CN202628304U - 一种组合式耐磨活塞环 - Google Patents

一种组合式耐磨活塞环 Download PDF

Info

Publication number
CN202628304U
CN202628304U CN 201220305108 CN201220305108U CN202628304U CN 202628304 U CN202628304 U CN 202628304U CN 201220305108 CN201220305108 CN 201220305108 CN 201220305108 U CN201220305108 U CN 201220305108U CN 202628304 U CN202628304 U CN 202628304U
Authority
CN
China
Prior art keywords
piston ring
ring
piston
wear resistant
gap
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 201220305108
Other languages
English (en)
Inventor
高静
袁代华
邓金智
斯明玉
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Chengdu Fanxinjia Technology Co Ltd
Original Assignee
Chengdu Fanxinjia Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Chengdu Fanxinjia Technology Co Ltd filed Critical Chengdu Fanxinjia Technology Co Ltd
Priority to CN 201220305108 priority Critical patent/CN202628304U/zh
Application granted granted Critical
Publication of CN202628304U publication Critical patent/CN202628304U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型提供了一种组合式耐磨活塞环,其主旨在解决活塞环窜气、窜油、耐磨性差等问题,该活塞环包括设置在同一环槽内组合使用的第一活塞环和第二活塞环,第一活塞环和第二活塞环上均设置有间隙,间隙与端面夹角为45°,所述第一活塞环外环侧厚度为内环侧的五分之一,所述第二活塞环外环侧厚度为内环侧的5倍,第一活塞环与第二活塞环其内圆半径、外圆半径均相等;所述第一活塞环和第二活塞环外圆面上设置有亚稳态非晶碳涂层。本实用新型广泛使用在汽车发动机汽缸中。

Description

一种组合式耐磨活塞环
技术领域
本实用新型涉及一种活塞环,特别涉及一种安装于汽车内燃机活塞中的一种组合式耐磨活塞环。
背景技术
内燃机作为一种常规动力机械,己广泛的在日常生活得到推广和应用。由于内燃机是通过使燃料(如汽油、石油等)在气缸内部燃烧而产生热能,再将该热能直接转换为动力和热力的发动机,因此,用于密封、控油及传热作用的活塞环便对内燃机的运行效率及是否能稳定运行有着关键性的作用。
目前,市面上采用的内燃机活塞环由于装配的需要,均制作成一个具有断口的金属圆环。然而在长期的使用过程中,该金属圆环的断口缝隙会越来越大,进而会影响内燃机的密封、控油和传热效果,使汽缸内压力降低,增大了窜气,窜油,量严重影响内燃机性能的稳定。而且目前,活塞环采用的表面处理方式主要是氮化处理或镀铬处理,随着汽车行业的高速发展,大功率、高扭矩、高输出的发动机被更多的设计出来,这就使得对发动机配套零部件的要求变得更加严格,作为发动机的最核心零部件——活塞环将面临更大的挑战。普通的氮化处理或镀铬处理层已经渐渐不能满足需求,主要表现在:1、涂层硬度低,耐磨损性能差;2、涂层的摩擦系数大,对缸套的攻击性大,抗拉缸性能差,而且会造成摩擦损失大,对节能环保不利。所以亟待解决上述技术问题。
实用新型内容
本实用新型的目的在于提供一种能够完善发动机密封性能、高耐磨、高抗拉缸性和低摩擦系属性的组合式活塞环。
为实现上述目的本实用新型采用以下技术方案:
    一种组合式耐磨活塞环,包括设置在同一环槽内组合使用的第一活塞环和第二活塞环,第一活塞环和第二活塞环上均设置有间隙,其特征在于:所述间隙与端面夹角为45°,所述第一活塞环外环侧厚度为内环侧的五分之一,所述第二活塞环外环侧厚度为内环侧的5倍,第一活塞环与第二活塞环其内圆半径、外圆半径均相等;所述第一活塞环和第二活塞环外圆面上设置有亚稳态非晶碳涂层。
所述第一活塞环和第二活塞环间隙相互错开180°设置。
本实用新型具有以下有益效果:
由于本实用新型采用以上技术方案,所述第一活塞环和第二活塞环能够相互有效的对其开口间隙进行封堵,有效的减少了窜气量,且由于在活塞环外表面上设置了亚稳态非晶碳涂层,降低了活塞环对缸套的攻击性,提供了环的抗拉缸性,大大延长了活塞环的使用寿命。
附图说明
图1为本实用新型的第一活塞环结构图;
图2为本实用新型的第二活塞环结构图;
图3为本实用新型的第一活塞环和第二活塞环组合状态图。
具体实施方式
     参见图1、图2、图3,本实用新型所述的一种组合式耐磨活塞环,包括设置在同一环槽内组合使用的第一活塞环和第二活塞环,第一活塞环和第二活塞环上均设置有间隙,其特征在于:所述间隙与端面夹角为45°,所述第一活塞环外环侧厚度为内环侧的五分之一,所述第二活塞环外环侧厚度为内环侧的5倍,第一活塞环与第二活塞环其内圆半径、外圆半径均相等,第一活塞环和第二活塞环外圆面上设置有亚稳态非晶碳涂层。第一活塞环和第二活塞环间隙对称180°设置。

Claims (2)

1.一种组合式耐磨活塞环,包括设置在同一环槽内组合使用的第一活塞环和第二活塞环,第一活塞环和第二活塞环上均设置有间隙,其特征在于:所述间隙与端面夹角为45°,所述第一活塞环外环侧厚度为内环侧的五分之一,所述第二活塞环外环侧厚度为内环侧的5倍,第一活塞环与第二活塞环其内圆半径、外圆半径均相等;所述第一活塞环和第二活塞环外圆面上设置有亚稳态非晶碳涂层。
2.根据权利要求1所述的一种组合式耐磨活塞环,其特征在于:所述第一活塞环和第二活塞环间隙相互错开180°设置。
  
CN 201220305108 2012-06-28 2012-06-28 一种组合式耐磨活塞环 Expired - Fee Related CN202628304U (zh)