CN109609089A - 一种煤炭抑尘剂及其制备方法 - Google Patents
一种煤炭抑尘剂及其制备方法 Download PDFInfo
- Publication number
- CN109609089A CN109609089A CN201811171817.XA CN201811171817A CN109609089A CN 109609089 A CN109609089 A CN 109609089A CN 201811171817 A CN201811171817 A CN 201811171817A CN 109609089 A CN109609089 A CN 109609089A
- Authority
- CN
- China
- Prior art keywords
- dust
- sodium
- coal
- mixing powder
- follows
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明涉及一种防止粉尘飞扬的抑尘剂,特别是一种煤炭抑尘剂及其制备方法。本发明的技术方案是:一种煤炭抑尘剂,其特征在于该抑尘剂是由质量百分比为:1—1.5%的混合粉剂和98.5—99%的水混合而成,其中混合粉剂是由质量百分比为:35—50%的羧甲基纤维素钠、23—30%羧甲基淀粉钠、19—25%硅酸钠、7—11%柠檬酸和0.4—1.0%聚丙烯酰胺混合而成。本发明中各组分来源广泛,配制简单,可以将粉剂先配制在一起,应用中只需将粉剂和水按比例调配后,喷洒在需要防尘物料表面,就可在其表面形成固化层,可有效防止粉尘对环境的污染,具有使用非常方便、价格低等特点。
Description
所属技术领域
本发明涉及一种防止粉尘飞扬的抑尘剂,特别是一种煤炭抑尘剂及其制备方法。
背景技术
煤炭运输过程中产生的煤尘污染是粉尘污染的一个主要来源。在我国煤炭运输一般都采用敞车运输,运输过程中,由于颠簸、风力、压差等原因造成煤粒扬尘,对环境形成污染。针对形成煤尘污染的污染源煤炭运输人们也采取了很多办法来抑制煤尘的形成,比如拉煤过程中给煤车盖篷布、向煤车喷水、煤车表面喷专用煤炭抑尘剂等方法,这些方法或多或少解决拉煤过程中煤尘飞扬的问题。例如给煤车盖篷布解决了拉煤过程中煤尘飞扬的问题,但比较费时,也会存在篷布被吹开或者破裂等问题;向煤车喷水煤尘暂时得到抑制,随着水分的蒸发,煤尘表面又会变得干燥,又会扬尘,只能在拉煤的过程中间隔喷水才会有好的效果,但条件又不具备;目前比较好的办法是给煤车表面喷洒专用的煤炭抑尘剂,操作方法简单,又能解决以上方法的不足,但由于煤炭抑尘剂价格较高,一般在每吨1.5—2万元,给煤炭运输企业造成较大的经济负担,制约了煤炭抑尘剂的使用。
发明内容
本发明的的目是提供一种低成本、生产方便、使用效果好的一种煤炭抑尘剂及其制备方法。
本发明的技术方案是:一种煤炭抑尘剂,其特征在于该抑尘剂是由质量百分比为:1—1.5%的混合粉剂和98.5—99%的水混合而成,其中混合粉剂是由质量百分比为:35—50%的羧甲基纤维素钠、23—30%羧甲基淀粉钠、19—25%硅酸钠、7—11%柠檬酸和0.4—1.0%聚丙烯酰胺混合而成。
上述羧甲基纤维素钠、羧甲基淀粉钠、硅酸钠、柠檬酸和聚丙烯酰胺的纯度均为工业级。
制备上述权利要求所述煤炭抑尘剂的方法,该方法的生产步骤为:
步骤一:混合粉剂的制备:按质量百分比为:35—50%的羧甲基纤维素钠、23—30%羧甲基淀粉钠、19—25%硅酸钠、7—11%柠檬酸和0.4—1.0%聚丙烯酰胺混合;
步骤二:将上述混合粉剂在常温状态下搅拌溶解后即为抑尘剂;
