CN202934090U - 一种耐磨的结晶器窄面铜板装置 - Google Patents

一种耐磨的结晶器窄面铜板装置 Download PDF

Info

Publication number
CN202934090U
CN202934090U CN 201220390256 CN201220390256U CN202934090U CN 202934090 U CN202934090 U CN 202934090U CN 201220390256 CN201220390256 CN 201220390256 CN 201220390256 U CN201220390256 U CN 201220390256U CN 202934090 U CN202934090 U CN 202934090U
Authority
CN
China
Prior art keywords
wear
copper plate
narrow
resisting
surface copper
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
CN 201220390256
Other languages
English (en)
Inventor
王文学
刘赵卫
赵敏
刘彩玲
王受田
杨超武
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
China National Heavy Machinery Research Institute Co Ltd
Original Assignee
China National Heavy Machinery Research Institute Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by China National Heavy Machinery Research Institute Co Ltd filed Critical China National Heavy Machinery Research Institute Co Ltd
Priority to CN 201220390256 priority Critical patent/CN202934090U/zh
Application granted granted Critical
Publication of CN202934090U publication Critical patent/CN202934090U/zh
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Abstract

本实用新型涉及冶金连铸设备,特别涉及一种耐磨的结晶器窄面铜板装置,其特征是:在窄面铜板下部的两侧安装耐磨垫块,窄面铜板和耐磨垫块之间设置有调整垫片,耐磨垫块和调整垫片通过键定位,并用螺栓固定在窄面铜板下部两侧。本实用新型具有延长窄面铜板使用寿命、减少结晶器维修量,保证铸坯角部的缓冷,改善铸坯角部裂纹,提高铸坯质量的特点。

Description

一种耐磨的结晶器窄面铜板装置
技术领域
本实用新型涉及冶金连铸设备,特别涉及一种耐磨的结晶器窄面铜板装置。 
背景技术
为延长结晶器窄面铜板的寿命,改善铸坯角部缓冷和角部裂纹,提高连铸机铸坯质量,多种结晶器技术已应用。但是目前窄面铜板角部在浇钢几千吨左右后就出现明显磨损,严重的时候铜板下部角部的镀层完全磨去且露出铜,铜板下部中间区域镀层完好。角部磨损的铜板如果继续使用轻则铸坯角部裂纹、铸坯渗铜、角部磨损加速,严重的时候会出现窄面漏钢事故。 
为解决上述问题,目前在结晶器中采用了铜板表面镀层技术、多锥度铜板技术、改变窄面铜板水缝等技术,但还是无法解决铜板下部角部的磨损严重、铜板寿命低的问题。在改善铸坯角部缓冷、减少角部裂纹方面也不明显。 
实用新型内容
本实用新型的目的在于克服上述现有技术的不足,提出一种耐磨的结晶器窄面铜板装置,在窄面铜板下部两侧安装耐磨垫块,具有提高窄面铜板边角部硬度、减少窄面铜板的磨损、延长窄面铜板使用寿命、减少维修量;改善铸坯角部缓冷和角部裂纹,提高铸坯质量的特点。 
本实用新型的技术方案为:一种耐磨的结晶器窄面铜板装置,其特征为:在窄面铜板下部的两侧安装耐磨垫块,窄面铜板和耐磨垫块之间设置有调整垫片,耐磨垫块和调整垫片通过键定位,并用螺栓固定在窄面铜板下部两侧。 
所述的耐磨垫块高度为50~250mm,宽度为15~30mm。 
所述的耐磨垫块采用硬度HB>280的钢。 
本实用新型的有益效果为:由于本实用新型在窄面铜板下方角部安装耐磨垫块,提高了铜板的耐磨性,延长窄面铜板使用寿命、减少维修量;改善铸坯角部缓冷和角部裂纹,提高连铸坯质量的特点。 
附图说明
图1是本实用新型的结构原理图; 
图2是本实用新型的A-A剖视图;
图3是本实用新型的B-B剖视图。
图中,1、窄面铜板;2、耐磨垫块;3、螺栓;4、调整垫片;5、键。 
具体实施方式
下面结合附图对本实用新型的结构原理和工作原理作详细叙述。 
实施例1:如图1、2、3所示一种耐磨的结晶器窄面铜板装置,其特征为:在窄面铜板1下部的两侧安装耐磨垫块2,窄面铜板1和耐磨垫块2之间设置有调整垫片4,耐磨垫块2和调整垫片4通过键5定位,并用螺栓3固定在窄面铜板1下部两侧。 
实施例2:与实施例1基本相同,不同之处在于耐磨垫块2高度为50~250mm,宽度为15~30mm。耐磨垫块2采用硬度HB>280的钢。安装好后必须通过调整垫片4将耐磨垫块2调整到等于或者低于窄面铜板工作面0.05~0.1mm。浇钢过程中,由于铸坯角部属于二维冷却,角部冷却强度大、凝固的坯壳强度较高,由于结晶器锥度的原因,在拉坯的过程中,铸坯和铜板紧密接触,铸坯角部和铜板的摩擦力较大,所以窄面铜板角部磨损较大。安装耐磨垫块后,角部为耐磨垫块和铸坯之间的摩擦,因而窄面铜板的耐磨性改善,保证了铸坯窄面传热的均匀性;同时铜板下部角部实现缓冷,角部冷却改善,提高了铸坯质量。 
本实施例没有详细叙述的部件和结构属本行业的公知部件和常用结构或常用手段,这里不一一叙述。 

Claims (3)

1.一种耐磨的结晶器窄面铜板装置,其特征是:在窄面铜板(1)下部的两侧安装耐磨垫块(2),窄面铜板(1)和耐磨垫块(2)之间设置有调整垫片(4),耐磨垫块(2)和调整垫片(4)通过键(5)定位,并用螺栓(3)固定在窄面铜板(1)下部两侧。
2.根据权利要求1所述的一种耐磨的结晶器窄面铜板装置,其特征是:所述的耐磨垫块(2)高度为50~250mm,宽度为15~30mm。
3.根据权利要求1所述的一种耐磨的结晶器窄面铜板装置,其特征是:所述的耐磨垫块(2)采用硬度HB>280的钢。
CN 201220390256 2012-08-08 2012-08-08 一种耐磨的结晶器窄面铜板装置 Expired - Lifetime CN202934090U (zh)