CN201718163U - 柔性透明电磁屏蔽膜 - Google Patents

柔性透明电磁屏蔽膜 Download PDF

Info

Publication number
CN201718163U
CN201718163U CN2010202183502U CN201020218350U CN201718163U CN 201718163 U CN201718163 U CN 201718163U CN 2010202183502 U CN2010202183502 U CN 2010202183502U CN 201020218350 U CN201020218350 U CN 201020218350U CN 201718163 U CN201718163 U CN 201718163U
Authority
CN
China
Prior art keywords
layer
electromagnetic shielding
film
shielding film
zao
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2010202183502U
Other languages
English (en)
Inventor
曾鸿斌
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Zhejiang Hansen Application Materials Co., Ltd.
Original Assignee
SHENZHEN HAISEN APPLIED MATERIALS CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SHENZHEN HAISEN APPLIED MATERIALS CO Ltd filed Critical SHENZHEN HAISEN APPLIED MATERIALS CO Ltd
Priority to CN2010202183502U priority Critical patent/CN201718163U/zh
Application granted granted Critical
Publication of CN201718163U publication Critical patent/CN201718163U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型涉及一种柔性透明电磁屏蔽膜,包括PET基底层和电磁屏蔽层,所述电磁屏蔽层包括用卷绕镀膜方法,在所述PET基底层上依次连续磁控溅射沉积的Nb2O5层、Ag层、ZAO层以及Nb2O5层,Nb2O5层作为介质层,Ag层作为导电层,ZAO层作为过渡介质层。与现有技术相比,本实用新型具有以下有益效果:降低了成本,提高了电磁屏蔽效果。

Description

柔性透明电磁屏蔽膜
技术领域  本实用新型涉及一种柔性透明电磁屏蔽膜,具体是指在透明的柔性基底上(例如PET聚酯膜),连续沉积Nb2O5/Ag/ZAO/Nb2O5多层透明导电膜,形成高性能的电磁屏蔽膜。
背景技术  柔性透明电磁屏蔽膜广泛应用于LCD(液晶显示),PDP(等离子显示),电子仪器窗口及计算机房的信息防泄漏和干扰等。
现有技术中,柔性透明电磁屏蔽膜包括有以下几种,分别存在不足之处:一、柔性透明导电ITO膜,其价格昂贵,且屏蔽效果欠佳而应用上受到很大限制;二、ITO/Ag/ITO多层透明导电膜系,该导电膜尽管解决了屏蔽效果,但成本更高;三、TiO2/NiCr/Ag/NiCr/TiO2多层膜系,存在TiO2膜沉积速度慢,NiCr过渡层影响透光率等缺陷。
发明内容  本实用新型所解决的技术问题是:为避免现有技术的不足之处提出一种成本低、屏蔽效果好的柔性透明电磁屏蔽膜。
解决上述技术问题采用的技术方案如下:本实用新型柔性透明电磁屏蔽膜,包括PET基底层和电磁屏蔽层,所述电磁屏蔽层包括用卷绕镀膜方法,在所述PET基底层上依次连续磁控溅射沉积的Nb2O5层、Ag层、ZAO层以及Nb2O5层,Nb2O5层作为介质层,Ag层作为导电层,ZAO层作为过渡介质层。
所述电磁屏蔽层包括10-13层,其中Ag层不少于三层,底层和外层均是Nb2O5层。
所述Nb2O5底层和外层的厚度为28-35nm,Nb2O5中间层厚度为56-70nm,Ag层厚度为10-18nm,ZAO层厚度为3-5nm。
与现有技术相比,本实用新型具有以下有益效果:降低了成本,提高了电磁屏蔽效果。
附图说明
图1是所述Nb2O5/Ag/ZAO/Nb2O5透明电磁屏蔽膜的3Ag多层膜系结构剖面图;
图2是所述Nb2O5/Ag/ZAO/Nb2O5透明电磁屏蔽膜的4Ag多层膜系结构剖面图。
具体实施方式
如图1所示,柔性透明电磁屏蔽膜是在透明的柔性基底PET膜1上,采用卷绕镀膜方法,连续磁控溅射沉积Nb2O5/Ag/ZAO/Nb2O5多层膜,形成10-13层高性能的柔性透明电磁屏蔽膜。其中,Ag层3不少于3层。所述Nb2O5层2作为底层-中间层-外层的介质层,ZAO膜是作为Ag层3之前的过渡层介质膜,Ag层3是作为导电层。所述PET膜1是透光良好的光学级聚酯薄膜,其厚度根据需要选择50-125μm。Nb2O5层2是高折射率介质,是光学匹配层,底层2和表层11厚度为28-35nm,而中间层厚度为56-70nm。Nb2O5层2是采用中频磁控溅射沉积的,其溅射速率较高。Ag层3主要起导电作用,电磁屏蔽效果由它决定,膜越厚,污染越少,导电性越好,电磁屏蔽效果也越好;但膜太厚了透光率下降,反射增大,一般根据需要兼顾光电性能控制在10-18nm。ZAO层4是过渡层也是高折射率层,其作用是对Ag层3沉积过程其保护作用,避免氧气氛对Ag层3的污染,以形成良好的金属-介质界面,提高光学匹配和电磁屏蔽效果,厚度为3-5nm。Ag层3和ZAO层4均采用直流磁控溅射沉积。
图2是Nb2O5/Ag/ZAO/Nb2O5透明电磁屏蔽膜的4层Ag膜系结构。与图1所述实施例的3层Ag膜系结构不同之处在于:在3Ag膜系基础上增加了三层,即增加了Ag/ZAO/Nb2O5三层膜。在所述4层A膜系结构中,相应各层膜的厚度要求和制备方法都与图1所述实施例的3层Ag膜系结构相同。

Claims (3)

1.一种柔性透明电磁屏蔽膜,其特征在于:包括PET基底层和电磁屏蔽层,所述电磁屏蔽层包括在所述PET基底层上依次连续磁控溅射沉积的Nb2O5层、Ag层、ZAO层以及Nb2O5层,Nb2O5层作为介质层,Ag层作为导电层,ZAO层作为过渡介质层。
2.如权利要求1所述的柔性透明电磁屏蔽膜,其特征在于:所述电磁屏蔽层包括10-13层,其中Ag层不少于三层,底层和外层均是Nb2O5层。
3.如权利要求2所述的柔性透明电磁屏蔽膜,其特征在于:所述Nb2O5底层和外层的厚度为28-35nm,Nb2O5中间层厚度为56-70nm,Ag层厚度为10-18nm,ZAO层厚度为3-5nm。
CN2010202183502U 2010-06-04 2010-06-04 柔性透明电磁屏蔽膜 Expired - Fee Related CN201718163U (zh)