CN2319166Y - 耐腐蚀的钢芯镀铜焊丝 - Google Patents
耐腐蚀的钢芯镀铜焊丝 Download PDFInfo
- Publication number
- CN2319166Y CN2319166Y CN 98228059 CN98228059U CN2319166Y CN 2319166 Y CN2319166 Y CN 2319166Y CN 98228059 CN98228059 CN 98228059 CN 98228059 U CN98228059 U CN 98228059U CN 2319166 Y CN2319166 Y CN 2319166Y
- Authority
- CN
- China
- Prior art keywords
- copper
- steel core
- welding wire
- protection structure
- outside
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型涉及的是一种耐腐蚀的钢芯镀铜焊丝,在钢芯外镀有铜保护层,在接近焊丝的端部处的镀铜层之外设置有能与该镀铜层相接触的阳极保护结构,该阳极保护结构由标准电极电位低于铜的金属材料构成。
Description
本实用新型涉及的是一种对使用于二氧化碳气体保护焊等焊接方法中的钢芯镀铜焊丝的改进,以提高其抗腐蚀的能力。
二氧化碳气体保护焊可保证和提高焊接质量。目前其所用的焊丝通常都是在铜芯外镀覆有铜保护层的钢芯镀铜焊丝,其铜质镀层的作用既可提高导电性,又可防止钢芯被锈蚀。但实践中发现,这种焊丝的铜质镀层仍会受大气腐蚀等作用的影响而被破坏,因此这种镀铜焊丝的保存期仍较短而不理想。特别是在气候潮湿及靠近海洋的地区,这种腐蚀现象就更为迅速,严重影响了钢芯镀铜焊丝的保存和使用性能。为此,目前国内外一般都是从提高镀铜质量和提高包装的密封干燥效果上着手解决,以期达到延长其保质期限的目的,但实际表明效果有限。尤其是在包装被打开后,焊丝即直接与大气接触,保质期便急剧缩短。
本实用新型的目的是针对上述情况,提供一种能大大提高这种钢芯镀铜焊丝抗腐蚀能力,可成倍延长其保质期限的耐腐蚀钢芯镀铜焊丝。
本实用新型的耐腐蚀的钢芯镀铜焊丝,在钢芯外同样镀有铜保护层。在接近焊丝的端部处的镀铜层之外设置有能与该镀铜层相接触的阳极保护结构,该阳极保护结构可由标准电极电位低于铜的金属材料构成,如常见的锰、镁、锌、钒等金属材料或是其各种形式的合金材料。所说的该阳极保护结构的设置,在保证其与镀铜层可靠紧密接触的前提下,可以采用各种简单方便和可行的方式,如,可以为包覆于镀铜层之外的镀层形式,或是为包夹于镀铜层之外的结构层等不同形式。根据电化学的原理,当焊丝外表的铜镀层与标准电极电位比其低的金属材料接触后,在发生电化学反应时,首先是低电极电位的该阳极保护材料进行反应而被腐蚀。因此,只有当该阳极保护材料被腐蚀完后,铜镀层才会开始被腐蚀。根据不同地区的大气腐蚀情况,选择适当的阳极保护材料和/或阳极保护材料的用量,就可以有效地避免焊丝的镀铜外层被腐蚀。试验表明,在同样具有较大腐蚀情况的地区,这种设置有阳极保护材料的钢芯镀铜焊丝与目前普通镀铜焊丝相比,保质期限可成倍地提高,说明了这种在焊丝外表设置牺牲阳极结构的方式提高焊丝的抗腐蚀性能是成功和有效的,而所花费的成本却十分低廉。
以下用附图所示的实例对本实用新型的上述内容作进一步说明。但不应将此理解为本实用新型上述主题的范围仅限于下述的实例。
图1:本实用新型耐腐蚀钢芯镀铜焊丝的结构
如图所示,本耐腐蚀钢芯镀铜焊丝中,在钢芯1外镀有铜保护层2。在接近焊丝端部部位处的镀铜层2之外,设置有能与该镀铜层2保持紧密接触的阳极保护结构3,该阳极保护结构由标准电极电位低于铜的锰、镁、锌、钒等金属材料或其合金材料构成。该阳极保护结构3的设置方式,可采用包覆于镀铜层2之外的镀层形式,也可以采用包夹于镀铜层2之外的结构形式。
Claims (3)
1.一种耐腐蚀的钢芯镀铜焊丝,在钢芯外镀有铜保护层,其特征在于在接近焊丝的端部处的镀铜层之外设置有能与该镀铜层(2)相接触的阳极保护结构(3),该阳极保护结构由标准电极电位低于铜的金属材料构成。
2.如权利要求1所述的焊丝,其特征在于所说的阳极保护结构(3)为包覆于镀铜层(2)之外的镀层形式。
3.如权利要求1所述的焊丝,其特征在于所说的阳极保护结构(3)为包夹于镀铜层(2)之外的结构形式。