CN202726328U - 压纹整形的焊接用银合金片材 - Google Patents

压纹整形的焊接用银合金片材 Download PDF

Info

Publication number
CN202726328U
CN202726328U CN 201220391636 CN201220391636U CN202726328U CN 202726328 U CN202726328 U CN 202726328U CN 201220391636 CN201220391636 CN 201220391636 CN 201220391636 U CN201220391636 U CN 201220391636U CN 202726328 U CN202726328 U CN 202726328U
Authority
CN
China
Prior art keywords
welding
alloy sheet
embossing
reshaped
silver alloy
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 201220391636
Other languages
English (en)
Inventor
胡迎春
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SICHUAN FEILONG ELECTRONIC MATERIALS CO Ltd
Original Assignee
SICHUAN FEILONG ELECTRONIC MATERIALS CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SICHUAN FEILONG ELECTRONIC MATERIALS CO Ltd filed Critical SICHUAN FEILONG ELECTRONIC MATERIALS CO Ltd
Priority to CN 201220391636 priority Critical patent/CN202726328U/zh
Application granted granted Critical
Publication of CN202726328U publication Critical patent/CN202726328U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型公开了一种压纹整形的焊接用银合金片材,其特征在于:压纹整形的焊接用银合金片材(1)的一表面上压制有波纹(2)。所说的波纹其条纹宽度0.1±0.05mm,条纹高度0.05±0.02mm。由于在银合金片材表面上形成一定规格的波浪形条纹并提高焊接面的直线度。整形完成后增加焊接面的粗糙度从而增加浸润性,增大焊料和母材的接触面积增加焊接强度,波浪形条纹减少大面积虚焊的出现,保证焊接面的直线度保障焊接产品的一致性。

Description

压纹整形的焊接用银合金片材
技术领域
    本实用新型涉及一种型材,尤其涉及一种压纹整形的焊接用银合金片材。
背景技术
众所周知,传统的银合金焊片焊接面为平面,其焊接性能并不理想,造成该类零件生产成本增加,性能不稳定。银合金与体积较大或者形状不规则的基体材料结合时一般都使用焊接方法,由于银合金多数为粉末合金,焊料对该类合金的浸润性较差,焊接完成后产品质量很难保证,产品质量的一致性较差,针对该严重不良检测,挑选十分麻烦。另外银合金件都比较贵重,该不良会形成巨大的损失。
实用新型内容
本实用新型的目的在于为了克服现有技术的不足而提供一种可以有效増加焊接强度,减少大面积虚焊的压纹整形的焊接用银合金片材。其具体技术方案为:压纹整形的焊接用银合金片材的一表面上压制有波纹。
所说的波纹其条纹宽度0.1±0.05mm,条纹高度0.05±0.02mm。
从本实用新型的技术方案可以看出,由于在银合金片材表面上形成一定规格的波浪形条纹并提高焊接面的直线度。整形完成后增加焊接面的粗糙度从而增加浸润性,增大焊料和母材的接触面积增加焊接强度,波浪形条纹减少大面积虚焊的出现,保证焊接面的直线度保障焊接产品的一致性。完全达到了本实用新型的发明目的。
附图说明
图1是本实用新型压纹整形的焊接用银合金片材断面示意图。
具体实施方式
下面结合附图对本实用新型作进一步详述。
实施例1,压纹整形的焊接用银合金片材1的一表面上压制有波纹2。所说的波纹其条纹宽度0.1±0.05mm,条纹高度0.05±0.02mm。

Claims (2)

1.一种压纹整形的焊接用银合金片材,其特征在于:压纹整形的焊接用银合金片材(1)的一表面上压制有波纹(2)。
2.根据权利要求1所述的一种压纹整形的焊接用银合金片材, 其特征在于:所说的波纹其条纹宽度0.1±0.05mm,条纹高度0.05±0.02mm。
CN 201220391636 2012-08-09 2012-08-09 压纹整形的焊接用银合金片材 Expired - Fee Related CN202726328U (zh)