927974T2 (de) | 1997-11-27 |
Family
ID=27339040
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
DE68927974T Expired - Fee Related DE68927974T2 (de) | 1988-12-07 | 1989-12-07 | Verfahren zur Unterdrückung der Bildung von Polymerkrusten |
Country Status (3)
Country | Link |
---|---|
US (1) | US5053466A (de) |
EP (1) | EP0372967B1 (de) |
DE (1) | DE68927974T2 (de) |
Families Citing this family (12)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH04320402A (ja) * | 1991-04-19 | 1992-11-11 | Shin Etsu Chem Co Ltd | 重合体スケール付着防止剤および重合体スケールの付着防止方法 |
US5442017A (en) * | 1991-09-24 | 1995-08-15 | Shin-Etsu Chemical Co., Ltd. | Process for producing polymer wherein polymer scale deposition is prevented |
DE69217327D1 (de) * | 1991-10-21 | 1997-03-20 | Shinetsu Chemical Co | Mittel zur Verhinderung von Polymerverkrustung, Polymerisationsgefäss, in dem die Verkrustung vermieden wird und Verfahren zur Herstellung von Polymeren unter Benutzung dieses Gefässes |
EP0538801A1 (de) * | 1991-10-21 | 1993-04-28 | Shin-Etsu Chemical Co., Ltd. | Mittel zur Verhinderung von Polymerverkrustung, Polymerisationsgefäss, in dem die Verkrustung vermieden wird und Verfahren zur Herstellung von Polymeren unter Benutzung dieses Gefässes |
US5424377A (en) * | 1992-12-30 | 1995-06-13 | Shin-Etsu Chemical Co., Ltd. | Process to prevent scale adhesion using condensation product of aromatic amine and a quinone |
US5442002A (en) * | 1993-07-22 | 1995-08-15 | Shin-Etsu Chemical Co., Ltd. | Polymer scale deposition preventive agent |
JP3317803B2 (ja) * | 1994-11-15 | 2002-08-26 | 信越化学工業株式会社 | 重合体スケール付着防止剤及びそれを使用する重合体製造方法 |
US5958301A (en) * | 1996-09-27 | 1999-09-28 | International Business Machines Corporation | Methods of fabricating branched electrially conductive polymers and precursors thereof |
US6241913B1 (en) * | 1996-09-27 | 2001-06-05 | International Business Machines Corporation | Branched electrically conductive polymers and precursors and applications thereof |
US6235348B1 (en) * | 1998-05-13 | 2001-05-22 | Shin-Etsu Chemical Co., Ltd. | Rust prevention |
JP3974882B2 (ja) * | 2003-08-07 | 2007-09-12 | 信越化学工業株式会社 | 重合体スケール付着防止剤 |
EP1514878B1 (de) * | 2003-09-05 | 2012-05-02 | Shin-Etsu Chemical Co., Ltd. | Polymerablagerungsinhibitor |
Family Cites Families (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5223187A (en) * | 1975-08-14 | 1977-02-21 | Shin Etsu Chem Co Ltd | Process for polymerizing vinyl monomers |
JPS58101103A (ja) * | 1981-12-11 | 1983-06-16 | Shin Etsu Chem Co Ltd | ビニル系単量体の重合方法 |
JPS58210902A (ja) * | 1982-05-31 | 1983-12-08 | Shin Etsu Chem Co Ltd | ビニル系単量体の重合方法 |
JPS6072902A (ja) * | 1983-09-30 | 1985-04-25 | Shin Etsu Chem Co Ltd | 重合体スケ−ル付着防止方法および重合体スケ−ル付着防止剤 |
-
1989
- 1989-12-06 US US07/446,681 patent/US5053466A/en not_active Expired - Fee Related
- 1989-12-07 EP EP89312778A patent/EP0372967B1/de not_active Expired - Lifetime
- 1989-12-07 DE DE68927974T patent/DE68927974T2/de not_active Expired - Fee Related
Also Published As
Publication number | Publication date |
---|---|
EP0372967A2 (de) | 1990-06-13 |
EP0372967B1 (de) | 1997-04-16 |
DE68927974D1 (de) | 1997-05-22 |
EP0372967A3 (de) | 1991-10-23 |
US5053466A (en) | 1991-10-01 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
DE3888928T2 (de) | Verfahren zur Unterdrückung der Bildung von Polymerkrusten. | |
DE69028152D1 (de) | Verfahren zur Herstellung von Polycarbonat-Polysiloxan-Blockcopolymeren | |
DE69307472T2 (de) | Verfahren zur Herstellung von Alpha-Olefinpolymeren | |
PT80641B (de) | Verfahren zur herstellung von dialkoxypyridinen | |
DE69116182D1 (de) | Verfahren zur Herstellung von alpha-Olefinpolymeren | |
DE3683466D1 (de) | Verfahren zur kontinuierlichen herstellung von propylen-ethylen-blockcopolymeren. | |
AT385282B (de) | Verfahren zur kontinuierlichen herstellung von aethanol | |
DE3578938D1 (de) | Verfahren zur modifizierung der oberflaeche von polymermaterialien. | |
DE69316271D1 (de) | Verfahren zur Herstellung von Alpha-Olefinpolymeren | |
DE68927974T2 (de) | Verfahren zur Unterdrückung der Bildung von Polymerkrusten | |
DE3751734D1 (de) | Verfahren zur Herstellung von alpha-Olefin-Blockcopolymeren | |
DE3581204D1 (de) | Verfahren zur polymerisation von buten-1. | |
DE3678637D1 (de) | Verfahren zur verbesserung der reinheit von propylenpolymeren. | |
DE68919193D1 (de) | Verfahren zur Unterdrückung der Bildung von Polymerkrusten. | |
DE68919163D1 (de) | Verfahren zur Unterdrückung der Bildung von Polymerkrusten. | |
DE68924572T2 (de) | Verfahren zur Unterdrückung der Bildung von Polymerkrusten. | |
DE69026611T2 (de) | Verfahren zur Bestimmung von Fruktosaminen | |
DE69114387D1 (de) | Verfahren zur Unterdrückung der Bildung von Polymerkrusten. | |
DE69112138T2 (de) | Zusammensetzung zur Unterdrückung der Bildung von Polymerkrusten und ein Verfahren dazu. | |
DE69313863T2 (de) | Verfahren zur herstellung von sulfonaten | |
DE69014661D1 (de) | Verfahren zur Unterdrückung der Bildung von Polymerkrusten. | |
DE68927119T2 (de) | Verfahren zur Herstellung von 4-Hydroxypyrimidin | |
AT381929B (de) | Verfahren zur herstellung von succinylobernstein- saeuredialkylestern | |
DE3990925T1 (de) | Verfahren zur herstellung/renovierung von fenstern | |
DE69021059D1 (de) | Verfahren zur Unterdrückung der Bildung von Polymerkrusten. |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
8364 | No opposition during term of opposition | ||
8339 | Ceased/non-payment of the annual fee |