CN1873150B - 利用废弃饮料罐、瓶作承重单元制造楼板的方法 - Google Patents
利用废弃饮料罐、瓶作承重单元制造楼板的方法 Download PDFInfo
- Publication number
- CN1873150B CN1873150B CN200510018812XA CN200510018812A CN1873150B CN 1873150 B CN1873150 B CN 1873150B CN 200510018812X A CN200510018812X A CN 200510018812XA CN 200510018812 A CN200510018812 A CN 200510018812A CN 1873150 B CN1873150 B CN 1873150B
- Authority
- CN
- China
- Prior art keywords
- bearing unit
- epoxy adhesive
- beverage
- plastic
- framework
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
一种利用废弃饮料罐、瓶作承重单元制造楼板的方法包括:利用模具生产出泡沫塑料框架2;框架2内放入承重单元1,另一泡沫塑料框架内部都涂上环氧粘接剂后和装有承重单元的框架合拢,加压制成一个整体块;铝合金型材内放有承重单元和注有泡沫或钢筋混凝土;整体块相连置于铝合金框架7内;整体块板上,下表面涂上环氧粘接剂层3,在环氧粘接剂层3上,分别粘贴上彩色钢板4,在上表面层的彩色钢板4装上复合木地板。其优点是:利用废弃饮料罐瓶作承重单元制造楼板重重轻,承重能力强,拆卸移动十分方便、组装快速。
Description
技术领域
本发明涉及建筑材料技术领域,具体地说是一种利用废弃饮料罐、瓶作承重单元制造楼板的方法。
背景技术
随着我国建设的飞跃发展,人民生活水平的提高,饮料基本上都是采用瓶、罐装水,铝罐饮料喝光后丢弃,再回炉,烧损率非常高,利用率低,造成很大的浪费,塑料饮料瓶也是只能回收再造粒利用,利用率也不高,这些薄壁的饮料瓶罐除此以外没有任何出路。
发明内容
本发明的目的是利用废弃饮料罐、瓶作承重单元制出重量轻,承载能力强的楼板。
本发明利用废弃饮料罐、瓶作承重单元制造楼板的方法包括:
1、利用模具生产出阻燃泡沫塑料框架;
2、在泡沫塑料框架内放入承重单元,承重单元和泡沫塑料框架用环氧粘接剂粘接,承重单元和承重单元之间用环氧粘接剂粘接,另一泡沫塑料框架内面都涂上环氧粘接剂后和装有承重单元的框架合拢。并用压力机加压制成一个整体块;
3、用铝合金挤压成的型材制成铝合金框架,铝合金型材内孔放有承重单元和孔空处注有高分子塑料或钢筋混凝土;
4、将前面1、2工序制成的整体块相连面涂上环氧粘接剂,把多个整体块粘接在一起置于铝合金挤压成的型材制成的铝合金框架内;
5、在置于铝合金框架中的制成的整体块板上,下表面涂上环氧粘接剂层,在环氧粘接剂层上,粘贴上彩色钢板,在彩色钢板另一表面上铺上复合木地板或其他饰面材料。
铝合金二片罐承重单元的制造方法可查看同日申请的专利,就是向废铝饮料罐、塑料饮料瓶中充0.6MPA的气体封牢。
本发明利用废弃饮料罐、瓶作承重单元制造楼板的方法的优点是:利用废弃饮料罐瓶作承重单元制造楼板重量轻,承重能力强,拆卸移动十分方便、组装快速。
附图说明
图1为平面结构示意图。
图2为楼板剖面结构图。
具体实施方式
实施例:
利用废弃饮料罐、瓶作承重单元制造楼板的方法包括:
1、利用模具生产出阻燃泡沫塑料框架2;
2、在泡沫塑料框架2内放入承重单元1,承重单元1和泡沫塑料框架2用环氧粘接剂粘接,承重单元1和承重单元1之间用环氧粘接剂粘接,另一泡沫塑料框架内部都涂上环氧粘接剂后和装有承重单元的框架合拢。并用压力机加压制成一个整体块;
3、用铝合金挤压成的型材制成铝合金框架7,铝合金型材内孔放有承重单元和孔空处注有高分子塑料或钢筋混凝土;
4、将前面1、2工序制成的整体块相连面涂上环氧粘接剂,把多个整体块粘接在一起置于铝合金挤压成的型材制成的铝合金框架7内;
5、在置于铝合金框架7中的制成的整体块板上,下表面涂上环氧粘接剂层3,在环氧粘接剂层3上,粘贴上彩色钢板4,在彩色钢板4的另一表面上,粘上复合木地板6。
Claims (1)
1.一种利用废弃饮料罐、瓶作承重单元制造楼板的方法,包括:
①利用模具生产出阻燃泡沫塑料框架(2);
②在泡沫塑料框架(2)内放入向废铝饮料罐、塑料饮料瓶中充0.6MPA的气体封牢的承重单元(1),向废铝饮料罐、塑料饮料瓶中充0.6MPA的气体封牢的承重单元(1)和泡沫塑料框架(2)用环氧粘接剂粘接,向废铝饮料罐、塑料饮料瓶中充0.6MPA的气体封牢的承重单元(1)和向废铝饮料罐、塑料饮料瓶中充0.6MPA的气体封牢的承重单元(1)之间用环氧粘接剂粘接,另一泡沫塑料框架内部都涂上环氧粘接剂后和装有承重单元的框架合拢,并用压力机加压制成一个整体块;
③用铝合金挤压成的型材制成铝合金框架(7),铝合金型材内孔放有承重单元和孔空处注有高分子塑料或钢筋混凝土;
④将前面1、2工序制成的整体块相连面涂上环氧粘接剂,把多个整体块粘接在一起置于铝合金挤压成的型材制成的铝合金框架(7)内;
⑤在置于铝合金框架(7)中的制成的整体块板的下表面涂上环氧粘接剂层(3),在环氧粘接剂层(3)上,粘贴上彩色钢板(4),在彩色钢板(4)的另一表面上,粘上复合木地板(6)。