Prior art keywords
pal material
purification
technology
pal
ultramicronising
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 200510127859
Other languages
English (en)
Inventor
曹发魁
牟森
张翀
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
GANSU KAIXI ECOLOGICAL ENVIRONMENT ENGINEERING Co Ltd
Original Assignee
GANSU KAIXI ECOLOGICAL ENVIRONMENT ENGINEERING Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by GANSU KAIXI ECOLOGICAL ENVIRONMENT ENGINEERING Co Ltd filed Critical GANSU KAIXI ECOLOGICAL ENVIRONMENT ENGINEERING Co Ltd
Priority to CN 200510127859 priority Critical patent/CN1978390A/zh
Publication of CN1978390A publication Critical patent/CN1978390A/zh
Pending legal-status Critical Current

Links

Landscapes

  • Fertilizers (AREA)

Abstract

本发明公开了一种PAL材料超微化和提纯加工工艺。经过提纯加工后其纯度可达90-97%,粒径可达2.93-3.00μm。由于有效组分(纯度)提高,粒度超微化后的性能优化,大幅度提高PAL材料的胶体性、吸附性、悬浮性、耐热性等性能。

Description

PAL材料微米、亚微米粉体提纯、超微化一体化工艺技术
技术领域
本发明所涉及PAL材料的提纯工艺技术和超微化工艺技术。主要是对PAL材料纯度的提选。
PAL材料所具有的独特的晶体结构和特殊的物化性能,如良好的吸附性、脱色性、悬浮性、缓释性、离子交换性、酸碱度可调性、胶体性、造浆性、抗盐性、热稳定性等优良的性能。经提纯、超微化后,可广泛用于国防、航天、建材、轻工、环保、医药、农业等领域。
由于PAL材料本身的粒度较细(一般小于10微米),其它杂质如石英、碳酸盐、长石、云母等的粒度相对较大,通常大于0.03毫米,杂质矿物与PAL材料矿物之间的比重较小。一般的常规选提方法无法达到分离提纯的目的。本超微化实施,还必须依赖装备(装备专案申请)进行。本发明充分利用PAL材料原料组分的粒度差、高分散性和装备的功能,进行提纯与超微化的。
背景技术
目前用于粉体提纯的技术有液相法、气相法、固相法(高能球磨),以及分散处理、研磨气选法等工艺技术。本发明的特点在于,采用湿法高分散、高速离心提纯工艺,不添加任何药物进行生产,无二次化学污染、环保效益好,具有循环经济特点。
发明内容
本发明的主要目的:
针对甘肃省的特色资源优势PAL材料独特结构与构造(PAL材料在甘肃远景储量占世界储量的80%),和该材料特有的富含以碘、硒、锌为代表的人体所需的有益元素,及该材料特有的吸附性、缓释性、催化性、胶体性、比表面积大、离子交换性(CEC)强、酸碱可控性强等性能。提高PAL材料的纯度技术和超微化技术的双技同步突破,为西部PAL材料优势资源广泛应用于工业、农业、医药、石油、化工、建材、航天、化妆品、生态环境保护治理等产业提供了技术、原料保证。
本发明是将PAL材料经无药加水搅拌、高速离心分离、二级浓缩后,干燥、粉碎后可达纯度为90-97%的微米、亚微米粉体(2.93-3.00μm)。
本发明在生产过程中不产生废弃物,尾渣、废水可做为副产品用于农业生产和保健领域,并产品化。生产过程生态化生产环节中,无任何环保负作用和潜在危害,资源的利用率达100%。
具体实施方式
首先是将原矿粉碎后,过100-200目筛后,加水均匀搅拌,经离心分离后,二级浓缩、喷雾干燥,即可成为高纯度(90-97%)超微粉体(2.93-3.00μm)产品,分离后的尾渣可做为相关产品,如:硅肥、土壤调理剂等。废水可循环使用,经净化处理后,可成为高品质纯净水,为高级饮品。

Claims (6)

1、一种PAL材料(其原料是坡缕石,经超微化提纯处理,坡缕石纯度>90%,粒径<8μ)的提纯、超微化工艺技术。由坡缕石(凹凸棒石)原矿为原料的提纯工艺技术及超微化工艺技术为双技同步技术。
2、根据权利要求1,将PAL材料原矿石粉碎后(100目-200目),经均匀搅拌(浓度:浆体10-25%)后,经过高速离心(1800r/min)提纯,(PAL材料从原矿含量20-30%提高到纯度达90-97%)。
3、根据权利要求1,提纯后浆液,经二级浓缩,喷雾干燥,即粒径为微米、亚微米级标准(2.93-3.00μm)。
4、根据权利要求1,无药提纯工艺,环保意义大。
5、根据权利要求1,提纯后的PAL材料精粉可直接用于医药、化工、食品添加剂等领域中。
6、根据权利要求1,对副产品进行产品化处理,资源利用率达到100%。
CN 200510127859 2005-12-06 2005-12-06 Pal材料微米、亚微米粉体提纯、超微化一体化工艺技术 Pending CN1978390A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN 200510127859 CN1978390A (zh) 2005-12-06 2005-12-06 Pal材料微米、亚微米粉体提纯、超微化一体化工艺技术

