CN109653469A - The levelling floor construction method of anti-hollowing essence - Google Patents
The levelling floor construction method of anti-hollowing essence Download PDFInfo
- Publication number
- CN109653469A CN109653469A CN201910097294.7A CN201910097294A CN109653469A CN 109653469 A CN109653469 A CN 109653469A CN 201910097294 A CN201910097294 A CN 201910097294A CN 109653469 A CN109653469 A CN 109653469A
- Authority
- CN
- China
- Prior art keywords
- absolute altitude
- altitude control
- control piece
- floor
- horizontal absolute
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The present invention relates to technical field of building construction, aiming at the problem that hollowing is easy to appear after ground tile paving, provide a kind of levelling floor construction method of anti-hollowing essence, comprising the following steps: S1, base cleaning;It is S2, thick levelling;S3, floor leveling;S4, it is laid with cement sand bed;S5, floor tile pretreatment;S6, ground tile paving.Height by controlling concrete layer is not less than 4cm, is conducive to the uniformity for improving concrete layer, so that concrete is not easy crack phenomenon occur during conserving molding, advantageously reduces after floor is laid with and is easy to appear hollowing.
Description
Technical field
The present invention relates to technical field of building construction, more specifically, it relates to a kind of levelling floor construction of anti-hollowing essence
Method.
Background technique
The superficial layer on floor, i.e. house earth surface or flooring, is made by timber or other materials.
Existing floor construction is usually first in base's laying dry cement mortar and levelling, then in dry cement bonded sand
Floor tile is adhered to be made by adhesive on slurry.But it is larger due to usually containing sand, stone isodensity in dry cement mortar
Gather materials, since sand, stone are easy that stirring is uneven in stirring so that be placed in the strength of cement mortar of top section compared with
It is weak.When dry cement mortar is during drying and moulding, and surface dehydration is too fast, be easy to cause in capillary generate compared with
Big negative pressure and dry cement mortar volume is sharply shunk, thus be easy so that being placed in the strong of the concrete of top section
Degree is difficult to resist the contraction of itself, so that dry cement mortar is easy to produce cracking, and then floor is easy to cause hollowing occur
The phenomenon that, therefore, still there is improved space.
Summary of the invention
In view of the deficiencies of the prior art, the present invention intends to provide a kind of anti-hollowing essence levelling floor construction side
Method has the advantages that reducing floor hollowing occurs.
To achieve the above object, the present invention provides the following technical scheme that
A kind of levelling floor construction method of anti-hollowing essence, comprising the following steps:
S1, base cleaning;
It is S2, thick levelling: pea gravel concreten bed course to be laid in base, the height of the pea gravel concreten bed course is not less than, and leads to
Cross the thick leveling concrete bed course of surveying setting-out;
S3, floor leveling: by making several consistent horizontal absolute altitude control pieces of shape size, the horizontal absolute altitude control piece is extremely
Few there are two planar horizontals to be arranged, and determines the position of horizontal absolute altitude control piece by measurement, then by horizontal absolute altitude control piece its
In a horizontal plane be bonded with the upper surface of pea gravel concreten layer, use the fixed horizontal absolute altitude control of polymer cement mortar
Part, and the upper surface of the horizontal absolute altitude control piece is controlled in same level height;
S4, it is laid with cement sand bed: being laid with cement sand bed on pea gravel concreten layer, led at once by aluminium side in horizontal absolute altitude
Control piece upper surface rolling, so that the upper surface of cement sand bed is flushed with the upper surface of horizontal absolute altitude control piece;
S5, floor tile pretreatment: it in one layer of back rubberised layer of floor tile backside coating and dries in the shade;
S6, ground tile paving: adhesive is coated on the back rubberised layer of floor tile and floor tile is adhered on cement sand bed, through conserving
Form floor.
