CN201792458U - 一种潜伏式进胶镶件 - Google Patents

一种潜伏式进胶镶件 Download PDF

Info

Publication number
CN201792458U
CN201792458U CN2010205510934U CN201020551093U CN201792458U CN 201792458 U CN201792458 U CN 201792458U CN 2010205510934 U CN2010205510934 U CN 2010205510934U CN 201020551093 U CN201020551093 U CN 201020551093U CN 201792458 U CN201792458 U CN 201792458U
Authority
CN
China
Prior art keywords
mold insert
glue
advances
glue feeding
running channel
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2010205510934U
Other languages
English (en)
Inventor
黄顺华
高登明
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Jiaxing Xinyuan Precision Mould Technology Co Ltd
Original Assignee
Jiaxing Xinyuan Precision Mould Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Jiaxing Xinyuan Precision Mould Technology Co Ltd filed Critical Jiaxing Xinyuan Precision Mould Technology Co Ltd
Priority to CN2010205510934U priority Critical patent/CN201792458U/zh
Application granted granted Critical
Publication of CN201792458U publication Critical patent/CN201792458U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型涉及一种潜伏式进胶镶件,包括镶件本体、进胶浇道;进胶浇道倾斜开在镶件本体内,浇道的浇口为破半边形状,镶件采用硬度较高的材料制作;采用上述措施,在浇口处切断产品更加容易,并且由于镶件本身耐磨,有利于增加模具的量产性。采用进胶镶件的形式,加工,维修、更换都会更加方便。

Description

一种潜伏式进胶镶件
技术领域
本实用新型涉及模具领域,尤其是一种潜伏式进胶镶件。
背景技术
潜伏式进胶为注塑模具上最常见的进胶方式之一,这种进胶方式是潜伏到产品里面进胶,在顶出产品时可以自动切断进胶口,减少人工剪胶口这个步骤,而且不会影响产品外观。
现有潜伏式进胶的设计方式是在模仁上开锥形孔。要先将模仁上斜孔斜度校正,加工较麻烦,当需要维修或设变此处时,都会比较麻烦。而且此种方式在量产过程中,切断胶口处经过塑胶料的长期磨损会变钝,导致在切断过程中切料不干净,从而对产品的品质造成影响。
实用新型内容
本实用新型所要解决的技术问题是提供一种潜伏式进胶镶件,以解决现有技术中在模仁上开锥形浇道所引起的加工、维修或设变此处时较麻烦,以及此种方式长期下去会造成切断胶口处变钝,切断过程中切料不干净的问题。
本实用新型解决其技术问题所采用的技术方案是:提供一种潜伏式进胶镶件,包括镶件本体、进胶浇道;进胶浇道为一锥形孔,并倾斜开在镶件本体内,倾斜角度为30°~50。
锥形进胶浇道自身张开角度为20°~30°。
锥形进胶浇道头部是半径为0.5~2mm的半球形。
锥形进胶浇道的浇口为破半边结构。
有益效果
1、由于此镶件选用硬度高的钢材,而且在进胶口处设计成破半孔的形式,增加切断处的锋利度,增加了它的寿命;
2、由于为镶件的形式,体积和重量相对模仁来说都要小很多,摆斜度和搬移都较方便,减少了加工难度;
3、维修或者设变时只需要将镶件拆出,更改完成后安装即可,大大减少了维修难度。
附图说明
图1为本实用新型剖视图。
图2为图1中A部分的放大图。
具体实施方式
下面结合具体实施例,进一步阐述本实用新型。应理解,这些实施例仅用于说明本实用新型而不用于限制本实用新型的范围。此外应理解,在阅读了本实用新型讲授的内容之后,本领域技术人员可以对本实用新型作各种改动或修改,这些等价形式同样落于本申请所附权利要求书所限定的范围。
如图1、图2所示,本实用新型包括镶件本体1、进胶浇道2;进胶浇道2为一锥形孔,该锥形孔倾斜开在镶件本体1内。并且锥形进胶浇道2的浇口5为破半边结构。
在模仁4内开出一个与进胶镶件同样形状的孔,将进胶镶件放入其中。
当开模后,顶出产品3时,浇道的浇口5同时切断进胶口。将进胶镶件选用硬度较高的钢材(>HRC45),并且将浇口5设计成破半边形状,可以更有效的在浇口5处切断产品3,镶件较耐磨,有利于增加模具的量产性。

Claims (5)

1.一种潜伏式进胶镶件,包括镶件本体(1)、进胶浇道(2);其特征在于:所述进胶浇道(2)为一锥形孔,并倾斜开在所述镶件本体(1)内,倾斜角度为30°~50°。
2.根据权利要求1所述的一种潜伏式进胶镶件,其特征在于:所述锥形进胶浇道(2)自身张开角度为20°~30°。
3.根据权利要求1或2所述的一种潜伏式进胶镶件,其特征在于:所述锥形进胶浇道(2)头部是半径为0.5~2mm的半球形。
4.根据权利要求1或2所述的一种潜伏式进胶镶件,其特征在于:所述进胶浇道(2)的浇口(5)为破半边结构。
5.根据权利要求3所述的一种潜伏式进胶镶件,其特征在于:所述进胶浇道(2)的浇口(5)为破半边结构。
CN2010205510934U 2010-09-30 2010-09-30 一种潜伏式进胶镶件 Expired - Fee Related CN201792458U (zh)