CN1342827A - 一种防止墙面裂缝的施工方法 - Google Patents

一种防止墙面裂缝的施工方法 Download PDF

Info

Publication number
CN1342827A
CN1342827A CN 00112522 CN00112522A CN1342827A CN 1342827 A CN1342827 A CN 1342827A CN 00112522 CN00112522 CN 00112522 CN 00112522 A CN00112522 A CN 00112522A CN 1342827 A CN1342827 A CN 1342827A
Authority
CN
China
Prior art keywords
wall surface
metope
putty
wire mesh
white cement
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 00112522
Other languages
English (en)
Inventor
郑月山
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN 00112522 priority Critical patent/CN1342827A/zh
Publication of CN1342827A publication Critical patent/CN1342827A/zh
Pending legal-status Critical Current

Abstract

一种防止墙面裂缝的施工方法,首先将墙面处理,确保107胶和白水泥腻子对墙面有较好的连结层,按墙面大小剪好不锈钢网丝,平整地贴在墙面上,用腻子刮压使不锈钢网丝平整、牢固地粘在墙面上,加水保养待墙面干后,再按涂刷工艺施工方法,刷外墙涂料。用这种方法可彻底防止墙面裂缝。

Description

一种防止墙面裂缝的施工方法
本发明涉及一种防止墙面裂缝的施工方法,适用于对建筑物装饰施工。
粉刷墙面裂缝,一直是建筑工程装饰的一大难题,墙面裂缝严重影响装饰效果。至今,尚未发现可长期防止墙面裂缝的可行方案。
本发明的目的是针对建筑物粉刷墙面易出现裂缝现象,提出一种杜绝墙面裂缝的施工方法。
本发明究其引起墙面裂缝造成的原因,一般说来引起墙面裂缝的主要因素有:水灰比、砂灰比的配合比例不当;墙面上、下层接合不当,粉刷施工不当;水泥、砂石质量不合格;长期受干湿、环境腐蚀、墙体内外结构发生变化等。从以上这些引起墙面裂纹的主要因素,从中找出合理的解决办法是:对于新墙面,要求其表面平整,抹光、墙面要求有较好的强度和硬度,保证107胶和白水泥腻子有较好的连结层。对于旧墙,着重解决底层旧涂层处理,采取铲、磨、砂等方法后,再用高压水冲洗,确保底层除净,保证107胶和白水泥腻子有较好的连结层。处理好墙面以后,选用不锈钢丝网作拉接筋,增加墙表面抗拉能力,将不锈钢丝网裁剪成需施工墙面大小,然后贴在墙面上,铺贴时应保证各部位平整,不得有膨起和皱折,满刮压涂一次具有抗水润滑性能的腻子,待干燥1-2小时后,再满收光压平一次,即得到平整、光滑、布满网格的墙面,处理好底层以后,加水保养待墙面干后,按普通涂刷工艺施工刷外墙涂料2-3遍。
下面结合实施例对本发明作进一步详细描述。首先处理好施工墙面,配制腻子,胶泥腻子的组分按重量百分比计为25%107胶、65-70%白水泥、5%石灰粉、润滑剂5%和1-2%抗水剂,乳泥腻子的组分按重量百分比计为苯丙乳液或丙烯酸树脂25%、白水泥65-70%、润滑剂5%和抗水剂1-2%,配腻子时务必充分揽拌混合均匀。取10-15目的不锈钢丝网,按施工墙面的尺寸裁剪好,将剪好的不锈纲丝网平整地贴在墙面上,将胶泥腻子均匀地涂刮在不锈钢丝网上,使不锈钢丝网牢牢地粘贴在墙面上,干燥1-2小时后,再均匀地涂刮一层乳泥腻子,压平,即得到平整、光滑、布满网格的墙面,处理好底层以后,加水保养待墙面干后,按涂刷工艺施工方法,刷外墙涂料2-3遍。采用这种方法处理的外墙,经实地施工,数年观察,未发现墙面裂纹。

Claims (2)

1、一种防止墙面裂缝的施工方法,其特征在于:按墙面大小,剪10-15目不锈钢网丝,将不锈钢网丝平整地贴在墙面上,涂刮一层胶泥腻子,干燥1-2小时,再涂刮一层乳泥腻子,加水保养待墙面干后,再刷外墙涂料。
2、按权利要求1所述的一种防止墙面裂缝的施工方法,其特征在于:按重量百分比计,胶泥腻子组分为:25% 107胶、65-70%白水泥、5%石灰粉、润滑剂5%和1-2%抗水剂;乳泥腻子为:25%苯丙乳液或丙烯酸树酯、65-70%白水泥、5%润滑剂和1-2%抗水剂。
CN 00112522 2000-09-08 2000-09-08 一种防止墙面裂缝的施工方法 Pending CN1342827A (zh)