By adopting the above technical scheme, 4cm is not less than by control concrete layer, so that the height of concrete layer subtracts significantly
It is small, though so that sand, stone in pea gravel concreten are settled down to bottom, it is also not far at the top of pea gravel concreten layer, thus favorably
In the uniformity for improving pea gravel concreten layer, so that concrete is not easy crack phenomenon occur during conserving molding, into
And advantageously reduce the case where being easy to appear hollowing phenomenon after floor is laid with;By first using the levelling horizontal absolute altitude control of infrared essence
The upper surface of part re-lays cement sand bed, so that cement mortar so that the upper surface of several horizontal absolute altitude control pieces flushes
Layer is flushed with the upper surface of horizontal absolute altitude control piece, is conducive to the levelling precision for improving cement sand bed, so that cement sand bed
Levelling error range controls within 4mm, consequently facilitating the laying of floor tile so that floor tile when being laid with without again levelling,
Be conducive to improve construction efficiency, meanwhile, so that being not easy between floor tile and cement sand bed there are gap, so that floor is not
It is easy to appear hollowing phenomenon;In addition, horizontal absolute altitude control piece can also play a supportive role to floor tile, so that the intensity of cement sand bed
Enhancing, so that cement sand bed is not easily susceptible to cracking, so that floor is not easy the phenomenon that hollowing occur;By elder generation on ground
One layer of back gluing of brick backside coating, then floor tile is adhered on cement sand bed with clay, be conducive to back gluing and be completely covered ground
The back side of brick, so that be not easy that there are gaps between the floor tile back side and back gluing, meanwhile, back gluing and adhesive have good
Compatibility, so that be not easy after ground tile paving is on cement sand bed, between floor tile and cement sand bed there are gap, into
And floor is made to be not easy hollowing phenomenon occur.
The present invention is further arranged to: the horizontal absolute altitude control piece is equipped with through-hole, and the through-hole runs through horizontal absolute altitude
Two horizontally disposed planes of control piece, in the step S3, behind the position for determining horizontal absolute altitude control piece, and by infrared
After line measuring instrument absolute altitude, polymer cement mortar, and the horizontal mark of adjustment before polymer cement mortar initial set are poured into through-hole
The height of high control piece makes the level height of the upper surface of horizontal absolute altitude control piece reach the absolute altitude of the infrared measurement machine;
By adopting the above technical scheme, after by the position of the horizontal absolute altitude control piece of determination, into through-hole, joints cement is with will be horizontal
Absolute altitude control piece is pre-fixed on concrete layer, convenient for the fixation of horizontal absolute altitude control piece, so that horizontal absolute altitude control piece is consolidated
Fixed operation is not necessarily to while carrying out manual fixation, is conducive to improve working efficiency;Meanwhile so that horizontal absolute altitude control piece is not easy to send out
The upward displacement of unboiled water square, the precision of the position for the absolute altitude control piece that is conducive to improve the standard, to be conducive to improve floor tile
Mat formation the accuracy of position.
The present invention is further arranged to: the polymer water silt particle in the step S3, in horizontal absolute altitude control piece through-hole
After starching drying and moulding, polymer cement mortar is smeared close to the periphery of pea gravel concreten layer one end in horizontal absolute altitude control piece, is made
Horizontal absolute altitude control piece is obtained to be fixed on pea gravel concreten layer.
By adopting the above technical scheme, by the through-hole of horizontal absolute altitude control piece joints cement to pre-fix after, then
Horizontal absolute altitude control piece smears cement close to the periphery of concrete layer one end with fixation, is conducive to enhancing horizontal absolute altitude control piece position
The stability set, so that horizontal absolute altitude control piece is less likely to occur to be displaced after being fixed, to be conducive to absolute altitude control of improving the standard
The position precision of product, so that the position of mating formation of floor tile is more accurate.
The present invention is further arranged to: in the step S4, the upper surface of cement sand bed and horizontal absolute altitude control piece
Upper surface flushes.
By adopting the above technical scheme, it is not less than 2cm by controlling the height of cement sand bed, is conducive to reinforced cement mortar
The intensity of layer, so that cement sand bed is not easily susceptible to cracking when being pressurized, so that being not easy between floor tile and cement sand bed
There are gaps, so that floor is not easy hollowing phenomenon occur.
