CN201487475U - 聚四氟乙烯内防腐管线 - Google Patents

聚四氟乙烯内防腐管线 Download PDF

Info

Publication number
CN201487475U
CN201487475U CN2009200312455U CN200920031245U CN201487475U CN 201487475 U CN201487475 U CN 201487475U CN 2009200312455 U CN2009200312455 U CN 2009200312455U CN 200920031245 U CN200920031245 U CN 200920031245U CN 201487475 U CN201487475 U CN 201487475U
Authority
CN
China
Prior art keywords
pipeline
corrosion
polytetrafluoroethylene
sprayed
anticorrosive coat
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2009200312455U
Other languages
English (en)
Inventor
崔海燕
郑延明
李国强
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN2009200312455U priority Critical patent/CN201487475U/zh
Application granted granted Critical
Publication of CN201487475U publication Critical patent/CN201487475U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型涉及一种防腐管线,特别涉及一种聚四氟乙烯内防腐管线。其技术方案是:主要由管道和防腐层组成,所述的防腐层喷涂在管道的内壁,防腐层主要由一层或一层以上的聚四氟乙烯涂料防腐涂层组成,厚度在0.02-0.5毫米。有益效果是:采用聚四氟乙烯涂料作为管线的防腐层,可以实现管道内表面自润滑,表面光滑度高,从而不会结蜡结垢,其不仅耐高温、耐低温,且耐酸碱效果非常好,其无毒无污染,是一种绿色环保的防腐产品。

Description

聚四氟乙烯内防腐管线
一、技术领域:
本实用新型涉及一种内防腐管线,特别涉及一种聚四氟乙烯内防腐管线。
二、背景技术:
目前钢铁制作的管道被普遍应用在传送各种液体的领域,如石油管道、大型污水管道等,但是钢铁制作的管道其管内壁,易结垢、易被腐蚀。为了解决这一问题,可以在管道内壁涂一层防腐涂层,例如:H87防腐漆、环氧粉沫、玻璃磷片、玻璃釉等材料,其存在的问题是:表面光滑度差,易结垢结蜡,导致管线堵塞,流速减缓,压力升高,造成安全隐患,进而容易引发泄漏事件造成环境污染及经济赔偿等严重后果。
三、发明内容:
本实用新型的目的就是针对现有技术存在的上述缺陷,提供一种聚四氟乙烯内防腐管线,其防腐效果好,表面具有自润滑功能。
其技术方案是:主要由管道和防腐层组成,所述的防腐层喷涂在管道的内壁,防腐层主要由一层或一层以上的聚四氟乙烯防腐涂层组成,厚度在0.02-0.5毫米。
上述的防腐层由表层、中层和底层组成,底层喷涂在管道内壁上,中层喷涂在底层表面,表层喷涂在中层表面。
本实用新型的有益效果是:采用聚四氟乙烯材料作为管线的防腐层,可以实现管道内表面自润滑,表面光滑度高,从而不会结蜡结垢,其不仅耐高温、耐低温,且耐酸碱效果非常好,其无毒无污染,是一种绿色环保的防腐产品。
四、附图说明:
附图1是本实用新型的结构示意图;
附图2是本实用新型的防腐层的截面图。
五、具体实施方式:
结合附图1和2,对本实用新型作进一步的描述:
其技术方案是:主要由管道1和防腐层2组成,所述的防腐层2喷涂在管道1的内壁,防腐层2主要由一层或一层以上的聚四氟乙烯涂料防腐涂层组成,当然也可以喷涂聚四氟乙烯涂料多层,使防腐涂层的总厚度在0.02-0.5毫米。其中,参照附图2,本实施例的防腐层2由表层2.1、中层2.2和底层2.3共三层组成,底层2.3喷涂在管道1内壁上,中层喷涂在底层表面,表层喷涂在中层表面,本实施例中每层厚度为0.01-0.02毫米,当然,防腐层也可以喷涂三层以上。
其喷涂工艺为:管道除锈、酸洗、水洗、磷化、清洗、烘干、聚四氟乙烯涂料喷涂三层、高温烧结、保温、成品产出。本实用新型不仅适用于石油工业用的输油管线的防腐处理,且可以应用于污水管线的防腐处理。

Claims (2)

1.一种聚四氟乙烯内防腐管线,其特征是:主要由管道(1)和防腐层(2)组成,所述的防腐层(2)喷涂在管道(1)的内壁,防腐层(2)主要由一层或一层以上的聚四氟乙烯防腐涂层组成,厚度在0.02-0.5毫米。
2.根据权利要求1所述的聚四氟乙烯内防腐管线,其特征是:所述的防腐层(2)由表层(2.1)、中层(2.2)和底层(2.3)组成,底层(2.3)喷涂在管道(1)内壁上,中层喷涂在底层表面,表层喷涂在中层表面。
CN2009200312455U 2009-08-04 2009-08-04 聚四氟乙烯内防腐管线 Expired - Fee Related CN201487475U (zh)