CN201442966U - 薄壁不锈钢管固溶热处理装置 - Google Patents

薄壁不锈钢管固溶热处理装置 Download PDF

Info

Publication number
CN201442966U
CN201442966U CN2009200293045U CN200920029304U CN201442966U CN 201442966 U CN201442966 U CN 201442966U CN 2009200293045 U CN2009200293045 U CN 2009200293045U CN 200920029304 U CN200920029304 U CN 200920029304U CN 201442966 U CN201442966 U CN 201442966U
Authority
CN
China
Prior art keywords
stainless steel
quartz glass
glass tube
thin
tube
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2009200293045U
Other languages
English (en)
Inventor
王春波
李恒财
张明
刘光信
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SHANDONG RONGTAI ELECTRIC FURNACE ENGINEER CO Ltd
Original Assignee
SHANDONG RONGTAI ELECTRIC FURNACE ENGINEER CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SHANDONG RONGTAI ELECTRIC FURNACE ENGINEER CO Ltd filed Critical SHANDONG RONGTAI ELECTRIC FURNACE ENGINEER CO Ltd
Priority to CN2009200293045U priority Critical patent/CN201442966U/zh
Application granted granted Critical
Publication of CN201442966U publication Critical patent/CN201442966U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型公开了一种薄壁不锈钢管固溶热处理装置,由于该薄壁不锈钢管固溶热处理装置包括密封石英玻璃管和套设于所述石英玻璃管的管壁上的感应器,所示石英玻璃管中通惰性气体,所述感应器与固态超音频电源连接,所以,不锈钢管在充满惰性气体的石英玻璃管中被感应加热,有效防止了不锈钢管表面起氧化皮,而且,固态超音频电源输出恒功率控制加热温度恒定。本实用新型温度容易控制且防止起氧化皮,解决了不锈钢管固溶加热难的问题。

Description

薄壁不锈钢管固溶热处理装置
技术领域
本实用新型涉及一种固溶热处理装置,尤其涉及一种对薄壁不锈钢管进行固溶热处理的装置。
背景技术
薄壁不锈钢管是水的准备、贮存、输送、净化、再生、海水淡化等水工业最佳选材。其优点是:耐腐蚀、抗地震、节水、卫生(无铁锈及铜绿色)、重量轻(减轻1/3)、少维修、寿命长(可使用40年)、寿命周期成本(LCC)低、属可回收再利用的绿色环保材料。薄壁不锈钢管的处理比较复杂,最主要的部分是热处理的加热固溶部分。不锈钢管需要直接加热到1150℃,普通加热炉无法实现,因为普通炉子加热温度不容易控制,而且容易起氧化皮。因此一直以来不锈钢管的固溶加热是一种比较难的技术。
实用新型内容
本实用新型所要解决的技术问题是:提供一种薄壁不锈钢管固溶热处理装置,该固溶热处理装置对不锈钢管进行恒温加热,且防止不锈钢管在固溶热处理过程中起氧化皮。
为解决上述技术问题,本实用新型的技术方案是:薄壁不锈钢管固溶热处理装置,包括,石英玻璃管,所述石英玻璃管两端开口并且在开口处安装有密封装置,所述石英玻璃管的内腔形成一个密闭的热处理通道,所述热处理通道具有一个惰性气体进口和一个惰性气体出口;感应器,所述感应器套设于所述石英玻璃管的管壁上并与固态超音频电源连接。
作为一种优选的技术方案,所述密封装置包括与所述薄壁不锈钢管相适配的密封圈。
采用了上述技术方案后,本实用新型的有益效果是:由于该薄壁不锈钢管固溶热处理装置包括密封石英玻璃管和套设于所述石英玻璃管的管壁上的感应器,所示石英玻璃管中通惰性气体,所述感应器与固态超音频电源连接,所以,不锈钢管在充满惰性气体的石英玻璃管中被感应加热,有效防止了不锈钢管表面起氧化皮,而且,固态超音频电源输出恒功率控制加热温度恒定。本实用新型温度容易控制且防止起氧化皮,解决了不锈钢管固溶加热难的问题。
附图说明
附图是本实用新型实施例的结构示意图。
附图中:1.惰性气体出口;2.密封圈;3.石英玻璃管;4.感应器;5.惰性气体进口;6.惰性气体阀门;7.不锈钢管。
具体实施方式
薄壁不锈钢管固溶热处理装置,如附图所示,包括:石英玻璃管3,所述石英玻璃管3两端开口并且在开口处设有与所述薄壁不锈钢管相适配的密封圈2,所述石英玻璃管的内腔形成一个密闭的不锈钢管7热处理通道,所述热处理通道上设有一个惰性气体进口5和一个惰性气体出口1;感应器4,所述感应器4套设于所述石英玻璃管3的管壁上并与固态超音频电源连接。
本实用新型实施例的工作原理:先将惰性气体阀门6打开,往石英玻璃管3中充满惰性气体,然后将不锈钢管7送入石英玻璃管3中,同时启动固态超音频电源,感应器4开始对不锈钢管7进行感应加热,从而不锈钢管7的内部被高频磁场加热,不锈钢管7加热后再经冷却从石英玻璃管中出来,完成不锈钢管的固溶热处理。通过固态电源恒功率输出使得加热温度恒定。
所述固态超音频电源可采用12KHz固态超音频电源,通过固态电源恒功率输出及红外实时测温仪使不锈钢管的温度自动恒定在1150℃。本实用新型经过实际生产作业测试,经过该装置所固溶热处理的不锈钢管表面光亮,并且结实无金属内部应力,提高了企业的产品质量。
本实用新型对不锈钢管进行固溶热处理时,由于是在密封的石英玻璃管中,且石英玻璃管中充满惰性气体,有效防止了不锈钢管与空气接触,从而避免了起氧化皮的问题。同时,所采用的固态超音频电源对感应器提供恒功率电源使得感应加热温度恒定且间接加热,能源利用率高,无污染。

Claims (2)

1.薄壁不锈钢管固溶热处理装置,其特征在于,包括:
石英玻璃管,所述石英玻璃管两端开口并且在开口处安装有密封装置,所述石英玻璃管的内腔形成一个密闭的热处理通道,所述热处理通道具有一个惰性气体进口和一个惰性气体出口;
感应器,所述感应器套设于所述石英玻璃管的管壁上并与固态超音频电源连接。
2.如权利要求1所述的薄壁不锈钢管固溶热处理装置,其特征在于,所述密封装置包括与所述薄壁不锈钢管相适配的密封圈。
CN2009200293045U 2009-07-03 2009-07-03 薄壁不锈钢管固溶热处理装置 Expired - Fee Related CN201442966U (zh)