The present invention is further arranged to: in the step S5, floor tile includes natural stone floor tile, artificial stone floor tile and ceramic tile,
Before natural stone floor tile coats back gluing, six face protective treatments first are carried out to natural stone floor tile.
By adopting the above technical scheme, since natural stone floor tile is as made of the direct sanding and polishing of natural stone, without other
Processing is conducive to improve natural stone floor tile by first carrying out six face protective treatments to natural stone floor tile before gluing is carried on the back in coating
Waterproof performance and alkali prevention performance, to be conducive to extend the service life of natural stone floor tile.
The present invention is further arranged to: in the step S6, after maintenance, the gap between adjacent floor tile is using U.S. seam
Treasured sealing.
By adopting the above technical scheme, the precious gap sealed between adjacent floor tile is stitched by using beauty, is conducive to improve floor
Impervious waterproof performance so that water is not easy to infiltrate into cement sand bed and concrete layer, to be conducive to extend cement
The service life of screed and concrete layer, so that cement sand bed and concrete layer are not easily susceptible to cracking, so that ground
Brick is not easy hollowing phenomenon occur;Meanwhile so that the gap between adjacent floor tile is not easy to shelter evil people and countenance evil practices, so that being adjacent to
Gap between brick is not allowed to be also easy to produce mould, and the cleaning for being also convenient for floor is swept;In addition, also helping the beautiful effect on enhancing floor
Fruit, so that the class on floor improves, to be conducive to improve the economic value on floor.
The present invention is further arranged to: in the step S6, floor tile reserves expansion joint in process of deployment, adjacent described to stretch
Spacing between contracting seam is 4-5 meters.
By adopting the above technical scheme, by reserving expansion joint during ground tile paving, be conducive to carry out building element
Protection so that building element because climate temperature changes expand with heat and contract with cold the case where when, building element is not allowed to be also easy to produce
Crack, to be conducive to extend the service life of building element.
The present invention is further arranged to: in the step S6, described adhesive uses soft flexible organic clay.
By adopting the above technical scheme, by using soft flexible organic clay as adhesive, so that adhesive has
There is certain elasticity, be conducive to the toughness for enhancing adhesive, so that adhesive floor tile is not easily susceptible to cracking when being pressurized;Together
When, also help enhancing floor tramples comfort level.
In conclusion the invention has the following advantages:
1. the height by control concrete layer is to be conducive to the uniformity for improving pea gravel concreten layer not less than 4cm, so that mixed
Solidifying soil is not easy crack phenomenon occur during conserving molding, advantageously reduces after floor is laid with and is easy to appear hollowing;
2. being poured by the upper surface of the first infrared levelling horizontal absolute altitude control piece of essence, then by the through-hole toward horizontal absolute altitude control piece
Polymer cement mortar layer can adjust the height of horizontal absolute altitude control piece, poly- before polymer cement mortar layer not initial set
After closing the drying of object cement mortar, the height of the upper surface of horizontal absolute altitude control piece is flushed, is conducive to improve cement sand bed
Levelling precision, so that the levelling error range of cement sand bed controls within 4mm, so that between floor tile and cement sand bed not
It is easy there are gap, so that floor tile is not easy hollowing occur;
3. horizontal absolute altitude control piece plays a supportive role to floor tile, so that cement sand bed is not easily susceptible to cracking, so that floor is not
It is easy to appear hollowing;
4. by the way that first floor tile is adhered on cement sand bed in one layer of back gluing of floor tile backside coating, then with clay, so that ground
It is not easy that there are gaps between the brick back side and back gluing, meanwhile, so that be not easy between floor tile and cement sand bed there are gap,
So that floor is not easy hollowing occur.
Specific embodiment
With reference to embodiments, invention is further described in detail.
A kind of levelling floor construction method of anti-hollowing essence, comprising the following steps:
S1, base cleaning, specific as follows:
With scour without sediment motion base, surface dust, dust in base are removed, then base is cleaned up, by the dirt removal in base
Completely, it dries, and by the soil compaction of base.
