CN205147239U - 一种制取铸造铝合金拉伸试棒的新型模具 - Google Patents

一种制取铸造铝合金拉伸试棒的新型模具 Download PDF

Info

Publication number
CN205147239U
CN205147239U CN201520933401.2U CN201520933401U CN205147239U CN 205147239 U CN205147239 U CN 205147239U CN 201520933401 U CN201520933401 U CN 201520933401U CN 205147239 U CN205147239 U CN 205147239U
Authority
CN
China
Prior art keywords
aluminium liquid
tensile test
test bar
sidewalk
sediment
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201520933401.2U
Other languages
English (en)
Inventor
苑高利
杜科选
葛素静
宗福春
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Hebei xinlizhong Nonferrous Metals Group Co., Ltd
Original Assignee
HEBEI LIZHONG GROUP
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by HEBEI LIZHONG GROUP filed Critical HEBEI LIZHONG GROUP
Priority to CN201520933401.2U priority Critical patent/CN205147239U/zh
Application granted granted Critical
Publication of CN205147239U publication Critical patent/CN205147239U/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本实用新型涉及一种制取铸造铝合金拉伸试棒的新型模具,包括浇注口、铝液通道、底铸横浇道、拉伸试棒部及补缩冒口,底铸横浇道的轴向两端密封,在底铸横浇道的管壁上依次间隔连通连接拉伸试棒部、避渣盲道及铝液通道,在铝液通道的顶部制有浇注口,在拉伸试棒部的顶部制有补缩冒口。本模具在铝液通道与试棒部之间制有一避渣盲道,铝液中的气体和渣由于密度小会在避渣盲道中上浮,留在避渣盲道顶端,同时由于避渣盲道中有一定的铝液,而使试棒底部与底铸横浇道连接处温度较高,铝液凝固速度减缓,进而使底铸横浇道能充分给试棒底部补缩,使试棒底部表面保证很好的光洁度且不容易产生缩松。

Description

一种制取铸造铝合金拉伸试棒的新型模具
技术领域
本实用新型属于铝合金制造领域,涉及拉伸试棒,尤其是一种制取铸造铝合金拉伸试棒的新型模具。
背景技术
目前,铸造铝合金拉伸试样制取时,夹渣、气孔、缩松、外观成型率是影响试棒质量的主要问题,日常生产中使用较多的立式试棒模具为GB/T1173-2013拉伸样模具,此模具对浇注温度和浇注速度要求较高,且使用过程中经常伴有夹渣、气孔、缩松和浇不足的现象出现,造成试棒合格率低,力学性能达不到要求,从而导致重新取样检测,造成重复性工作。
GB/T1173-2013拉伸样模具的主要缺点是:①对模具温度以及铝液温度要求较高②对浇注速度要求比较严格③试棒成品率及力学性能偏低。
实用新型内容
本实用新型的目的在于克服现有技术的不足之处,提供一种制取铸造铝合金拉伸试样的新型模具,此模具能够有效减少试棒的气孔和夹渣,缩松现象也得到明显改善。
本实用新型解决技术问题所采用的技术方案是:
一种制取铸造铝合金拉伸试棒的新型模具,包括浇注口、铝液通道、底铸横浇道、拉伸试棒部及补缩冒口,底铸横浇道的轴向两端密封,在底铸横浇道的管壁上依次间隔连通连接拉伸试棒部、避渣盲道及铝液通道,在铝液通道的顶部制有浇注口。
而且,在拉伸试棒部的顶部制有补缩冒口。
本实用新型的优点和积极效果是:
1、本模具在铝液通道与试棒部之间制有一避渣盲道,铝液中的气体和渣由于密度小会在避渣盲道中上浮,留在避渣盲道顶端,同时由于避渣盲道中有一定的铝液,而使试棒底部与底铸横浇道连接处温度较高,铝液凝固速度减缓,进而使底铸横浇道能充分给试棒底部补缩,使试棒底部表面保证很好的光洁度且不容易产生缩松。
2、本模具结构设计科学合理,使铝液是从下往上走,不会出现浇不足的现象,气和渣密度比铝小会上浮到铝液表面,不会留在试棒中,试棒顶端的冒口能够很好的为试棒上部补缩,使试棒保证很好光洁度和致密性。
附图说明
图1为本模具的结构图。
具体实施方式
下面结合附图并通过具体实施例对本实用新型作进一步详述,以下实施例只是描述性的,不是限定性的,不能以此限定本实用新型的保护范围。
一种制取铸造铝合金拉伸试棒的新型模具,包括浇注口1、铝液通道2、底铸横浇道4、避渣盲道3、拉伸试棒部5及补缩冒口6,底铸横浇道的轴向两端密封,在底铸横浇道的管壁上依次间隔连通连接拉伸试棒、避渣盲道及铝液通道,在拉伸试棒部的顶部制有补缩冒口,在铝液通道的顶部制有浇注口。
浇注过程中,将铝液从浇注口浇入,尽量保证浇注口内铝液是满的,以减少铝液流动过程中带入的气体,当铝液流到避渣盲道位置时,铝液中的气体和渣由于密度小会在避渣盲道中上浮,留在避渣盲道顶端,同时由于避渣盲道中有一定的铝液,而使试棒底部与底铸横浇道连接处温度较高,铝液凝固速度减缓,进而使底铸横浇道能充分给试棒底部补缩,使试棒底部表面保证很好的光洁度且不容易产生缩松。GB/T1173-2013试棒模具浇注过程中试棒部分是上下一起浇注,在铝液上下接触部位容易出现气孔、夹渣,如果铝液温度或者模具温度偏低,就会造成接触部位浇不足。而本模具铝液是从下往上走,不会出现浇不足的现象,气和渣密度比铝小会上浮到铝液表面,不会留在试棒中,试棒顶端的冒口能够很好的为试棒上部补缩,使试棒保证很好光洁度和致密性。
以上所述的仅是本实用新型的优选实施方式,应当指出,对于本领域的普通技术人员来说,在不脱离实用新型构思的前提下,还可以做出若干变形和改进,这些都属于本实用新型的保护范围。

Claims (2)

1.一种制取铸造铝合金拉伸试棒的新型模具,包括浇注口、铝液通道、底铸横浇道、拉伸试棒部及补缩冒口,底铸横浇道的轴向两端密封,其特征在于:在底铸横浇道的管壁上依次间隔连通连接拉伸试棒部、避渣盲道及铝液通道,在铝液通道的顶部制有浇注口。
2.根据权利要求1所述的制取铸造铝合金拉伸试棒的新型模具,其特征在于:在拉伸试棒部的顶部制有补缩冒口。
CN201520933401.2U 2015-11-20 2015-11-20 一种制取铸造铝合金拉伸试棒的新型模具 Active CN205147239U (zh)