Prior art keywords
mineral
water
floculating
crushed
floculating agent
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN 96117146
Other languages
English (en)
Other versions
CN1065215C (zh
Inventor
刘炯天
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
China University of Mining and Technology CUMT
Original Assignee
China University of Mining and Technology CUMT
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by China University of Mining and Technology CUMT filed Critical China University of Mining and Technology CUMT
Priority to CN 96117146 priority Critical patent/CN1065215C/zh
Publication of CN1180667A publication Critical patent/CN1180667A/zh
Application granted granted Critical
Publication of CN1065215C publication Critical patent/CN1065215C/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Links

Landscapes

  • Separation Of Suspended Particles By Flocculating Agents (AREA)

Abstract

本发明涉及一种适用闭路澄清水系统的矿物型凝聚剂的使用方法。选用微溶或易溶特性的高价金属离子盐作矿物型凝聚剂,将矿物粉碎至粉末状,以0.1—0.2kg/m3的量加入到已澄清的复用循环水中,通过改变水质达到改变悬浮体等的分散状态,即悬浮体改性,使悬浮的微细颗粒呈凝聚状态。本发明与化学凝聚剂比较,有利于彻底澄清确保水质;对愈呈分散状态悬浮体系,经济性愈好,相对造价愈低;系统运行稳定,不受来料及添加系统波动影响,无二次污染。

