CN201428823Y - 金属钼和锆刚玉组合闸板 - Google Patents
金属钼和锆刚玉组合闸板 Download PDFInfo
- Publication number
- CN201428823Y CN201428823Y CN2009201035835U CN200920103583U CN201428823Y CN 201428823 Y CN201428823 Y CN 201428823Y CN 2009201035835 U CN2009201035835 U CN 2009201035835U CN 200920103583 U CN200920103583 U CN 200920103583U CN 201428823 Y CN201428823 Y CN 201428823Y
- Authority
- CN
- China
- Prior art keywords
- plate
- zirconium corundum
- molybdenum
- flashboard
- fused alumina
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
一种用于浮法玻璃生产线的金属钼和锆刚玉组合闸板,它包括有锆刚玉闸板体和由置于锆刚玉闸板体上端的矩形槽钢、置于矩形槽钢上面的连接钢板及竖置在矩形槽钢上的卡固螺钉组成的闸板吊装钢构件,在锆刚玉闸板体的前面由上至下依次设置有耐热钢板、锆刚玉砖板和金属钼板,其中的耐热钢板经连接螺钉固定在矩形槽钢上,锆刚玉砖板与耐热钢板和金属钼板分别通过侧向装配有紧固螺钉的镶嵌配合结构相连接。本实用新型解决了现行锆刚玉闸板易受高温玻璃熔液冲刷侵蚀的问题,从而使闸板的使用寿命大大提高,同时提高了玻璃产品的质量。本实用新型特别适用于熔液温度相对较高的高硼硅浮法玻璃的生产。
Description
技术领域
本实用新型涉及浮法玻璃生产设备,具体涉及一种金属钼和锆刚玉组合闸板。
背景技术
在浮法玻璃生产过程中,闸板的作用是调节玻璃熔液流量的大小,以控制玻璃熔液拉引量在生产正常范围内波动,确保玻璃板拉引的质量。现有技术的闸板一般由锆刚玉耐火材料的闸板体和装配在阀板体上端的吊装钢构件组成。该种闸板在使用过程中,锆刚玉闸板体底部受流动玻璃熔液冲刷侵蚀严重,成为影响闸板使用寿命的主要问题,并且锆刚玉闸板在被冲刷侵蚀的同时还会污染玻璃熔液,对玻璃产品的质量产生影响。对于在生产过程中熔液温度相对较高的高硼硅玻璃的生产,闸板易被冲刷侵蚀的问题尤为突出。
发明内容
本实用新型的目的在于针对上述问题,提供一种抵御高温玻璃熔液冲刷侵蚀性能好,特别适用于高硼硅浮法玻璃生产的金属钼和锆刚玉组合闸板。
实现上述目的的技术方案是:一种金属钼和锆刚玉组合闸板,它包括有锆刚玉闸板体和由置于锆刚玉闸板体上端的矩形槽钢、置于矩形槽钢上面的连接钢板及竖置在矩形槽钢上的卡固螺钉组成的闸板吊装钢构件,在锆刚玉闸板体的上端面上设置有闸板体卡固用金属垫板,在锆刚玉闸板体的前面由上至下依次设置有耐热钢板、锆刚玉砖板和金属钼板,其中的耐热钢板经连接螺钉固定在矩形槽钢上,锆刚玉砖板与耐热钢板和金属钼板分别通过侧向装配有紧固螺钉的镶嵌配合结构相连接。
本实用新型将闸板下部设置成金属钼板与锆刚玉板双层组合结构,金属钼板保护锆刚玉闸板体不受高温玻璃熔液冲刷侵蚀,同时金属钼板插入玻璃熔液内,在玻璃熔液与锆刚玉闸板体的保护下与空气隔绝,以防止金属钼板氧化,从而有效的解决了闸板受高温玻璃熔液冲刷侵蚀的问题,使闸板的使用寿命大大提高,同时提高了玻璃的产品质量。
附图说明
图1是本金属钼和锆刚玉组合闸板结构示意图;
图2是图1的左视图。
具体实施方式
结合附图对本实用新型的具体实施方式进行说明。
如附图,本金属钼和锆刚玉组合闸板包括有锆刚玉闸板体1和由置于锆刚玉闸板体1上端的矩形槽钢2、置于槽钢2上面的连接钢板3及竖置在槽钢2上的卡固螺钉4组成的闸板吊装钢构件,在锆刚玉闸板体1的上端面上设置有闸板体卡固用金属垫板5,在锆刚玉闸板体的前面由上至下依次设置有耐热钢板7、锆刚玉砖板8和金属钼板10,其中的耐热钢板7经连接螺钉6固定在矩形槽钢2上,锆刚玉砖板8与耐热钢板7和金属钼板10分别通过侧向装配有紧固螺钉9的镶嵌配合结构相连接。
附图实施例给出的锆刚玉砖板8与耐热钢板7和金属钼板10的镶嵌配合连接结构,是在耐热钢板7和金属钼板10的连接边上设置燕尾槽,在锆刚玉砖板的连接边上设置与燕尾槽相吻合的燕尾形凸体,通过燕尾形凸体与燕尾槽的镶嵌配合实现相接板间的连接。
Claims (1)
1、一种金属钼和锆刚玉组合闸板,包括有锆刚玉闸板体(1)和由置于锆刚玉闸板体(1)上端的矩形槽钢(2)、置于矩形槽钢(2)上面的连接钢板(3)及竖置在矩形槽钢(2)上的卡固螺钉(4)组成的闸板吊装钢构件,在锆刚玉闸板体(1)的上端面上设置有闸板体卡固用金属垫板(5),其特征是:在锆刚玉闸板体(1)的前面由上至下依次设置有耐热钢板(7)、锆刚玉砖板(8)和金属钼板(10),其中的耐热钢板(7)经连接螺钉(6)固定在矩形槽钢(2)上,锆刚玉砖板(8)与耐热钢板(7)和金属钼板(10)分别通过侧向装配有紧固螺钉(9)的镶嵌配合结构相连接。