CN110924360A - 一种混凝土构筑物沉降缝的修复方法 - Google Patents
一种混凝土构筑物沉降缝的修复方法 Download PDFInfo
- Publication number
- CN110924360A CN110924360A CN201910836060.XA CN201910836060A CN110924360A CN 110924360 A CN110924360 A CN 110924360A CN 201910836060 A CN201910836060 A CN 201910836060A CN 110924360 A CN110924360 A CN 110924360A
- Authority
- CN
- China
- Prior art keywords
- settlement joint
- repairing
- settlement
- adhesive
- joint
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种混凝土构筑物沉降缝的修复方法,属于水工构筑物工程领域。该沉降缝修复方法包括清理、防渗处理、填充、防水,以及加固保护和养护等步骤。该方法在修复混凝土沉降缝的同时,双层速效堵漏水泥夹止水条并外贴柔性防水材料的结构既保证了构筑物的防渗漏效果,又保持了原有的柔性结构,使构筑物更能抵抗温度变化、沉降等因素的影响,适用于池壁、底板等部位,且施工方法简便、修复效果好。
Description
技术领域
本发明涉及水工构筑物工程领域,尤其涉及一种混凝土构筑物沉降缝的修复方法。
背景技术
在大型混凝土构筑物的设计和施工中,由于构筑物超长、超宽,常会采用各种变形缝来适应温湿度变形、地基沉降、地震等影响,放置埋入式止水带的沉降缝是最为常见的结构之一。然而柔性的沉降缝处往往是整个混凝土构筑物最薄弱的环节,常由于多种因素发生渗漏,而常用的混凝土裂缝修复方法往往会破坏了沉降缝处原有的柔性结构,并不适合沉降缝的功能要求。
发明内容
为了克服现有技术的不足,本发明的目的在于提供一种既防渗漏,又能保持柔性结构的混凝土构筑物沉降缝的修复方法。
本发明所采用的技术方案如下:
一种混凝土构筑物沉降缝的修复方法,主要包括以下步骤:
清理:将构筑物中的水排空,清除沉降缝中原有填充物,将沉降缝两侧混凝土表面清理干净,必要时进行打磨,如有蜂窝、空洞等提前进行修补;
防渗处理:第一层填充速效堵漏水泥;再填充遇水膨胀止水条;之后再填充一层速效堵漏水泥;
填充:在沉降缝口处用木条连续封堵,之后向空隙中灌注填充物,灌注完成后拆去木条;
防水:保持沉降缝周围池壁平整、干燥、干净,用粘合剂将防水的固定材料粘在池壁上,对修复后的沉降缝起到防水作用。
进一步地,还包括加固保护步骤:在固定材料粘贴牢固后,可抹压粘结砂浆保护层,再抹压抗裂砂浆,之后再涂刷两道永凝液,涂刷时要把砂浆边沿各扩大50mm范围为宜。
进一步地,还包括养护:夏季要及时苫盖并进行喷水养生,冬季要注意保温。
相比现有技术,本发明的有益效果在于:
在修复混凝土沉降缝的同时,双层速效堵漏水泥夹止水条并外贴柔性防水材料的结构既保证了构筑物的防渗漏效果,又保持了原有的柔性结构,使构筑物更能抵抗温度变化、沉降等因素的影响,适用于池壁、底板等部位,且施工方法简便、修复效果好。
附图说明
图1为池内壁沉降缝缝修复方法剖面示意图。
图2为池底板沉降缝缝修复方法剖面示意图。
具体实施方式
本实施例提供了一种混凝土构筑物沉降缝的修复方法,主要方法为:
清理:将构筑物中的水排空,清除沉降缝中原有填充物,将沉降缝两侧混凝土表面用钢丝刷清理干净,必要时可用金刚砂布进行打磨,如有蜂窝、空洞等提前进行修补;
防渗处理:第一层填充40mm速效堵漏水泥,抹平、密实、避免残留物;待水泥干后,再填充遇水膨胀止水条,必须保证沉降缝内密实填满,必要时可以再添加一层遇水膨胀橡胶条,能更进一步地增加防水功能;之后再填充一层40mm速效堵漏水泥,这样做是为了保证在橡胶条在遇水膨胀时,有一个很好的约束环境;
填充:在沉降缝口处用木条连续封堵,木条间隔300mm留一个10mm孔,之后向空隙中灌注填充物,灌注完成后24h拆去木条;
防水:保持沉降缝周围池壁平整、干燥、干净,用粘合剂将防水的固定材料粘在池壁上,对修复后的沉降缝起到防水作用。
加固保护:在固定材料粘贴牢固后,可抹压粘结砂浆保护层,再抹压抗裂砂浆,之后再涂刷两道永凝液,涂刷时要把砂浆边沿各扩大50mm范围为宜。
养护:夏季要及时苫盖并进行喷水养生,冬季要注意保温。
优选地,所述填充用填充物为聚氨酯发泡剂。
优选地,所述固定用粘合剂可为氯丁胶,涂胶厚度0.05mm,固定材料可为氯丁橡胶片或氯丁橡胶板等,厚度2mm左右。
优选地,所述粘结砂浆保护层厚度5-6mm,抗裂砂浆厚度5-6mm。
上述实施方式仅为本发明的优选实施方式,不能以此来限定本发明保护的范围,本领域的技术人员在本发明的基础上所做的任何非实质性的变化及替换均属于本发明所要求保护的范围。
Claims (4)
1.一种混凝土构筑物沉降缝的修复方法,其特征在于:
清理:将构筑物中的水排空,清除沉降缝中原有填充物,将沉降缝两侧混凝土表面清理干净,必要时进行打磨,如有蜂窝、空洞等提前进行修补;
防渗处理:第一层填充速效堵漏水泥;再填充遇水膨胀止水条;之后再填充一层速效堵漏水泥;
填充:在沉降缝口处用木条连续封堵,之后向空隙中灌注填充物,灌注完成后拆去木条;
防水:保持沉降缝周围池壁平整、干燥、干净,用粘合剂将防水的固定材料粘在池壁上,对修复后的沉降缝起到防水作用。
2.如权利要求1所述的沉降缝修复方法,其特征在于:
还包括加固保护步骤:在固定材料粘贴牢固后,可抹压粘结砂浆保护层,再抹压抗裂砂浆,之后再涂刷两道永凝液。
3.如权利要求1-2所述的沉降缝修复方法,其特征在于:
所述填充步骤的填充剂为聚氨酯发泡剂。
4.如权利要求1-2所述的沉降缝修复方法,其特征在于:
所述固定用粘合剂为氯丁胶,固定材料为氯丁橡胶片或氯丁橡胶板。