It is S2, thick levelling, specific as follows:
The dimensional parameters of base are measured according to architectural drawing, and are done in base according to architectural drawing, by level corresponding
Graticule and production ash cake absolute altitude.
Pea gravel concreten is poured in base to form pea gravel concreten bed course, control pea gravel concreten bed course pours height
Degree is 5cm, and passes through the elevation line marked slightly levelling pea gravel concreten bed course, so that the upper surface water of pea gravel concreten bed course
It is flat.
S3, ground essence are levelling, specific as follows:
It pours to form the consistent horizontal absolute altitude control piece of several shape sizes, in the present embodiment, horizontal absolute altitude control using cement
Product is cylindrical, and the center of horizontal absolute altitude control piece, which is run through, has through-hole so that the section of horizontal absolute altitude control piece is in circle
It is cyclic annular.The outer diameter of horizontal absolute altitude control piece is 20cm, and the internal diameter of horizontal absolute altitude control piece is 5cm, the height of horizontal absolute altitude control piece
Degree is 2cm.
After pea gravel concreten bed course, which conserves, to be formed, horizontal absolute altitude control piece is determined according to architectural drawing and by measurement
Position, and the fixation position of horizontal absolute altitude control piece is marked, it is corresponding solid that horizontal absolute altitude control piece is then placed in its
Positioning is set, so that the annulus bottom surface of horizontal absolute altitude control piece is bonded with the upper surface of concrete cushion.Adjacent level absolute altitude control
At a distance of 1.5m between product.
Polymer water slurry liquid then is poured into the through-hole of horizontal absolute altitude control piece, so that horizontal absolute altitude control piece is pre- solid
Due on concrete layer.
Then by the upper surface of the levelling horizontal absolute altitude control piece of infrared ray essence, the wherein height of the infrared measurement machine absolute altitude
Height than horizontal absolute altitude control piece is higher by 2mm, makes the upper surface of horizontal absolute altitude control piece by lifting horizontal absolute altitude control piece
Height reach the height of infrared ray absolute altitude.When raising horizontal absolute altitude control piece, it is located at not pre-hardening in horizontal absolute altitude control piece
Polymer cement mortar flowed to out of through-hole between horizontal absolute altitude control piece lower surface and pea gravel concreten layer upper surface between
Gap.
After the polymer water slurry liquid in the through-hole of horizontal absolute altitude control piece is dry, in horizontal absolute altitude control piece close to mixed
The outer circumferential walls of solidifying soil layer one end smear polymer water slurry liquid again, so that horizontal absolute altitude control piece is fixed on pea gravel concreten layer
On.
S4, it is laid with cement sand bed, specific as follows:
After the polymer cement mortar for fixing of horizontal absolute altitude control piece outer circumferential walls is dry, filled on concrete cushion
Cement mortar is filled the water, and is conserved to form cement sand bed.It is logical by aluminium side between every two adjacent horizontal absolute altitude control piece
The upper surface of cement sand bed is flushed with the upper surface of horizontal absolute altitude control piece.
S5, floor tile pretreatment, specific as follows:
Floor tile includes natural stone floor tile, artificial stone floor tile and ceramic tile.First uniformly it is coated in six outer surfaces of natural stone floor tile
Machine silicon waterproof coating, when coating organosilicon waterproof coating, respectively in the horizontal and vertical each painting of the front and back of natural stone floor tile
It covers primary.After the completion of organic silicon water-proofing coating is coated and is conserved, then respectively to natural stone floor tile, artificial stone floor tile or ceramic tile
The back side uniformly coats back gluing, and stands 10h-12h, to form back rubberised layer, while to carry on the back rubberised layer far from the floor tile back side
Plane it is parallel with tile surface.
S6, ground tile paving, specific as follows:
Organic clay is uniformly coated on the back rubberised layer at the floor tile back side, then floor tile is adhered to cement mortar by organic clay
On layer, so that floor tile is fixed on cement sand bed.
During being laid with floor tile, expansion joint is reserved, is spaced 4.5m between adjacent expansion seam.
