CN110415607A - 显示面板及其制作方法 - Google Patents
显示面板及其制作方法 Download PDFInfo
- Publication number
- CN110415607A CN110415607A CN201910672175.XA CN201910672175A CN110415607A CN 110415607 A CN110415607 A CN 110415607A CN 201910672175 A CN201910672175 A CN 201910672175A CN 110415607 A CN110415607 A CN 110415607A
- Authority
- CN
- China
- Prior art keywords
- metal wire
- display panel
- substrate
- modified layer
- side edge
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
一种显示面板及其制作方法,所述显示面板制作方法用于改善金属漏光,包括将基板通过蚀刻方法进行蚀刻,将基板通过蚀刻方法进行蚀刻后,在所述基板的金属线侧边缘设置改性层,在所述基板的金属线侧边缘设置改性层后,移除所述基板上的光阻层。通过设置改性层吸收衍射光的反射,达到减少金属线侧边缘漏光,提升显示画面对比度的效果。
Description
【技术领域】
本揭示涉及显示技术领域,具体涉及显示面板及其制作方法。
【背景技术】
请一并参阅图1及图2,其分别为现有技术的显示面板的上视示意图与图1中R1位置的横截面示意图,如图所示,由基板S下方向上照射的入射光IR1为线偏振光,且面板上的金属线ML交叉处不是直角,因此金属线ML边缘会产生衍射SC1,衍射SC1再被金属线ML边缘的金属锥(Metal Taper)反射,从而产生反射光RF1,导致现有显示面板普遍存在的漏光问题。
故,有需要提供一种显示面板及其制作方法,以解决现有技术存在的问题。
【发明内容】
为解决上述问题,本揭示提出一种显示面板及其制作方法,其可达到减少金属线侧边缘漏光,提升显示画面对比度的效果。
为达成上述目的,本揭示提供一种显示面板制作方法,用于改善金属漏光,包括将基板通过蚀刻方法进行蚀刻,将基板通过蚀刻方法进行蚀刻后,在所述基板的金属线侧边缘设置改性层,在所述基板的金属线侧边缘设置改性层后,移除所述基板上的光阻层。
于本揭示其中的一实施例中,所述改性层是通过氧化方法设置在所述金属线上。
于本揭示其中的一实施例中,所述改性层是通过热处理方法设置在所述金属线上。
于本揭示其中的一实施例中,所述改性层是通过离子注入方法设置在所述金属线上。
于本揭示其中的一实施例中,所述金属线的材料包含铜。
为达成上述目的,本揭示还提供一种显示面板,用于改善金属漏光,包括基板;金属线,设置在所述基板上,其中所述金属线的侧边缘设置有改性层。
于本揭示其中的一实施例中,所述改性层的含氧量高于所述金属线的侧边缘的含氧量。
于本揭示其中的一实施例中,所述改性层的含碳量高于所述金属线的侧边缘的含碳量。
于本揭示其中的一实施例中,所述改性层的离子含量高于所述金属线的侧边缘的离子含量。
由于本揭示的显示面板及其制作方法,所述显示面板制作方法用于改善金属漏光,包括将基板通过蚀刻方法进行蚀刻,将基板通过蚀刻方法进行蚀刻后,在所述基板的金属线侧边缘设置改性层,在所述基板的金属线侧边缘设置改性层后,移除所述基板上的光阻层。通过设置改性层吸收衍射光的反射,达到减少金属线侧边缘漏光,提升显示画面对比度的效果。
为让本揭示的上述内容能更明显易懂,下文特举优选实施例,并配合所附图式,作详细说明如下:
【附图说明】
图1显示现有技术的显示面板的俯视示意图;
图2显示图1中R1位置的横截面示意图;
图3显示根据本揭示的一实施例的显示面板制作方法流程图;
图4显示根据本揭示的一实施例的显示面板的第一状态的方块示意图;
图5显示根据本揭示的一实施例的显示面板的第二状态的方块示意图;
图6显示根据本揭示的一实施例的显示面板的第三状态的方块示意图;
【具体实施方式】
以下实施例的说明是参考附加的图示,用以例示本揭示可用以实施的特定实施例。本揭示所提到的方向用语,例如[上]、[下]、[前]、[后]、[左]、[右]、[内]、[外]、[侧面]等,仅是参考附加图式的方向。因此,使用的方向用语是用以说明及理解本揭示,而非用以限制本揭示。
在图中,结构相似的单元是以相同标号表示。
请参照图3,其显示根据本揭示的一实施例的显示面板制作方法流程图,其中,显示面板制作方法包含:
流程S1:将基板通过蚀刻方法进行蚀刻。
流程S2:将基板通过蚀刻方法进行蚀刻后,在所述基板的金属线侧边缘设置改性层。