Description

矿物型凝聚剂的使用方法
本发明涉及一种利用天然矿物原料作凝聚剂的使用方法。更具体具体说是一种微溶或易溶于水的高价金属离子盐的矿物作凝聚剂的使用方法。
目前,研制和商业化的净水剂都是化学制品。从原理上讲,它们分为两大类:凝聚剂和絮凝剂。凝聚剂主要为无机盐类,它们的作用是通过水中溶解离子压缩双电层,使得微细颗粒相互凝聚。絮凝剂则是通过其大分子的桥联作用使已凝聚的粒团絮凝成更大的絮团而迅速沉降。对于呈凝聚态的悬浮体系,这两种药剂的单独应用或配合均可达到明显澄清水效果。但对于呈分散状态的悬浮体系,实际当中往往由于系统运行不稳定或运行费用太高,使总体净水效果差或失效。另外,使用化学制品的净水剂有二次污染,药剂消耗非常惊人,处理呈分散状态的悬浮体系的费用相当高。
本发明的目的是提供一种能确保悬浮液澄清水,且运行成本大大降低,无二次污染的矿物型凝聚剂的使用方法。对于呈分散状态的悬浮体系,澄清效果也非常好。
本发明的目的可以通过以下方式来实现:一种适用闭路澄清水系统的矿物型凝聚剂的使用方法,选用具有微溶或易溶特性的高价金属离子盐作为矿物型的凝聚剂,这类矿物是:石膏(CaSO4·2H2O)、光卤石(KCl·MgCl2·6H2O)、钾盐镁(KCl·MgSO4·3H2O)和白钠镁钒(Na2SO4·MgSO4·4H2O),将矿物型的凝聚剂粉碎至粉末状,然后,将粉末状的矿物型凝聚剂以粉剂或固水两相混合物,加入到已澄清处理的复用循环水中,加入量为0.1~0.2kg/m3,为了加速溶解,可用泵送或专门机械搅拌进行。
本发明与现有技术相比具有如下效果:本发明采用了矿物原料作凝聚剂,通过改变水质达到改变悬浮体系的分散状态,即悬浮体改性,使悬浮的微细颗粒呈凝聚状态,这样矿物型凝聚剂可完全取代通用的化学类凝聚剂,并减少或不用絮凝剂。本发明与化学型凝聚剂比较:①有利于彻底澄清,确保澄清水质;②愈呈分散状态,悬浮愈好,经济性愈好,相对造价愈低;③系统运行稳定,不易受来料及添加系统波动的影响;④价格便宜,地产、无二次污染。
下面用实施例对本发明作进一步详述:
矿物型凝聚剂取自天然矿物,这些天然矿物具有如下特性:微溶或易溶性,高价金属离子盐;这类矿物是:石膏、光卤石、钾盐镁和白钠镁钒。粉碎后可直接加入到已澄清处理的循环水中,也可将粉末先溶解后加入到澄清的循环水中,为了更进一步加强溶解而不使矿物型凝聚剂沉淀,可用泵送或者专门的机械搅拌,将加入矿物型凝聚剂的溶液送到循环系统中。矿物型凝聚剂加入到悬浮体后,首先在水中溶解并呈离子状态存在,这些离子从根本上改变了悬浮液水质状况,水质硬度和矿化度增加;PH值基本保持不变,依靠高价金属离子压缩颗粒表面双电层,使其失去电性,降低凝聚能垒,便成微细颗粒的凝聚,这种作用实质上把悬浮分散体系从分散态向凝聚态转变,即悬浮分散体系改性。从宏观上讲,矿物型凝聚剂可以取代通用的化学类凝聚剂,甚至减少不用凝聚剂,能达到同样的效果,而费用则降低80%以上。
实施例一:将石膏(CaSO4·2H2O)粉碎至粉末状,以0.15kg/m3加入到澄清处理的复用循环水中,由于杂质存在及添加方式的影响,溶解后残留物大致为15%。投放石膏前,煤泥水的PH值为7.5。将粉末状的石膏粉以0,15kg/m3加入到澄清处理的复用循环水中,用泵送加到循环的煤泥水中,最后得到的澄清的水的水质浊度为6~12,PH值基本保持不变。与用碱式氯化铝和聚丙烯酰胺处理煤泥水相比,降低成本80.22%。
实施例二:将光卤石(KCl·MgCl2·6H2O)粉碎至粉末状,以0.16kg/m3加入到澄清处理的复用循环水中,由于杂质存在及添加方式的影响,溶解后残留物大得为10%。投放光卤石前,煤泥水的PH值为7.6。将粉末状的光卤石以0.16kg/m3加入到澄清处理的复用循环水中,用专门机械搅拌来加强溶解,然后,将加入光卤石的澄清处理水加入到系统中去,最后得到澄清的水的水质浊度为8~10,而PH值基本保持不变,与用碱式氯化铝和聚丙烯酰胺处理煤泥水相比,降低成本81.50%。
实施例三:将钾盐镁(KCl·MgSO4·3H2O)粉碎至粉末状,以0.15kg/m3加入到澄清处理的复用循环水中,由于杂质存在及添加方式的影响,溶解后残留物大得为10%,投钾盐镁前,煤泥水的PH值为7.5。将粉状的钾盐镁以0.15kg/m3加入到澄清处理的复用循环水中,运行后得到澄清的水的水质浊度为10~15,PH值基本保持不变,与用碱式氯化铝和聚丙烯酰胺处理煤泥水相比降低成本80%。
实施例四:将白钠镁钒(Na2SO4·MgSO4·4H2O)粉碎至粉末状,以0.16kg/m3加入到澄清处理的复用循环水中,由于杂质存在及添加方式的影响,溶解后残留物大得为10%,投钾盐镁前,煤泥水的PH值为7.5。将粉状的钾盐镁以0.16kg/m3加入到澄清处理的复用循环水中,运行后得到澄清的水的水质浊度为9~13,PH值基本保持不变,与用碱式氯化铝和聚丙烯酰胺处理煤泥水相比降低成本80%。

Claims (4)

1.一种矿物型凝聚剂的使用方法,其特征在于:将具有微溶或易溶特性的高价金属离子盐的粉末状矿物,以0.1~0.2kg/m3的量加入到已澄清处理的复用循环水中,然后送入系统来改变水质达到对悬浮体改性,使悬浮的微细颗粒呈凝聚状态。
2.根据权利要求1所述的矿物型凝聚剂的使用方法,其特征在于:所述的矿物为石膏、光卤石、钾盐镁或白钠镁钒。
3.根据权利要求1或2所述的矿物型凝聚剂的使用方法,其特征在于:所述的被粉碎至粉末状的矿物以粉剂直接加入。
4.根据权利要求1所述的矿物型凝聚剂的使用方法,其特征在于:所述的被粉碎至粉末状的矿物以固水两相混合物加入。
CN 96117146 1996-10-22 1996-10-22 一种矿物型凝聚剂处理循环水的方法 Expired - Fee Related CN1065215C (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN 96117146 CN1065215C (zh) 1996-10-22 1996-10-22 一种矿物型凝聚剂处理循环水的方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN 96117146 CN1065215C (zh) 1996-10-22 1996-10-22 一种矿物型凝聚剂处理循环水的方法

