CN2300464Y CN 97238779 CN97238779U CN2300464Y CN 2300464 Y CN2300464 Y CN 2300464Y CN 97238779 CN97238779 CN 97238779 CN 97238779 U CN97238779 U CN 97238779U CN 2300464 Y CN2300464 Y CN 2300464Y
Authority
CN
China
Prior art keywords
copper tube
copper pipe
opening part
upper opening
crystallizer
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 97238779
Other languages
English (en)
Inventor
桂源
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN 97238779 priority Critical patent/CN2300464Y/zh
Application granted granted Critical
Publication of CN2300464Y publication Critical patent/CN2300464Y/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Links

Landscapes

  • Continuous Casting (AREA)

Abstract

本实用新型公开了一种用于方坯连铸设备中的结晶器铜管,其上、下口部位分别为端面密封和周边密封方式,铜管外表的四个面纵向布有波纹槽,铜管的上口部位具有定位止口,从而较好地解决了整体均匀性冷却和铜管上口部位易变形的问题,可大大延长铜管使用寿命和提高拉坯速度。

Description

一种结晶器铜管
一种涉及方坯连铸设备用的结晶器铜管。
钢水在结晶器铜管内连续结晶而形成钢坯,现有方坯连铸设备使用的结晶器铜管,钢水注入后,通过铜管壁传热冷却,钢水即开始冷凝形成薄壳,由于铜管四角与四个外表面冷却不均匀,铜管的上口部位变形,形成气隙而阻碍热的传导,因此直接影响连铸设备拉坯速度和铜管本身的使用寿命。
本实用新型的目的是针对上述缺陷和问题,而提供一种具有冷却均匀,能延长使用寿命,且有利于提高拉坯速度的结晶器铜管。
为实现上述目的,本实用新型的结晶器铜管,其上、下口部位分别采用端面密封和周边密封。为解决冷却的均匀性,铜管外表的四个面沿纵向布有波纹槽,这种形式最大限度地增加了热传导面积,波纹槽又便于水的分流。铜管的上口部位设置有定位止口,以实现润滑法兰与铜管的配合联接,防止拉坯时铜管变形。
采用这种结构形式的结晶器铜管,具有的显著优点是:
1、有利于整体的热传导平衡,铜管角部与外表处的钢水能均匀凝固,从而大大提高了冷却效果,并且大幅度提高了拉坯速度和铸坯质量。
2、由于铜管上口部位设置有定位止口,润滑法兰与铜管配合联接后,具有可靠的密封性,从而可防止铜管上口部位的变形,有利于延长铜管使用寿命和提高拉坯速度。
图1是本实用新型的主视图;
图2为图1的左视图;
图3为图1横截面剖视图。
实施例:如图1-3所示,本实施例的结晶器铜管1经由模具挤压、加工成,其上口部位为端面密封方式,下口部位为周边密封,以满足铜管1工作中自由伸缩的要求。铜管外表的四个面沿纵向布有波纹槽2,铜管1上口部位有定位止口3。

Claims (1)

1、一种方坯连铸设备用的结晶器铜管,其上、下口部位分别为端面密封和周边密封,其特征在于:铜管(1)外表的四个面纵向布有波纹槽(2),铜管(1)上口部位有定位止口(3)。
CN 97238779 1997-08-20 1997-08-20 一种结晶器铜管 Expired - Fee Related CN2300464Y (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN 97238779 CN2300464Y (zh) 1997-08-20 1997-08-20 一种结晶器铜管

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN 97238779 CN2300464Y (zh) 1997-08-20 1997-08-20 一种结晶器铜管

Publications (1)

Publication Number Publication Date
CN2300464Y true CN2300464Y (zh) 1998-12-16

Family

ID=33948993

Family Applications (1)

Application Number Title Priority Date Filing Date
CN 97238779 Expired - Fee Related CN2300464Y (zh) 1997-08-20 1997-08-20 一种结晶器铜管

Country Status (1)

Country Link
CN (1) CN2300464Y (zh)

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN100344394C (zh) * 2003-04-16 2007-10-24 康卡斯特股份公司 用于连铸的管形锭模
CN104858378A (zh) * 2015-06-15 2015-08-26 大连华锐重工集团股份有限公司 直口阶梯曲线带铣槽式结晶器铜管及结晶器
CN109822065A (zh) * 2019-04-11 2019-05-31 安徽工业大学 一种连铸结晶器的宽面铜板及具有该铜板的连铸结晶器

Cited By (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN100344394C (zh) * 2003-04-16 2007-10-24 康卡斯特股份公司 用于连铸的管形锭模
CN104858378A (zh) * 2015-06-15 2015-08-26 大连华锐重工集团股份有限公司 直口阶梯曲线带铣槽式结晶器铜管及结晶器
CN109822065A (zh) * 2019-04-11 2019-05-31 安徽工业大学 一种连铸结晶器的宽面铜板及具有该铜板的连铸结晶器
CN109822065B (zh) * 2019-04-11 2024-03-22 安徽工业大学 一种连铸结晶器的宽面铜板及具有该铜板的连铸结晶器

Similar Documents

Publication Publication Date Title
CN2300464Y (zh) 一种结晶器铜管
CN101696848B (zh) 一种带保温装置的水内冷输送板坯辊道
CA2247785A1 (en) Molds for a continuous casting system
CN100574937C (zh) 一种金属复合管坯的制造方法和制造金属复合管坯的装置
CN206839072U (zh) 一种铝锭冷却装置
CN210172516U (zh) 一种生产方型真空锭用工模具
CN2652559Y (zh) 一种炼钢连铸用均匀冷却高效结晶器
CN1621179A (zh) 铝合金气膜连续铸造结晶器
CN111644827A (zh) 一种水循环冷却玻璃瓶罐模具及其加工方法
CN2338546Y (zh) 无水耐高温阀门
CN214133846U (zh) 一种合金砂浆泵铸造模具
CN110076327A (zh) 一种带有冷却系统的奥贝磨球成型模具
CN212371144U (zh) 一种镶拼式压铸模冷却排气块
CN204365995U (zh) 一种超导炼钢连铸结晶器总成
CN217343504U (zh) 一种冷却效果好的结晶器
CN212265058U (zh) 一种水循环冷却玻璃瓶罐模具
CN212419590U (zh) 低压铸造升液管密封保温冷却装置
CN211363420U (zh) 一种挤出模具薄悬壁冷却系统
CN2389030Y (zh) 半连续铸造结晶器
CN218516910U (zh) 一种立磨选粉机下部轴承的自吸冷却装置
CN217834681U (zh) 一种吹瓶模具颈部隔热机构
CN211516030U (zh) 一种压铸模具冷却装置
CN2319152Y (zh) 弹性热应力自适应组合板条结晶器
CN212884918U (zh) 一种具有辅助推送结构的连铸热钢输送装置
CN2330840Y (zh) 高风温水冷热风阀门的阀板

Legal Events

Date Code Title Description
C14 Grant of patent or utility model
GR01 Patent grant
C19 Lapse of patent right due to non-payment of the annual fee
CF01 Termination of patent right due to non-payment of annual fee