CN2699103Y - 一种短骨架塑料复合电熔套筒 - Google Patents

一种短骨架塑料复合电熔套筒 Download PDF

Info

Publication number
CN2699103Y
CN2699103Y CN 200420059787 CN200420059787U CN2699103Y CN 2699103 Y CN2699103 Y CN 2699103Y CN 200420059787 CN200420059787 CN 200420059787 CN 200420059787 U CN200420059787 U CN 200420059787U CN 2699103 Y CN2699103 Y CN 2699103Y
Authority
CN
China
Prior art keywords
skeleton
plastic composite
composite electric
electric melting
length
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 200420059787
Other languages
English (en)
Inventor
林宝清
张伟
张作军
王学钢
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
DAQING OIL FIELD CHANGYUAN PIPE INDUSTRY Co Ltd
Original Assignee
DAQING OIL FIELD CHANGYUAN PIPE INDUSTRY Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by DAQING OIL FIELD CHANGYUAN PIPE INDUSTRY Co Ltd filed Critical DAQING OIL FIELD CHANGYUAN PIPE INDUSTRY Co Ltd
Priority to CN 200420059787 priority Critical patent/CN2699103Y/zh
Application granted granted Critical
Publication of CN2699103Y publication Critical patent/CN2699103Y/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型涉及一种短骨架塑料复合电熔套筒。主要解决现有的骨架塑料复合电熔套筒在塑料管材焊接时效果差及质量不稳定的问题。其特征在于:筒形骨架(2)的侧壁均匀开有通孔,骨架(2)长度为筒体(1)长度的2/5~3/5。该短骨架塑料复合电熔套筒在管材焊接时,熔池压力低,焊接效果好及质量稳定。

Description

一种短骨架塑料复合电熔套筒
技术领域:
本实用新型涉及一种输送工业用水、石油、燃气等介质的塑料复合管所用的接头,属于一种短骨架塑料复合电熔套筒。
背景技术:
塑料复合管广泛应用于石油、化工、煤炭、冶金、火力发电、制药及市政建设等行业和领域,在施工中为了达到塑料复合管长距离输送的目的,塑料复合管之间需用电熔套筒连接为一体,通过套筒内壁预埋的电熔线加热塑料复合管,在套筒内将两塑料管熔焊成为一体。而现有的塑料复合电熔套筒中的骨架,其轴向长度与电熔套筒轴向长度大体相当,这种套筒在管材焊接时,熔池压力过高,冷却时不能及时充分补塑,常产生焊接冒料、内壁塌陷、焊接面有收缩气孔等现象,焊接质量不稳定。
实用新型内容:
为了克服现有的骨架塑料复合电熔套筒在塑料管材焊接时效果差及质量不稳定的不足,本实用新型提供一种短骨架塑料复合电熔套筒,该短骨架塑料复合电熔套筒在管材焊接时,熔池压力低,管材焊接效果好及质量稳定。
本实用新型的技术方案是:该短骨架塑料复合电熔套筒包括筒体,筒体内置有骨架,筒形骨架的侧壁均匀开有通孔,骨架长度为筒体长度的2/5~3/5。
上述的骨架长度为筒体长度的1/2;骨架的材质为钢。
本实用新型具有的有益效果是:该复合电熔套筒的筒体内固定开有均匀孔的钢质筒形骨架,骨架长度为筒体长度的2/5~3/5,由于骨架的筒壁开有均匀孔及其长度短,所以熔池压力低,冷却时能及时充分补塑,不会产生焊接冒料、内壁塌陷、焊接面有收缩气孔等现象,焊接效果好及质量稳定。并且产品重量轻、结构简单及制造成本低。
附图说明:
附图1是本实用新型结构剖视图。
图中1-筒体,2-骨架。
具体实施方式:
下面结合附图将对本实用新型作进一步说明:
由图1所示,该短骨架塑料复合电熔套筒包括筒体1,筒体1内固定有骨架2,骨架2由钢板均匀冲孔卷筒焊接而成,并与热塑性塑料复合成筒体1,骨架2长度为筒体1长度的2/5~3/5,其优选长度为筒体1长度的1/2。由于骨架的筒壁开有均匀孔及其长度短,所以熔池压力低,冷却时能及时充分补塑,不会产生焊接冒料、内壁塌陷、焊接面有收缩气孔等现象,焊接效果好及质量稳定。并且产品重量轻、结构简单及制造成本低。

Claims (3)

1、一种短骨架塑料复合电熔套筒,包括筒体(1),筒体(1)内置有骨架(2),其特征在于:筒形骨架(2)的侧壁均匀开有通孔,骨架(2)长度为筒体(1)长度的2/5~3/5。
2、根据权利要求1所述的短骨架塑料复合电熔套筒,其特征在于:骨架(2)长度为筒体(1)长度的1/2为优选长度。
3、根据权利要求1或2所述的短骨架塑料复合电熔套筒,其特征在于:骨架(2)的材质为钢。
CN 200420059787 2004-05-24 2004-05-24 一种短骨架塑料复合电熔套筒 Expired - Fee Related CN2699103Y (zh)