CN1194110C - 一种无污染含铅废弃物再生纯铅冶炼工艺 - Google Patents

一种无污染含铅废弃物再生纯铅冶炼工艺 Download PDF

Info

Publication number
CN1194110C
CN1194110C CNB001275763A CN00127576A CN1194110C CN 1194110 C CN1194110 C CN 1194110C CN B001275763 A CNB001275763 A CN B001275763A CN 00127576 A CN00127576 A CN 00127576A CN 1194110 C CN1194110 C CN 1194110C
Authority
CN
China
Prior art keywords
kilogram
stirrer
mins
rev
speed
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CNB001275763A
Other languages
English (en)
Other versions
CN1355324A (zh
Inventor
朱卫敏
周正华
沈嘉麟
陈正明
杜平钟
顾秀峰
韩鹰
黄惠明
张�杰
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shanghai Feilun Non-Ferrous Smeltery
Shanghai flywheel Industrial Co., Ltd.
Original Assignee
SHANGHAI FEILUN NON-FERROUS SMELTERY
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SHANGHAI FEILUN NON-FERROUS SMELTERY filed Critical SHANGHAI FEILUN NON-FERROUS SMELTERY
Priority to CNB001275763A priority Critical patent/CN1194110C/zh
Publication of CN1355324A publication Critical patent/CN1355324A/zh
Application granted granted Critical
Publication of CN1194110C publication Critical patent/CN1194110C/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本发明涉及一种无污染含铅废弃物再生纯铅冶炼工艺,其特征是:将含铅废弃物熔化,加入木屑,及以锑、锡、砷含量加入氢氧化钠、硝酸钠,加片碱,硝酸钠搅拌,按分析铜的含量加入赤磷,搅拌机搅拌后去除渣得再生纯铅,本发明优点是能使含铅废弃物再生纯铅冶炼时所去除的灰渣、小颗粒、黑渣重复循环使用而不造成对环境的污染。

Description

一种无污染含铅废弃物再生纯铅冶炼工艺
技术领域
本发明涉及一种铅冶炼工艺,特别是一种无污染含铅废弃物再生纯铅冶炼工艺。
背景技术
目前一般的含铅废弃物再生铅冶炼时由于会产生大量的含铅废渣而容易产生污染,而铅废弃物对人体的危害很大。
发明内容
本发明的目的是提供一种无污染物排出的含铅废弃物再生纯铅冶炼工艺。本发明的技术方案是设计一种无污染含铅废弃物再生纯铅冶炼工艺,其特征是:(1)将含铅废弃物在330℃时熔化,(2)将温度设定在380℃,将0.05~0.075%的木屑加入炉内,放入搅拌机以250转/分速度,搅拌10~15分后撩去灰渣,(3)升温至500℃,搅拌机以250转/分速度,搅拌10~15分后取样分析炉内料的锑、锡、砷含量,以下述比例加入氢氧化钠和硝酸钠,
每千克锑加0.7千克的氢氧化钠和0.4千克的硝酸钠,
每千克锡加0.5千克的氢氧化钠和0.2千克的硝酸钠,
每千克砷加1.0千克的氢氧化钠和0.5千克的硝酸钠,
(4)加入2~3%的片碱,将搅拌机以250转/分速度,搅拌10~15分后加入1.0~1.5%的硝酸钠,搅拌至出现小颗粒去除,(5)再次加入2~3%的片碱,将搅拌机以250转/分速度,搅拌10~15分,加入1.0~2.0%的硝酸钠,搅拌至出现小颗粒去除,(6)将温度设定在340℃~360℃,取炉内样品分析铜的含量,以每千克铜加2千克赤磷的比例加入赤磷,以每次0.5千克的量投入赤磷,搅拌机以250转/分速度,搅拌20~40分后,将搅拌机以100~150转/分速度搅拌,直至出现黑渣,将搅拌机以50转/分速度搅拌去渣,(7)升温至410℃出炉浇铸铅锭。本发明的优点是能使含铅废弃物再生纯铅冶炼时所去除的灰渣、小颗粒、黑渣重复循环使用而不造成对环境的污染。
下面结合实施例对本发明作详细说明,
具体实施方式
(1)将含铅废弃物4000千克在330℃时熔化,(2)将温度设定在380℃,将2~3千克的木屑加入炉内,放入搅拌机以250转/分速度,搅拌10~15分后撩去灰渣,(3)升温至500℃,搅拌机以250转/分速度,搅拌10~15分后取样分析炉内料的锑、锡、砷含量,以下述比例加入氢氧化钠和硝酸钠,
每千克锑加0.7千克的氢氧化钠和0.4千克的硝酸钠,
每千克锡加0.5千克的氢氧化钠和0.2千克的硝酸钠,
每千克砷加1.0千克的氢氧化钠和0.5千克的硝酸钠,
(4)加入100千克的片碱,将搅拌机以250转/分速度,搅拌10~15分后加入50千克的硝酸钠,搅拌至出现小颗粒去除,(5)再次加入100千克的片碱,将搅拌机以250转/分速度,搅拌10~15分,加入50~75千克的硝酸钠,搅拌至出现小颗粒去除,(6)将温度设定在350℃,取炉内样品分析铜的含量,以每千克铜加2千克赤磷的比例加入赤磷,以每次0.5千克的量投入赤磷,搅拌机以250转/分速度,搅拌20~40分后,将搅拌机以100~150转/分速度搅拌,直至出现黑渣,将搅拌机以50转/分速度搅拌去渣,(7)升温至410℃出炉浇铸铅锭。

Claims (1)

1、一种无污染含铅废弃物再生纯铅冶炼工艺,其特征是:(1)将含铅废弃物在330℃时熔化,(2)将温度设定在380℃下,以含铅废弃物重量计将0.05~0.075%的木屑加入炉内,放入搅拌机以250转/分速度,搅拌10~15分后撩去灰渣,(3)升温至500℃,搅拌机以250转/分速度,搅拌10~15分后取样分析炉内料的锑、锡、砷含量,以下述比例加入氢氧化钠和硝酸钠,
      每千克锑加0.7千克的氢氧化钠和0.4千克的硝酸钠,
      每千克锡加0.5千克的氢氧化钠和0.2千克的硝酸钠,
      每千克砷加1.0千克的氢氧化钠和0.5千克的硝酸钠,
(4)加入2~3%的片碱,将搅拌机以250转/分速度,搅拌10~15分后加入1.0~1.5%的硝酸钠,搅拌至出现小颗粒去除,(5)再次加入2~3%的片碱,将搅拌机以250转/分速度,搅拌10~15分,加入1.0~2.0%的硝酸钠,搅拌至出现小颗粒去除,(6)将温度设定在340℃~360℃,取炉内样品分析铜的含量,以每千克铜加2千克赤磷的比例加入赤磷,以每次0.5千克的量投入赤磷,搅拌机以250转/分速度,搅拌20~40分后,将搅拌机以100~150转/分速度搅拌,直至出现黑渣,将搅拌机以50转/分速度搅拌去渣,(7)升温至410℃出炉浇铸铅锭。
CNB001275763A 2000-11-27 2000-11-27 一种无污染含铅废弃物再生纯铅冶炼工艺 Expired - Fee Related CN1194110C (zh)