CN1459468A - 环保型聚氯乙烯 - Google Patents

环保型聚氯乙烯 Download PDF

Info

Publication number
CN1459468A
CN1459468A CN 02115266 CN02115266A CN1459468A CN 1459468 A CN1459468 A CN 1459468A CN 02115266 CN02115266 CN 02115266 CN 02115266 A CN02115266 A CN 02115266A CN 1459468 A CN1459468 A CN 1459468A
Authority
CN
China
Prior art keywords
polyvinyl chloride
calcium
environmental protection
pvc
zinc stabilizer
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 02115266
Other languages
English (en)
Inventor
谭颂斌
李国伟
康明
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
DONGGUAN YINXI PLASTICS Co Ltd
Original Assignee
DONGGUAN YINXI PLASTICS Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by DONGGUAN YINXI PLASTICS Co Ltd filed Critical DONGGUAN YINXI PLASTICS Co Ltd
Priority to CN 02115266 priority Critical patent/CN1459468A/zh
Publication of CN1459468A publication Critical patent/CN1459468A/zh
Pending legal-status Critical Current

Abstract

本发明涉及化工产品技术领域,特指一种环保型聚氯乙烯。本发明由PVC树脂(TK-1000)、轻质钙(CCR)、重质钙(LT-2500)、可塑剂(DINP)、内滑剂(6A)、外滑剂(SA-1807)、环氧大豆油(B-22)、钙锌稳定剂(SA-180)、钙锌稳定剂(SP-1745)、抗氧化剂(1010)、抗紫外线剂(UV)组成,本发明克服了普通聚氯乙烯在加工和使用过程的不足之处,可以达到非常高的安全规范要求与环保要求,同时大大降低了重金属的含量。

Description

环保型聚氯乙烯
技术领域:
本发明涉及化工产品技术领域,特指一种环保型聚氯乙烯。
背景技术:
聚氯乙烯(PVC)是一种可塑性强、用途极为广泛的通用塑胶原料,长期以来,PVC的加工都是使用重金属盐稳定剂,尤其是铅系稳定剂。但是,铅等重金属对人体有害。为了使其达到环保标准,有的厂家使用钙锌稳定剂,这种方式虽然降低了PVC的重金属含量,但同时也降低了PVC的物理性能,随着经济的快速发展和人民生活水平的不断提高,社会对PVC应用的环保性能和其它物理性能提出了越来越严格的要求,怎样才能做到既使PVC达到环保性能,又不降低物理性能,是摆在生产厂家面前的一个急需解决的问题。
发明内容:
本发明的目的就在于针对现有技术的不足之处而提供一种可以解决上述问题的环保聚氯乙烯。
为达到本发明的目的,本发明由采用独特的配方,即:PVC树脂(TK-1000)、轻质钙(CCR)、重质钙(LT-2500)、可塑剂(DINP)、内滑剂(6A)、外滑剂(SA-1807)、环氧大豆油(B-22)、钙锌稳定剂(SA-180)、钙锌稳定剂(SP-1745)、抗氧化剂(1010)、抗紫外线剂(UV)组成,其各成分的配比为:PVC树脂(TK-1000)45%~48%、轻质钙(CCR)8%~10%、重质钙(LT-2500)15.5%~17.5%、可塑剂(DINP)21%~25%、内滑剂(6A)0.4%、外滑剂(SA-1807)0.4%、环氧大豆油(B-22)0.5%~1.0%、钙锌稳定剂(SA-180)2.0%~2.2%、钙锌稳定剂(SP-1745)0.8%~1.2%、抗氧化剂(1010)0.2%、抗紫外线剂(UV)0.2%~0.3%。
通过上述配方设计,本发明克服了普通聚氯乙烯在加工和使用过程的不足之处,可以达到美国UL的安全规范要求与环保要求,其耐老化残率75%以上、绝缘电阻阻值750MΩ/KF以上、加速老化30天不会出现较大的颜色变化,本发明同时还大大降低了重金属的含量,其内的各重金属含量与欧洲EN-71环保标准相比较如下图所示:
                                                             单位:PPM
项目 锑Sb 砷As 钡Ba 镉Cd 铬Cr 铅Pb 汞Hg 硒Se
 EN-71  60  25  1000  75  60  90  60  500
 本发明  <5 <2.8 <10 <5 <5 <5 <6.7 <10
从上表可以看出,本发明的重金属含量远远低于欧洲EN-71环保标准所规定的重金属含量标准,同时也符合美国ASTM963-96、EPA3050B和欧洲PREN1122标准,环保效果十分显著,具有非常好的使用价值。
具体实施方式:
本发明的配方具有如下特点:
1.采用吸水性少的钙锌稳定剂,提高了PVC的绝缘电阻值和耐侯性。
2.添加抗老化剂,克服钙锌稳定剂抗老化性能差的缺陷。
3.采用溴系阻燃剂,既增强阻燃性能,又不含重金属锑。
4.优化其它助剂的组合,如填料、颜料、滑剂等,确保在达到欧美环保标准的同时全面提高其物理性能。
本发明的生产过程由配料、混炼、挤出三大工艺组成,配料就是将各种原材料按配方定量进行配比;混炼就是将定量配比的所有原材料高速混合,挤出就是用双螺杆挤出机将高速混合的原料进行加温塑化,形成塑胶颗粒产品。其生产过程是先配料速混并伴有检测,再将混料塑化并挤压切粒,最后经冷却并检测得出合格品。
上述各原料的配比如下:PVC树脂(TK-1000)45%~48%、轻质钙(CCR)8%~10%、重质钙(LT-2500)15.5~17.5%、可塑剂(DINP)21%~25%、内滑剂(6A)0.4%、外滑剂(SA-1807)0.4%、环氧大豆油(B-22)0.5%~1.0%、钙锌稳定剂(SA-180)2.0%~2.2%、钙锌稳定剂(SP-1745)0.8%~1.2%、抗氧化剂(1010)0.2%、抗紫外线剂(UV)0.2%~0.3%。

Claims (1)

1.环保型聚氯乙烯,其特征在于:它由PVC树脂(TK-1000)、轻质钙(CCR)、重质钙(LT-2500)、可塑剂(DINP)、内滑剂(6A)、外滑剂(SA-1807)、环氧大豆油(B-22)、钙锌稳定剂(SA-180)、钙锌稳定剂(SP-1745)、抗氧化剂(1010)、抗紫外线剂(UV)组成,其各成分的配比为:PVC树脂(TK-1000)45%~48%、轻质钙(CCR)8%~10%、重质钙(LT-2500)15.5~17.5%、可塑剂(DINP)21%~25%、内滑剂(6A)0.4%、外滑剂(SA-1807)0.4%、环氧大豆油(B-22)0.5%~1.0%、钙锌稳定剂(SA-180)2.0%~2.2%、钙锌稳定剂(SP-1745)0.8%~1.2%、抗氧化剂(1010)0.2%、抗紫外线剂(UV)0.2%~0.3%。
CN 02115266 2002-05-24 2002-05-24 环保型聚氯乙烯 Pending CN1459468A (zh)