After the completion of floor tile is pasted, 14h is conserved, then be coated in the gap of adjacent floor tile using U.S. seam treasured, so that phase
Gap sealing before adjacent floor tile, to form floor.
The embodiment of present embodiment is presently preferred embodiments of the present invention, not limits protection of the invention according to this
Range, therefore: the equivalence changes that all structures under this invention, shape, principle are done, should all be covered by protection scope of the present invention it
It is interior.
Claims (8)
1. a kind of levelling floor construction method of anti-hollowing essence, it is characterized in that: the following steps are included:
S1, base cleaning;
It is S2, thick levelling: pea gravel concreten bed course is laid in base, the height of the pea gravel concreten bed course is not less than 4cm, and
Pass through the thick leveling concrete bed course of surveying setting-out;
S3, floor leveling: by making several consistent horizontal absolute altitude control pieces of shape size, the horizontal absolute altitude control piece is extremely
Few there are two planar horizontals to be arranged, and determines the position of horizontal absolute altitude control piece by measurement, then by horizontal absolute altitude control piece its
In a horizontal plane be bonded with the upper surface of pea gravel concreten layer, use the fixed horizontal absolute altitude control of polymer cement mortar
Part, and the upper surface of the horizontal absolute altitude control piece is controlled in same level height;
S4, it is laid with cement sand bed: being laid with cement sand bed on pea gravel concreten layer, led at once by aluminium side in horizontal absolute altitude
Control piece upper surface rolling, so that the upper surface of cement sand bed is flushed with the upper surface of horizontal absolute altitude control piece;
S5, floor tile pretreatment: it in one layer of back rubberised layer of floor tile backside coating and dries in the shade;
S6, ground tile paving: adhesive is coated on the back rubberised layer of floor tile and floor tile is adhered on cement sand bed, through conserving
Form floor.
2. the levelling floor construction method of anti-hollowing essence according to claim 1, it is characterized in that: the horizontal absolute altitude control piece
It is equipped with through-hole, the through-hole runs through two horizontally disposed planes of horizontal absolute altitude control piece, in the step S3, determines water
Behind the position of flat absolute altitude control piece, and by after the infrared measurement machine absolute altitude, pouring polymer cement mortar into through-hole, and
The height of the horizontal absolute altitude control piece of adjustment before polymer cement mortar initial set, keeps the level of the upper surface of horizontal absolute altitude control piece high
Degree reaches the absolute altitude of the infrared measurement machine.
3. the levelling floor construction method of anti-hollowing essence according to claim 2, it is characterized in that: working as water in the step S3
After polymer cement mortar drying and moulding in flat absolute altitude control piece through-hole, in horizontal absolute altitude control piece close to pea gravel concreten layer
Polymer cement mortar is smeared in the periphery of one end, so that horizontal absolute altitude control piece is fixed on pea gravel concreten layer.
4. the levelling floor construction method of anti-hollowing essence according to claim 1 to 3, it is characterized in that: the step S4
In, the upper surface of cement sand bed is flushed with the upper surface of horizontal absolute altitude control piece.
5. the levelling floor construction method of anti-hollowing essence according to claim 1 to 3, it is characterized in that: the step S5
In, floor tile includes natural stone floor tile, artificial stone floor tile and ceramic tile, before natural stone floor tile coats back gluing, to natural stone first
Brick carries out six face protective treatments.
6. the levelling floor construction method of anti-hollowing essence according to claim 1 to 3, it is characterized in that: the step S6
In, after maintenance, the gap between adjacent floor tile is using the precious sealing of U.S. seam.
7. the levelling floor construction method of anti-hollowing essence according to claim 1 to 3, it is characterized in that: the step S6
In, it is the expansion joint 8mm-10mm that floor tile reserves width in process of deployment, and the spacing between the adjacent expansion joint is 4-5 meters.
8. the levelling floor construction method of anti-hollowing essence according to claim 1 to 3, it is characterized in that: the step S6
In, described adhesive uses soft flexible organic clay.