流程S3:在所述基板的金属线侧边缘设置改性层后,移除所述基板上的光阻层。
于本揭示其中的一实施例中,所述改性层T1是通过氧化方法设置在所述金属线M1上。
于本揭示其中的一实施例中,所述改性层T1是通过热处理方法设置在所述金属线M1上。
于本揭示其中的一实施例中,所述改性层T1是通过离子注入方法设置在所述金属线M1上。
请参照图4、图5及图6,其分别显示根据本揭示的一实施例的显示面板的第一状态的方块示意图、根据本揭示的一实施例的显示面板的第二状态的方块示意图及根据本揭示的一实施例的显示面板的第三状态的方块示意图。
本揭示提供一种显示面板制作方法,用于改善金属漏光,如图4绘示显示面板的第一状态40,其中,基板B1上方设置有金属线M1,光阻层PR设置金属线M1上方。在显示面板的第一状态下,可将基板B1通过蚀刻方法进行蚀刻。请进一步参阅图5,图5绘示显示面板的第二状态50,其中,金属线M1的侧边缘Mf进一步设置有改性层T1。请进一步参阅图6,图6绘示显示面板的第三状态60,其中,金属线M1上方的光阻层PR被移除。
请进一步参阅图6,在第三状态下的显示面板60中,通过增加设置改性层T1于金属线M1的侧边缘Mf上,使得由基板B1下方向上照射的入射光IR1产生衍射SC2照射改性层T1,通过改性层T1的粗造表面对入射光形成漫反射,减少衍射SC2的镜面反射。换言之,相较于先前技术,本发明的显示面板进一步达到减少金属线M1漏光以提升显示面板的显示画面对比度的效果。
于本揭示一实施例中,改性层T1覆盖金属线M1的侧边缘Mf。
于本揭示其中的一实施例中,所述改性层T1的含氧量高于所述金属线M1的侧边缘Mf的含氧量。
于本揭示其中的一实施例中,所述改性层T1的含碳量高于所述金属线M1的侧边缘Mf的含碳量。
于本揭示其中的一实施例中,所述改性层T1的离子含量高于所述金属线M1的离子含量。
于本揭示其中的一实施例中,所述金属线M1的材料包含铜。
于本揭示其中的一实施例中,所述改性层T1的构成材料包含氧化铜。
于本揭示其中的一实施例中,通过对所述金属线M1施加氧化电浆(O2 plasma)处理,生成改性层T1。举例而言,当所述金属线M1的构成材料包含铜,所述改性层T1的构成材料包含氧化铜。
由于本揭示的面板及其制作方法,所述显示面板制作方法用于改善金属漏光,包括将基板通过蚀刻方法进行蚀刻,将基板通过蚀刻方法进行蚀刻后,在所述基板的金属线侧边缘设置改性层,在所述基板的金属线侧边缘设置改性层后,移除所述基板上的光阻层。通过设置改性层吸收衍射光的反射,达到减少金属线侧边缘漏光,提升显示画面对比度的效果。
尽管已经相对于一个或多个实现方式示出并描述了本揭示,但是本领域技术人员基于对本说明书和附图的阅读和理解将会想到等价变型和修改。本揭示包括所有这样的修改和变型,并且仅由所附权利要求的范围限制。特别地关于由上述组件执行的各种功能,用于描述这样的组件的术语旨在对应于执行所述组件的指定功能(例如其在功能上是等价的)的任意组件(除非另外指示),即使在结构上与执行本文所示的本说明书的示范性实现方式中的功能的公开结构不等同。此外,尽管本说明书的特定特征已经相对于若干实现方式中的仅一个被公开,但是这种特征可以对给定或特定应用而言是期望和有利的其他实现方式的一个或多个其他特征组合。而且,就术语“包括”、“具有”、“含有”或其变形被用在具体实施方式或权利要求中而言,这样的术语旨在以与术语“包含”相似的方式包括。
以上仅是本揭示的优选实施方式,应当指出,对于本领域普通技术人员,在不脱离本揭示原理的前提下,还可以做出若干改进和润饰,这些改进和润饰也应视为本揭示的保护范围。
Claims (10)
1.一种显示面板制作方法,其特征在于,包括:
将基板通过蚀刻方法进行蚀刻;
将基板通过蚀刻方法进行蚀刻后,在所述基板的金属线侧边缘设置改性层;
在所述基板的金属线侧边缘设置改性层后,移除所述基板上的光阻层。
2.如权利要求1所述的显示面板制作方法,其特征在于,所述改性层是通过氧化方法设置在所述金属线上。
3.如权利要求1所述的显示面板制作方法,其特征在于,所述改性层是通过热处理方法设置在所述金属线上。
4.如权利要求1所述的显示面板制作方法,其特征在于,所述改性层是通过离子注入方法设置在所述金属线上。
5.如权利要求1所述的显示面板,其特征在于,所述金属线的材料包含铜。
6.一种显示面板,其特征在于,包括:
基板;
金属线,设置在所述基板上;
其中所述金属线的侧边缘设置有改性层。
7.如权利要求1所述的显示面板,其特征在于,所述改性层的含氧量高于所述金属线的侧边缘的含氧量。
8.如权利要求1所述的显示面板,其特征在于,所述改性层的含碳量高于所述金属线的侧边缘的含碳量。
9.如权利要求1所述的显示面板,其特征在于,所述改性层的离子含量高于所述金属线的侧边缘的离子含量。
10.如权利要求1所述的显示面板,其特征在于,所述金属线的材料包含铜。