Publications (2)

Publication Number Publication Date
CN1180667A true CN1180667A (zh) 1998-05-06
CN1065215C CN1065215C (zh) 2001-05-02

Family

ID=5124081

Family Applications (1)

Application Number Title Priority Date Filing Date
CN 96117146 Expired - Fee Related CN1065215C (zh) 1996-10-22 1996-10-22 一种矿物型凝聚剂处理循环水的方法

Country Status (1)

Country Link
CN (1) CN1065215C (zh)

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2007082492A1 (fr) * 2006-01-20 2007-07-26 China University Of Mining And Technology Procédé d'épuration de haute efficacité pour le recyclage d'eau de suspension de charbon
CN104229963A (zh) * 2014-09-16 2014-12-24 中国矿业大学(北京) 一种煤泥水澄清的凝聚剂添加控制方法
CN107100625A (zh) * 2017-05-03 2017-08-29 中国矿业大学 覆岩注水充填降低导高的保水开采方法

Cited By (6)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2007082492A1 (fr) * 2006-01-20 2007-07-26 China University Of Mining And Technology Procédé d'épuration de haute efficacité pour le recyclage d'eau de suspension de charbon
CN100429156C (zh) * 2006-01-20 2008-10-29 中国矿业大学 一种循环煤泥水的高效澄清方法
AU2007207277B2 (en) * 2006-01-20 2011-03-03 China University Of Mining And Technology A high efficiency purifying method for recycling coal slurry water
CN104229963A (zh) * 2014-09-16 2014-12-24 中国矿业大学(北京) 一种煤泥水澄清的凝聚剂添加控制方法
CN104229963B (zh) * 2014-09-16 2016-05-18 中国矿业大学(北京) 一种煤泥水澄清的凝聚剂添加控制方法
CN107100625A (zh) * 2017-05-03 2017-08-29 中国矿业大学 覆岩注水充填降低导高的保水开采方法

Also Published As

Publication number Publication date
CN1065215C (zh) 2001-05-02

Similar Documents

Publication Publication Date Title
US3932275A (en) Process for the treatment of mineral slimes
US4783265A (en) Water treatment
JPS6128361B2 (zh)
CN101935095B (zh) 一种聚硅酸絮凝剂的制备方法
CN106745624A (zh) 一种无机‑有机杂化絮凝材料及其制备方法
CN107512799A (zh) 壳聚糖改性黏土的方法及其除藻技术应用
CN104445749B (zh) 一种选矿尾矿废水的处理方法
WO2021128922A1 (zh) 2-(3-取代脲基)-n-羟基-2-氧乙酰亚胺基氰化物类化合物在浮选中的应用
CN102963967A (zh) 选钼尾矿浆处理药剂及其制备方法
CN108495821A (zh) 用于从废水中去除硫酸盐和金属的组合物和方法
CN1065215C (zh) 一种矿物型凝聚剂处理循环水的方法
EP0784596B1 (en) Purification of polar liquid wastes containing suspended solvated particles
CN101492192A (zh) 一种含氟废水处理用混凝剂及其应用工艺
WO2021128771A1 (zh) 2-氰基-n-(取代氨甲酰)乙酰胺类化合物在含钙矿物浮选中的应用
EP0056793A1 (en) A pumpable composition for water-purifying purpose containing iron(II)sulphate
JPH09276604A (ja) 凝塊剤
JP4272122B2 (ja) 凝集沈殿水処理方法及び装置
CN1018629B (zh) 一种复合高分子混凝剂及配制方法
JP2006320836A (ja) 汚濁水処理用瞬間凝集剤とこれを用いた汚濁水処理方法
CN109319896A (zh) 用粉煤灰和钒钛磁铁矿制备絮凝剂的方法
JP2003245504A (ja) 排水の処理方法及びその装置
JPH10309403A (ja) 粉体状凝集剤組成物及び凝集処理方法
CN109157870B (zh) 一种用于澄清含有粘性物质的悬浮液的组合物
CN1308990A (zh) 一种复合絮凝剂及使用方法
RU2675871C1 (ru) Способ осаждения сапонитовой пульпы с применением кальцийалюмосиликатного реагента

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C14 Grant of patent or utility model
GR01 Patent grant
C19 Lapse of patent right due to non-payment of the annual fee
CF01 Termination of patent right due to non-payment of annual fee