CN1986217A - 一种制作皮革模具压花板的方法 - Google Patents
一种制作皮革模具压花板的方法 Download PDFInfo
- Publication number
- CN1986217A CN1986217A CN 200610122166 CN200610122166A CN1986217A CN 1986217 A CN1986217 A CN 1986217A CN 200610122166 CN200610122166 CN 200610122166 CN 200610122166 A CN200610122166 A CN 200610122166A CN 1986217 A CN1986217 A CN 1986217A
- Authority
- CN
- China
- Prior art keywords
- pattern
- plate
- silica gel
- steel plate
- embossing
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种制作皮革模具压花板的方法,包括如下步骤:用激光三维抄数机对准皮样取得皮样的单元图案,在电脑中用程序将扫描图案处理成可输出驱动雕刻机的程序;驱动电脑雕刻机在亚克力板上雕刻出皮样花纹图案;按每100克矽胶加5-20克矽油,把流动性较好的矽胶灌在刻好图案的亚克力板上,取得单元图案的矽胶模,在矽胶模涂上1000目-3000目的纯银粉作为镀体,放入电镀槽进行电镀铜板,电镀时间为1-5日,制出一块印有图案的铜板;开好一块和上述铜板大小相同的钢板,将印有图案的铜板放置在钢板表面,在熔锡的作用下复合在一起。将复合好的铜板抛光并清洗干净,然后再镀一层硬铬,制成压花板。这种方法制作简单,制作压花板的质量高。
Description
技术领域
本发明涉及皮革模具压花板,具体涉及一种制作皮革模具压花板的方法。
背景技术
在现有技术中,常规的制作皮革压花板的步骤如下:1、电脑扫描皮样图案;2、然后出菲林;3、把感光液喷在钢板上拿到感光架上进行感光;4、用天哪水洗出图案;5、再用硝酸腐蚀出图案;6、抛光打磨;7、送去电镀一层硬铬,压花板制作完成,这种做法的缺点是,压花板的花纹是直的,没有弧度,在同一块钢板上,很难做出几种不同深度图案,因需要用具有腐蚀性的化学制剂,因此,采用这种方法制作压花板,不安全、不环保。
发明内容
本发明针对现在技术中存在的上述缺陷,提供一种制作皮革模具压花板的方法,采用这种方法制作的压花板,精度高,花纹逼真,可以制作出更细小的花纹。
提供一种制作皮革模具压花板的方法,方法包括如下步骤:
用激光三维抄数机对准皮样进行扫描,取得皮样的单元图案,单元图案的规格一般可为1-500平方毫米。
将扫描下来的数据输入电脑,在电脑中用程序将扫描图案处理成可输出驱动雕刻机的程序;
用处理好的电脑程序驱动电脑雕刻机在亚克力板上雕刻出皮样图案;
按每100克矽胶加5-20克矽油,每100克矽胶加凝固水1-10克的配比,把流动性较好的矽胶灌在刻好图案的亚克力板上,取得单元图案的矽胶模,可根据压花板面积的大小需要,重复灌注一块或若干块,然后把两块印有图案的矽胶模相并接,拼接成更大面积的单元图案,可多块拼接;如果采用可大面积雕刻的电脑雕刻机进行雕刻,也可以不用拼接;
将并接好的矽胶模涂上1000目-3000目的纯银粉作为镀体,放入电镀槽进行电镀铜板,电镀时间为1-5日,制出一块印有图案的铜板;
开好一块和上述铜板大小相同的钢板,一般钢板用45号钢;10毫米厚,将钢板放在加热板上进行加热,将钢板加热到220度,将锡放进钢板面溶解,将印有图案的铜板放置在钢板表面,在熔锡的作用下复合在一起。将复合好的铜板抛光并清洗干净,然后再镀一层硬铬,制成压花板。
在上述制作皮革模具压花板的方法中,还包括将拼接好的矽胶图案放入真空机中,对矽胶模进行抽真空步骤,可使矽胶板的气泡减小,灌出来的图案更清晰、更平坦;真空机的规格内径长为1600毫米,宽为1300毫米,高为450毫米。
