CN202087779U - 细长孔砂芯 - Google Patents

细长孔砂芯 Download PDF

Info

Publication number
CN202087779U
CN202087779U CN2011201525352U CN201120152535U CN202087779U CN 202087779 U CN202087779 U CN 202087779U CN 2011201525352 U CN2011201525352 U CN 2011201525352U CN 201120152535 U CN201120152535 U CN 201120152535U CN 202087779 U CN202087779 U CN 202087779U
Authority
CN
China
Prior art keywords
elongated hole
core
sand core
utility
model
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2011201525352U
Other languages
English (en)
Inventor
陆乾
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
WUXI DEQIAN ENERGY EQUIPMENT CO Ltd
Original Assignee
WUXI DEQIAN ENERGY EQUIPMENT CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by WUXI DEQIAN ENERGY EQUIPMENT CO Ltd filed Critical WUXI DEQIAN ENERGY EQUIPMENT CO Ltd
Priority to CN2011201525352U priority Critical patent/CN202087779U/zh
Application granted granted Critical
Publication of CN202087779U publication Critical patent/CN202087779U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型其涉及一种用于铸出铸件上的细长孔的砂芯,该细长孔砂芯是管体结构。本实用新型提供了一种后续处理工艺简单、目标件质量稳定的细长孔砂芯。

Description

细长孔砂芯
技术领域
本实用新型属铸造领域,涉及一种砂芯,尤其涉及一种用于铸出铸件上的细长孔的砂芯。
背景技术
目前在铸造过程中,当需要在铸件上铸出细长孔时,常规的做法是采用一般内孔砂芯,合箱完成后达到浇注条件时,通过浇注系统浇入钢水,浇注完成后钢水和砂型一并冷却至一定温度,开箱清砂,铸件清砂完毕后最后清理铸件上的细长孔。虽然该方法能够铸出细长孔,但在钢水凝固的过程中,由于高温钢水的热辐射作用,细长孔砂芯极易烧结,导致细长孔内壁粘砂、结疤,严重的甚至会堵塞铸件的细长孔导致铸件报废;另外,细长孔的砂芯强度不高,起模时的一般碰撞极易导致芯子损毁,造成砂芯的报废。
实用新型内容
为了解决背景技术中存在的上述技术问题,本实用新型提供了一种后续处理工艺简单、目标件质量稳定的细长孔砂芯。
本实用新型的技术解决方案是:本实用新型提供了一种细长孔砂芯,其特殊之处在于:所述细长孔砂芯是管体结构。
上述管体是无缝管体。
上述管体的截面呈圆形、椭圆形、三角形、矩形或多边形。
上述管体的是钢质的管体。
本实用新型的优点是:本实用新型提供了一种细长孔砂芯,包括一个结构简单的无缝钢管,在使用时,将干砂灌注无缝钢管中,形成一个钢管整体;配箱、验箱完成后形成目标件铸型,浇注钢水后,钢管与熔融的钢水融为一体进而形成细长孔,也就形成了铸件上所需要的细长孔。通过简单的清砂后,铸件上的细长孔内壁非常光滑,无夹杂物及无粘砂,无需对细长孔的内壁进行特殊处理,简化了细长孔的后续处理工艺。同时,由于无缝钢管的存在,在钢管内的砂型不容易损毁,也进一步的保证了细长孔的质量。
附图说明
图1是本实用新型所提供的细长孔砂芯使用状态参考图。
具体实施方式
本实用新型提供了一种细长孔砂芯,该细长孔砂芯是管体结构,该管体2是无缝管体,其截面可以呈圆形、椭圆形、三角形、矩形或多边形等多种形态,管体2的材质、形状与细长孔所在铸件的材质是一致,比如当细长孔所在铸件的材质为SC450则采用SC450材质的管体。
参见图1,本实用新型在使用时,1为普通砂芯,2为特殊耐热砂芯,首先将内层砂芯1、2填充在管体4中,配箱时将管体4下至规定位置。浇注钢水后,管体4与熔融的钢水3融为一体进而使铸件成形一体形成细长孔,本实用新型主要解决了铸造时很难铸出细长孔的问题。通过简单的清砂后(风铲去掉事先保存在管体4内部的内层干砂1、2),铸件上的细长孔内壁非常光滑,几乎无夹杂物及粘砂现象,无需对细长孔的内壁进行特殊处理,简化了细长孔的后续处理工艺。

Claims (4)

1.一种细长孔砂芯,其特征在于:所述细长孔砂芯是管体结构。
2.根据权利要求1所述的细长孔砂芯,其特征在于:所述管体是无缝管体。
3.根据权利要求1或2所述的细长孔砂芯,其特征在于:所述管体的截面呈圆形、椭圆形、三角形、矩形或多边形。
4.根据权利要求3所述的细长孔砂芯,其特征在于:所述管体的是钢质的管体。
CN2011201525352U 2011-05-13 2011-05-13 细长孔砂芯 Expired - Fee Related CN202087779U (zh)