上述混合粉剂与水的重量比为1—1.5:98.5—99。
在本发明的技术方案中,羧甲基纤维素钠、羧甲基淀粉钠是主要的成膜剂,配合使用,形成网络结构,能保证煤炭表面形成较厚的固化层。柠檬酸可以调节煤炭抑尘剂的PH值在6~8之间。硅酸钠在PH值6~8时能形成粘性硅酸胶状物,能增加抑尘剂的粘性和吸湿性,同时增加固化层的强度。添加少量的聚丙烯酰胺可以使抑尘剂形成一种共聚物,进一步增加抑尘剂的粘性,将煤粒紧紧粘结在一起。本发明中硅酸钠和柠檬酸的配合使用可以大大降低羧甲基纤维素钠的用量,硅酸钠和柠檬酸的价格是羧甲基纤维素钠价格的一半,极大的降低了抑尘剂的成本,使用效果也和含有大量羧甲基纤维素钠的抑尘剂使用效果一样。
本发明中各组分来源广泛,配制简单,可以将粉剂先配制在一起,应用中只需将粉剂和水按比例调配后,喷洒在需要防尘物料表面,就可在其表面形成固化层,可有效防止粉尘对环境的污染,使用非常方便,吨价格只是现有抑尘剂价格的一半左右。
具体实施方式
以制备1000Kg煤炭抑尘剂为例,对本技术方案说明如下。
实施例1:
步骤一:混合粉剂的制备:称取4.2Kg的羧甲基纤维素钠、2.5Kg的羧甲基淀粉钠、2.1Kg的硅酸钠、0.8Kg的柠檬酸和0.4Kg的聚丙烯酰胺将其混合得10Kg混合粉剂;
上述羧甲基纤维素钠、羧甲基淀粉钠、硅酸钠、柠檬酸和聚丙烯酰胺的纯度均为工业级。
步骤二:在搅拌状态下将上述10 Kg的混合粉剂加入到990Kg的水中,搅拌20分钟充分溶解后,即可做为抑尘剂喷洒在需要防止粉尘污染的物质表面,如喷洒在拉煤车车厢中煤的表面,就可使表面的煤形成固化层,有效防止了煤炭运输过程中,粉尘对环境的污染。
实施例2:
步骤一:混合粉剂的制备:称取7.5Kg的羧甲基纤维素钠、3.45Kg的羧甲基淀粉钠、2.85Kg的硅酸钠、1.05Kg的柠檬酸和0.15Kg的聚丙烯酰胺混合得15Kg的混合粉剂;
上述羧甲基纤维素钠、羧甲基淀粉钠、硅酸钠、柠檬酸和聚丙烯酰胺的纯度均为工业级。
步骤二:在搅拌状态下将上述15 Kg的混合粉剂加入到985Kg的水中,搅拌30分钟混合均匀后,即可做为抑尘剂喷洒在需要防止粉尘污染的物质表面,如喷洒在拉煤车车厢中煤的表面,就可使表面的煤形成固化层,有效防止了煤炭运输过程中,粉尘对环境的污染。
实施例3:
步骤一:混合粉剂的制备:称取4.6Kg的羧甲基纤维素钠、3.9Kg的羧甲基淀粉钠、3.3Kg的硅酸钠、1.4Kg的柠檬酸和0.5Kg的聚丙烯酰胺混合得13.7Kg的混合粉剂;
上述羧甲基纤维素钠、羧甲基淀粉钠、硅酸钠、柠檬酸和聚丙烯酰胺的纯度均为工业级。
步骤二:在搅拌状态下将上述13.7 Kg的混合粉剂加入到986.3Kg的水中,搅拌25分钟混合均匀后,即可做为抑尘剂喷洒。
Claims (3)
1.一种煤炭抑尘剂,其特征在于该抑尘剂是由质量百分比为:1—1.5%的混合粉剂和98.5—99%的水混合而成,其中混合粉剂是由质量百分比为:35—50%的羧甲基纤维素钠、23—30%羧甲基淀粉钠、19—25%硅酸钠、7—11%柠檬酸和0.4—1.0%聚丙烯酰胺混合而成。
2.根据权利要求1所述的煤炭抑尘剂,其特征在于上述羧甲基纤维素钠、羧甲基淀粉钠、硅酸钠、柠檬酸和聚丙烯酰胺的纯度均为工业级。
3.制备上述权利要求所述煤炭抑尘剂的方法,该方法的生产步骤为:
步骤一:混合粉剂的制备:按质量百分比为:35—50%的羧甲基纤维素钠、23—30%羧甲基淀粉钠、19—25%硅酸钠、7—11%柠檬酸和0.4—1.0%聚丙烯酰胺混合;
步骤二:将上述混合粉剂在常温状态下搅拌溶解后即为抑尘剂;
上述混合粉剂与水的重量比为1—1.5:98.5—99。