CN1113884A - 烧碱的生产方法 - Google Patents

烧碱的生产方法 Download PDF

Info

Publication number
CN1113884A
CN1113884A CN 94110619 CN94110619A CN1113884A CN 1113884 A CN1113884 A CN 1113884A CN 94110619 CN94110619 CN 94110619 CN 94110619 A CN94110619 A CN 94110619A CN 1113884 A CN1113884 A CN 1113884A
Authority
CN
China
Prior art keywords
caustic soda
production
causticizing
lowered
concentration
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 94110619
Other languages
English (en)
Inventor
门伟
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN 94110619 priority Critical patent/CN1113884A/zh
Publication of CN1113884A publication Critical patent/CN1113884A/zh
Pending legal-status Critical Current

Abstract

本发明是烧碱的生产方法,属化工生产领域。
本发明采用苛化法生产烧碱,生产中采用过量碳酸钠反应,苛化完毕后,经低温析出Na2CO3制得高浓度的NaOH溶液可不经蒸发浓缩直接生产浓度大于30%的液体烧碱产品。从而使生产工艺简单化,生产成本较低,生产能耗也较少。

Description

本发明是烧碱的生产方法,属化工生产领域。
已知的生产烧碱的苛化法,只能生产10%的烧碱溶液,为生产液碱产品,需消耗大量的能源进行蒸发浓缩,从而使生产工艺复杂,生产成本高,本发明的目的在于采用苛化法直接生产NaOH含量≥42%的液体烧碱产品,从而使生产工艺大为简化,节约大量能源生产成本降低,发明的实施方法如下:
在1000份重量的水中,维持25-120℃的温度加入200-1200份重量的Na2CO3,加入50-1350份重量的Ca(OH)2搅拌反应0.5-50小时,使溶液的Na2CO3大部分转化为NaOH。苛化反应完毕后,过滤所得溶液,得到固体CaCO3,水洗后废弃,过滤母液降温至-10-20℃析出Na2CO3·10H2O结晶,分离的结晶作为Na2CO3及水原料重新用于前述配料生产进行苛化反应,即此部分结晶在生产过程中循环使用,所得的分离母液为NaOH重量含量>10%的烧碱溶液。采用上述工艺可制得NaOH重量含量≥42%,杂质Na2CO3重量含量<3%的液碱商品,直接出售使用。
烧碱是基本无机化学工业产品,在国民经济中有着重要的地位,目前大量采用的烧碱生产方法是电解法,此法由于联产氯产品,使烧碱的产量受氯产品市场的影响,这就使烧碱的供应发生困难。如美国最近已开始重新采用苛化法进行烧碱生产。用本发明的方法,可简易地大量生产低成本的烧碱,满足市场需求,具有良好的经济效益和社会效益。

Claims (1)

1、烧碱的生产方法,其特征在于:在1000份重量的水中,加入200-1200份重量的Na2CO3,加入50-1350份重量的Ca(OH)2,进行苛化反应,苛化反应完毕后,将分离反应沉淀物后的分离母液降温至-10-20℃,分离析出的Na2CO3·10H2O结晶循环使用,重新作为原料用于苛化生产,分离母液为液碱产品。
CN 94110619 1994-06-01 1994-06-01 烧碱的生产方法 Pending CN1113884A (zh)