CN1978361A - Pal材料微米、亚微米粉体提纯工艺技术 - Google Patents

Pal材料微米、亚微米粉体提纯工艺技术 Download PDF

Info

Publication number
CN1978361A
CN1978361A CN 200510127858 CN200510127858A CN1978361A CN 1978361 A CN1978361 A CN 1978361A CN 200510127858 CN200510127858 CN 200510127858 CN 200510127858 A CN200510127858 A CN 200510127858A CN 1978361 A CN1978361 A CN 1978361A
Authority
CN
China
Prior art keywords
pal material
pal
polygorskite
purifying technology
purity
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 200510127858
Other languages
English (en)
Inventor
曹发魁
牟森
张翀
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
GANSU KAIXI ECOLOGICAL ENVIRONMENT ENGINEERING Co Ltd
Original Assignee
GANSU KAIXI ECOLOGICAL ENVIRONMENT ENGINEERING Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by GANSU KAIXI ECOLOGICAL ENVIRONMENT ENGINEERING Co Ltd filed Critical GANSU KAIXI ECOLOGICAL ENVIRONMENT ENGINEERING Co Ltd
Priority to CN 200510127858 priority Critical patent/CN1978361A/zh
Publication of CN1978361A publication Critical patent/CN1978361A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种PAL材料提纯加工工艺。经过提纯加工后其纯度可达90-97%。由于有效组分(纯度)提高、性能优化,大幅度提高PAL材料的胶体性、吸附性、悬浮性、耐热性等性能。

Description

PAL材料微米、亚微米粉体提纯工艺技术
技术领域
本发明所涉及PAL材料的提纯工艺技术,主要是对PAL材料纯度的提选。PAL材料所具有的独特的晶体结构和特殊的物化性能,如良好的吸附性、脱色性、悬浮性、缓释性、离子交换性、酸碱度可调性、胶体性、造浆性、抗盐性、热稳定性等优良的性能。可广泛用于国防、航天、建材、轻工、环保、医药、农业等领域。
由于PAL材料本身的粒度较细(一般小于10微米),其它杂质如石英、碳酸盐、长石、云母等的粒度相对较大,通常大于0.03毫米,杂质矿物与PAL材料矿物之间的比重较小。一般的常规选提方法无法达到分离提纯的目的。本发明充分利用PAL材料原料组分的粒度差、高分散性进行提纯。
背景技术
目前用于粉体提纯的技术有液相法、气相法、固相法(高能球磨),以及分散处理、研磨气选法等工艺技术。本发明的特点在于,采用湿法高分散、高速离心提纯工艺,不添加任何药物进行生产,无二次化学污染、环保效益好,具有循环经济特点。
发明内容
本发明的主要目的:
针对甘肃省的特色资源优势PAL材料独特结构与构造(PAL材料在甘肃远景储量占世界储量的80%),和该材料特有的富含以碘、硒、锌为代表的人体所需的有益元素,及该材料特有的吸附性、缓释性、催化性、胶体性、比表面积大、离子交换性(CEC)强、酸碱可控性强等性能。PAL材料超微化技术工艺的突破,为西部PAL材料优势资源广泛应用于工业、农业、医药、石油、化工、建材、航天、化妆品、生态环境保护治理等产业提供了技术、原料保证。
本发明是将PAL材料经无药加水搅拌、高速离心分离、二级浓缩后,喷雾、干燥,纯度为90-97%。
本发明在生产过程中不产生废弃物,尾渣、废水可做为副产品用于农业生产和保健领域并产品化。生产过程生态化生产环节中,无任何环保负作用和潜在危害,资源的利用率达100%。
具体实施方式
首先是将原矿粉碎后,过100-200目筛后,加水均匀搅拌,经离心分离后,二级浓缩、喷雾干燥即可成为高纯度(90-97%)超微粉体产品。分离后的尾渣可做为相关产品,如:硅肥、土壤调理剂等。废水可循环使用,经净化处理后,可成为高品质纯净水,为高级饮品。

Claims (6)

1、一种PAL材料(其原料是坡缕石,经超微化提纯处理,坡缕石纯度>90%,粒径<8μ)提纯工艺技术。由坡缕石(凹凸棒石)原矿为原料的提纯工艺技术。
2、根据权利要求1,将PAL材料原矿石粉碎后(100目-200目),经均匀搅拌(浓度:浆体10-25%)后,经过高速离心(1800r/min)提纯,(PAL材料从原矿含量20-30%提高到纯度达90-97%)。
3、根据权利要求1,提纯后浆液,经二级浓缩,喷雾干燥。
4、根据权利要求1,无药提纯工艺,环保意义大。
5、根据权利要求1,提纯后的PAL材料精粉可直接用于医药、化工、食品添加剂等领域中。
6、根据权利要求1,对副产品进行产品化处理,资源利用率达到100%。
CN 200510127858 2005-12-06 2005-12-06 Pal材料微米、亚微米粉体提纯工艺技术 Pending CN1978361A (zh)