本发明的有益效果如下;通过采用激光三维抄数机对皮样进行扫描,相比传统的采样方法,可以采集到皮样中的更细小纹路,采用这种方法制作皮革模具压花板,可以解决现有技术不能做深花图案压花板的问题,这种压花板可随意加深,顺滑流畅,立体感非常强。可使压花板图案顺滑流畅,深浅随意,只使用少量的化学物质,具有环保的优点。
具体实施方式
提供一种制作皮革模具压花板的方法,方法包括如下步骤:
1)、用激光三维抄数机对准皮样进行扫描,取得皮样的单元图案,单元图案的规格一般可为1-500平方毫米。
2)、将扫描下来的数据输入电脑,在电脑中用程序将扫描图案处理成可输出驱动雕刻机的程序;
3)、用处理好的电脑程序驱动电脑雕刻机在亚克力板上雕刻出皮样图案;
4)、按每100克矽胶加5-20克矽油,每100克矽胶加凝固水1-10克的配比,把流动性较好的矽胶灌在刻好图案的亚克力板上,取得单元图案的矽胶模,可根据压花板面积的大小需要,重复灌注一块或若干块,然后把两块印有图案的矽胶模相并接,拼接成更大面积的单元图案,可多块拼接;
5)、将并接好的矽胶涂上1000目-3000目的纯银粉作为镀体,放入电镀槽进行电镀铜板,电镀时间为1-5日,制出一块印有图案的铜板;
6)、开好一块和上述铜板大小相同的钢板,一般钢板用45*钢;10毫米厚,将钢板放在加热板上进行加热,将钢板加热到220度,将锡放进钢板面溶解,将印有图案的铜板放置在钢板表面,在熔锡的作用下复合在一起。
7)、将复合好的铜板抛光并清洗干净,然后再镀一层硬铬,制成压花板。
在上述制作皮革模具压花板的方法中,还包括将拼接好的矽胶图案放入真空机中,对矽胶模进行抽真空步骤,可使矽胶板的气泡减小,灌出来的图案更清晰、更平坦;真空机的规格内径长为1600毫米,宽为1300毫米,高为450毫米。
并接好的矽胶模可涂上体积为1000-3000目的纯银粉作为镀体,放入电镀槽进行电镀铜板,一般电镀时间为1-5日,可得到一块有图案的铜板。
开好一块和铜板大小的钢板,一般钢板可采用45*钢。10毫米厚,然后把钢板入在一块加热板进行加热,(加热板可自制,规格是长1700毫米,宽1300毫米,高600毫米,解剖加热板有三层,上层有10毫米铁板;中间层是相向出入水槽可起降温作用,下层是电发热管,将钢板加热到220度,章动角焊锡放进钢板面溶解,然后与印有图案的铜板复合在一起。将复合好的铜板抛光好,并清洗干净,然后再镀上一层硬铬,制得成品压花板。
Claims (2)
1、一种制作皮革模具压花板的方法,方法包括如下步骤:
1)、用激光三维抄数机对准皮样进行扫描,取得皮样的单元图案,单元图案的规格一般可为1-500平方毫米。
2)、将扫描下来的数据输入电脑,在电脑中用程序将扫描图案处理成可输出驱动雕刻机的程序;
3)、用处理好的电脑程序驱动电脑雕刻机在亚克力板上雕刻出皮样花纹图案;
4)、按每100克矽胶加5-20克矽油,每100克矽胶加凝固水1-10克的配比,把流动性较好的矽胶灌在刻好图案的亚克力板上,取得单元图案的矽胶模,可根据压花板面积的大小需要,重复灌注一块或若干块,然后把两块印有图案的矽胶模相并接,拼接成更大面积的单元图案,可多块拼接;在雕刻机可以雕刻大板时,也可以不用拼接,直接用雕刻机在亚克力板上雕刻出客户所需要的花纹图案;
5)、将并接好的矽胶涂上1000目-3000目的纯银粉作为镀体,放入电镀槽进行电镀铜板,电镀时间为1-5日,制出一块印有图案的铜板;
6)、开好一块和上述铜板大小相同的钢板,钢板用45号钢;10毫米厚,将钢板放在加热板上进行加热,将钢板加热到220度,将锡放进钢板面溶解,将印有图案的铜板放置在钢板表面,在熔锡的作用下复合在一起。
7)、将复合好的铜板抛光并清洗干净,然后再镀一层硬铬,制成压花板。
2、根据权利要求1所述制作皮革模具压花板的方法,还包括将拼接好的矽胶图案放入真空机中,对矽胶模进行抽真空步骤,可使矽胶板的气泡减小,灌出来的图案更清晰、更平坦;真空机的规格内径长为1600毫米,宽为1300毫米,高为450毫米。