CN202129434U - 密封铅酸蓄电池板栅的铸模结构 - Google Patents
密封铅酸蓄电池板栅的铸模结构 Download PDFInfo
- Publication number
- CN202129434U CN202129434U CN201120184283U CN201120184283U CN202129434U CN 202129434 U CN202129434 U CN 202129434U CN 201120184283 U CN201120184283 U CN 201120184283U CN 201120184283 U CN201120184283 U CN 201120184283U CN 202129434 U CN202129434 U CN 202129434U
- Authority
- CN
- China
- Prior art keywords
- grid
- storage battery
- acid storage
- lead acid
- molds
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型提供了一种密封铅酸蓄电池板栅的铸模结构,包括一由复数个板栅模具构成的板栅模具组,两挂耳、至少一导铅口,所述两挂耳分别设于板栅模具组的两侧,每该板栅模具通过一极耳与相邻的挂耳固定连接,所述导铅口位于所述板栅模具组的上方,所述导铅口与板栅模具组之间设置有一缓冲条。本实用新型利用缓冲条延长脱模剂的使用时间,单位时间内脱模剂喷涂次数减少,极大提高了铸片效率。
Description
【技术领域】
本实用新型涉及一种电池行业的铸模结构,尤其涉及一种电动助力车用密封铅酸蓄电池板栅的铸模结构。
【背景技术】
为了降低城市大气的主要污染源燃油汽车废气,并缓解世界石油储量逐渐减少而引起的能源危机,电动车和混合电动车作为一种智能的交通工具应运而生,并在世界范围内已逐步形成有广阔前景的产业,而作为电动车核心的车载电源成为制约电动车发展的主要因素。车载电池是电动车的心脏,开发电动车的竞争,最重要的是开发车载动力电源的竞争。作为电动车和混合电动车的车载电源,相比其它的化学电源,铅蓄电池仍是近十年的首选。随着铅蓄电池工业的发展与进步,本世纪七十年代开始出现了铅蓄电池气体再化合密封技术。该技术表明了铅酸蓄电池的发展进入了新的历史时期。
板栅是铅蓄电池的基本物质之一,它占蓄电池总质量的20%-30%,板栅主要有两大功能:支撑活性物质,充当活性物质的载体;传导和汇集电流,使电流均匀分布在活性物质上。它既对电池活性物质提供机械支撑,又是电流流动的主渠道,因此它不但是极板的“脊骨”,更是极板“血液循环”体系。
目前,现有铅酸蓄电池板栅的铸模结构通常包括一由复数个板栅模具构成的板栅模具组,两挂耳、至少一导铅口,两挂耳分别位于板栅模具组的两侧,每该板栅模具通过一极耳与相邻的挂耳固定连接,且导铅口位于板栅模具组的上方;其在浇铸过程中一般预先用脱模剂喷涂铸模以起到隔热的作用,从而使熔融状态的金属顺利注满模具,防止模具表面受熔融金属液的直接作用,脱模剂可使铸件容易脱模,并且表面光滑。但是脱模剂喷涂完毕后,用符合温度要求的熔融金属液从高位定量注入铸模内,铅液自上往下流产生一定冲击力,使脱模剂易脱落以至于使用时间缩短,导致需经常喷涂脱模剂。
【实用新型内容】
本实用新型所要解决的技术问题在于提供一种延长脱模剂使用时间的密封铅酸蓄电池板栅的铸模结构。
本实用新型是通过以下技术方案解决上述技术问题的:一种密封铅酸蓄电池板栅的铸模结构,包括一由复数个板栅模具构成的板栅模具组,两挂耳、至少一导铅口,所述两挂耳分别设于板栅模具组的两侧,每该板栅模具通过一极耳与相邻的挂耳固定连接,所述导铅口位于所述板栅模具组的上方,其特征在于:所述导铅口与板栅模具组之间设置有一缓冲条。
所述缓冲条的截面形状为长方形。
本实用新型的优点在于:在导铅口下方增加一条缓冲条,减缓铅液进入铸模的冲击力,延长脱模剂的使用时间。
【附图说明】
图1为本实用新型密封铅酸蓄电池板栅的铸模结构示意图。
【具体实施方式】
参照图1所示,本实用新型密封铅酸蓄电池板栅的铸模结构,含有一由复数个板栅模具11构成的板栅模具组1,两个挂耳2、至少一个导铅口3,所述两个挂耳2分别设于板栅模具组1的两侧,每一个板栅模具11通过一极耳4与相邻的挂耳2固定连接,所述导铅口3位于所述板栅模具组1的上方,本实施例中板栅模具11的数量为4个。所述导铅口3与板栅模具组1之间设置有一缓冲条5。为使制造工艺简单,将所述缓冲条5的截面形状设为为长方形。缓冲条5的尺寸优选为:宽度为5mm,厚度为2mm,长度为290mm。
当应用本实用新型工作时,先喷涂脱模剂,然后将一定温度的铅液从高位铅勺定量注入铸模内,铅液自上而下先流经缓冲条5,减弱了一定的冲击力,再流入铸模内的各个部件中,由于缓冲条的设置,减缓了铅液进入铸模的冲击力,延长脱模剂的使用时间,单位时间内脱模剂喷涂次数减少,极大地提高了铸片效率。
以上所述仅为本实用新型的较佳实施例,凡依本实用新型申请专利范围所做的均等变化与修饰,皆应属本实用新型的涵盖范围。
Claims (2)
1.一种密封铅酸蓄电池板栅的铸模结构,包括一由复数个板栅模具构成的板栅模具组,两挂耳、至少一导铅口,所述两挂耳分别位于板栅模具组的两侧,每该板栅模具通过一极耳与相邻的挂耳固定连接,所述导铅口位于所述板栅模具组的上方,其特征在于:所述导铅口与板栅模具组之间设置有一缓冲条。
2.如权利要求1所述的密封铅酸蓄电池板栅的铸模结构,其特征在于:所述缓冲条的截面形状为长方形。