CN109531039A - 辊筒轴承室磨损修复方法 - Google Patents
辊筒轴承室磨损修复方法 Download PDFInfo
- Publication number
- CN109531039A CN109531039A CN201811110411.0A CN201811110411A CN109531039A CN 109531039 A CN109531039 A CN 109531039A CN 201811110411 A CN201811110411 A CN 201811110411A CN 109531039 A CN109531039 A CN 109531039A
- Authority
- CN
- China
- Prior art keywords
- bearing
- chamber surface
- worn
- bearing chamber
- prosthetic material
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种辊筒轴承室磨损修复方法,包括下述步骤:1、在轴承室表面涂抹脱模剂,然后晾干;2、再在轴承室表面烤油,然后打磨;3、清洗轴承室表面;4、将金属修复材料均匀涂抹至磨损的轴承室表面,然后使用样板尺沿油槽基准面刮出修复尺寸;5、金属修复材料初固化后,打磨修复轴承室表面及高点;6、再次涂抹少量金属修复材料后直接装配轴承。本发明的特点是:操作简单,修复工作方便快捷,延长压延机的使用寿命,减少停机时间,保证生产效率。
Description
技术领域
本发明涉及压延机维护领域,具体涉及一种压延机的辊筒轴承室磨损修复方法。
背景技术
压延机是借助于辊筒间强大的剪切力,并配以相应的加工温度,使黏流态的物料多次受到挤压和延展作用,最终成为具有宽度和厚度的薄片制品的一种加工设备,压延机的轴承组件保证辊筒的正常转动,但在使用过程中,轴承容易磨损,磨损严重时影响生产。
发明内容
本发明的目的在于克服上述不足问题,提供一种辊筒轴承室磨损修复方法。
本发明为实现上述目的所采用的技术方案是:辊筒轴承室磨损修复方法,包括下述步骤:1、在轴承室表面涂抹脱模剂,然后晾干;2、再在轴承室表面烤油,然后打磨;3、清洗轴承室表面;4、将金属修复材料均匀涂抹至磨损的轴承室表面,然后使用样板尺沿油槽基准面刮出修复尺寸;5、金属修复材料初固化后,打磨修复轴承室表面及高点;6、再次涂抹少量金属修复材料后直接装配轴承。
采用无水乙醇清洗轴承室表面。
轴承室表面烤油后用磨光机或砂纸打磨。
使用砂纸打磨修复轴承室表面及高点。。
本发明的特点是:操作简单,修复工作方便快捷,延长压延机的使用寿命,减少停机时间,保证生产效率。
具体实施方式
本发明为一种辊筒轴承室磨损修复方法,包括下述步骤:1、在轴承室表面涂抹薄薄一层脱模剂,越薄越好,晾干备用,2、在轴承室表面烤油,用磨光机或砂纸打磨;3、用无水乙醇清洗表面,确保表面干净、干燥、结实;4、将金属修复材料均匀涂抹至磨损的轴承室表面,然后使用样板尺沿油槽基准面刮出修复尺寸;5、待金属修复材料初固化后,使用砂纸打磨修复轴承室表面及高点;6、再次涂抹薄薄一层少量的金属修复材料后直接装配轴承即可。
以上所述,仅为本发明较佳的具体实施方式,但本发明的保护范围并不局限于此,任何熟悉本技术领域的技术人员在本发明披露的技术范围内,根据本发明的技术方案及其发明构思加以等同替换或改变,都应涵盖在本发明的保护范围之内。
Claims (4)
1.辊筒轴承室磨损修复方法,其特征在于包括下述步骤:
1、在轴承室表面涂抹脱模剂,然后晾干;
2、再在轴承室表面烤油,然后打磨;
3、清洗轴承室表面;
4、将金属修复材料均匀涂抹至磨损的轴承室表面,然后使用样板尺沿油槽基准面刮出修复尺寸;
5、金属修复材料初固化后,打磨修复轴承室表面及高点;
6、再次涂抹少量金属修复材料后直接装配轴承。
2.如权利要求1所述的辊筒轴承室磨损修复方法,其特征在于:采用无水乙醇清洗轴承室表面。
3.如权利要求1所述的辊筒轴承室磨损修复方法,其特征在于:轴承室表面烤油后用磨光机或砂纸打磨。
4.如权利要求1所述的辊筒轴承室磨损修复方法,其特征在于:使用砂纸打磨修复轴承室表面及高点。