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN 200510127859 CN1978390A (zh) 2005-12-06 2005-12-06 Pal材料微米、亚微米粉体提纯、超微化一体化工艺技术

Publications (1)

Publication Number Publication Date
CN1978390A true CN1978390A (zh) 2007-06-13

Family

ID=38129726

Family Applications (1)

Application Number Title Priority Date Filing Date
CN 200510127859 Pending CN1978390A (zh) 2005-12-06 2005-12-06 Pal材料微米、亚微米粉体提纯、超微化一体化工艺技术

Country Status (1)

Country Link
CN (1) CN1978390A (zh)

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN103641126A (zh) * 2013-12-11 2014-03-19 甘肃金宇生态环境工程有限公司 一种利用非金属矿物坡缕石制备高性能pal材料的方法
CN103783262A (zh) * 2013-12-11 2014-05-14 甘肃金宇生态环境工程有限公司 一种养殖产业安全、绿色天然饲用材料的制备方法
CN105315097A (zh) * 2015-03-11 2016-02-10 兰州大学 一种生物营养强化肥料的制备方法

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN103641126A (zh) * 2013-12-11 2014-03-19 甘肃金宇生态环境工程有限公司 一种利用非金属矿物坡缕石制备高性能pal材料的方法
CN103783262A (zh) * 2013-12-11 2014-05-14 甘肃金宇生态环境工程有限公司 一种养殖产业安全、绿色天然饲用材料的制备方法
CN105315097A (zh) * 2015-03-11 2016-02-10 兰州大学 一种生物营养强化肥料的制备方法

Similar Documents

Publication Publication Date Title
CN102205972B (zh) 一种凹凸棒土的改性方法
CN104961123A (zh) 一种天然石墨矿剥离提纯方法
CN102513221A (zh) 一种碳酸盐磷矿反浮选组合捕收剂及其制备方法
CN105289837B (zh) 一种利用重晶石‑萤石共生矿制备重晶石粉的工艺
CN103130260B (zh) 一种硫酸钡的生产方法
CN101823722A (zh) 一种由钙基膨润土制备膨润土无机凝胶的方法
CN104445300A (zh) 以磷尾矿为原料用氨循环法制取氢氧化镁、碳酸钙并分离出磷矿的方法
IN2013MU01494A (zh)
CN102936019A (zh) 一种利用高岭土制备磁性4a分子筛的方法
CN101293226B (zh) 一种碳酸盐磷矿反浮选捕收剂
CN101864199A (zh) 一种改性复合超细滑石粉制备方法
CN104060108A (zh) 一种从高钙含钒硅质页岩中提取钒的方法
CN1978361A (zh) Pal材料微米、亚微米粉体提纯工艺技术
CN102452656A (zh) 低品位膨润土的提纯方法
CN103848430B (zh) 一种从钙基膨润土中分离提纯蒙脱石的方法
CN1978390A (zh) Pal材料微米、亚微米粉体提纯、超微化一体化工艺技术
CN101798095B (zh) 富钾岩石预脱硅制备硅酸钾钠溶液的工艺
CN103131873B (zh) 利用混酸分离铝质岩中的锂元素并制备碳酸锂的方法
CN105149219A (zh) 一种用于非洲砂质硅藻土矿的干法选矿方法
CN105149084A (zh) 一种用于非洲砂质硅藻土矿的干湿法选矿方法
CN101700894A (zh) 选矿法制取合成硫酸钾工艺
CN1978063A (zh) Pal材料微米、亚微米粉体超微化工艺技术
CN108393198A (zh) 一种用于微细粒锡石浮选的组合药剂及其使用方法
CN101857256B (zh) 从低品位一水硬铝石型铝土矿中脱除二氧化硅的方法
CN105152716B (zh) 一种磷矿酸法选矿及选矿过程中产生的酸液的处理工艺及应用

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C02 Deemed withdrawal of patent application after publication (patent law 2001)
WD01 Invention patent application deemed withdrawn after publication