CN108708067A - A kind of warp knit lace and its method for weaving - Google Patents
A kind of warp knit lace and its method for weaving Download PDFInfo
- Publication number
- CN108708067A CN108708067A CN201810597038.XA CN201810597038A CN108708067A CN 108708067 A CN108708067 A CN 108708067A CN 201810597038 A CN201810597038 A CN 201810597038A CN 108708067 A CN108708067 A CN 108708067A
- Authority
- CN
- China
- Prior art keywords
- warp knit
- weaving
- spacer screen
- lace
- comb
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The present invention relates to a kind of warp knit lace and its method for weaving, the weaving of warp knit lace spacer screen includes the following steps:Braiding, pre-setting, sizing.The improvement that above-mentioned technical proposal passes through technique so that form three kinds of warp binds of the spacer screen structure of lace together, the relative position of yarn has been fixed.Warp knit lace spacer screen after cutting apart with a knife or scissors, detect by an unaided eye find rabbet at it is smooth, be not in contraction, curling metaboly pull or wash after will not deform.
Description
Technical field
The present invention relates to textile technology field, more particularly to a kind of warp knit lace and its method for weaving.
Background technology
Warp knit lace is well received in the market in underwear, underpants.Elastic warp knit lace on the market does clothing at present, cuts out version
After rabbet must be avoided in later stage washing, decoherenced in wearing process, performance is influenced along one layer of lining cloth of rabbet overseam.This
A operational sequence had both increased the cost of manufacture of production firm, and the edge after overseam is since thickness increases, the comfort level of dress
It is greatly reduced.Also occurs the arbitrary sanction scheme of some warp knit high speed machine plain cloths on the market at present, by originally at comb of enclosing the land
On the basis of be added one it is identical walk yarn track lopping spandex, shunk using two kinds of raw materials inconsistent, cut apart with a knife or scissors after-contraction and block line
Circle, reaches arbitrary sanction purpose.But this method is limited in warp knit high speed machine plain cloth and can play a role, and multi-bar passes through
Volume machine is jacquard comb due to providing broadwise connection, including provides the spandex comb of elastic reaction, how does not have lopping function
It is always the problem of this kind of type to make on-run in broadwise.
Invention content
For this reason, it may be necessary to provide a kind of method for weaving for solving the problems, such as multi-bar warp knitting machine sanction version sealing and decoherencing.
To achieve the above object, a kind of method for weaving of warp knit lace is inventor provided, the warp knit lace spacer screen
Weaving includes the following steps:
Braiding:It is woven using multi-bar warp knitting machine, the sley bar includes that ground comb, jacquard comb and spandex are combed, describedly
Comb uses spandex covered yarn, the spandex comb and jacquard comb band yarn in the same direction using spandex covered yarn, jacquard comb;Obtain warp knit lace
Spacer screen semi-finished product;
Pre-setting:By warp knit lace spacer screen semi-finished product be put into forming machine carry out pre-setting, forming machine speed be 25-28 codes/
Minute, temperature is 180-190 DEG C;Combed in the step, jacquard comb charging spandex covered yarn in spandex can with spandex comb in
Spandex it is melt bonded.
Sizing:The spacer screen semi-finished product of pre-setting are carried out shaping with forming machine, forming machine speed be set as 25-28 codes/point
Clock, temperature setting are 160-180 DEG C, obtain warp knit lace spacer screen.
Further, further include following deoiling step:Machine is washed with water in woven warp knit lace spacer screen semi-finished product to carry out
Oil removing is washed, washing temperature is 99-101 DEG C, and speed is 24-26 codes/minute, washing time 2-5 minutes;The deoiling step exists
After the braiding step, before the pre-setting step.
Further, the twist of the spandex covered yarn is twisted for 600-800.
Further, the upper secret degree of yarn be 15-23 rows/centimetre, in order to make comb, jacquard comb, spandex comb three kinds
Yarn material is in close contact, and weaving debugging web frame compacts direction tune, and adjustment direction is that tightly comb send Jacquard to be advisable;The warp knit
The density of lace spacer screen semi-finished product be 38-45 rows/centimetre, ensure that finished product has the requirement of enough elasticity and texture softness, ammonia
It is in the same direction that synthetic fibre, which combs direction with jacquard comb direction,.
Inventor additionally provides a kind of warp knit lace, the warp knit lace by any of the above-described method for weaving weaving and
At.
It is different from the prior art, the improvement that above-mentioned technical proposal passes through technique so that form the three of the spacer screen structure of lace
Kind warp binds together, fixed by the relative position of yarn.After cutting apart with a knife or scissors spacer screen, detects by an unaided eye and find flower bud at rabbet
Silk is smooth, is not in the metaboly of contraction, curling, is not in deformation after pullling or washing.Using in the lace
Clothing cut out the rabbet after version, not in the case of overseam, are deformed in deformation or water-washing process even if pullling in use, due to ammonia
There is synthetic fibre restorative and yarn relative position to have fixed, and loosens and may return to reset condition later, durable.The present invention knits
The warp knit lace made, underwear producer are not necessarily to overseam after cutting out version, directly make underpants, not only reduce recruitment cost, but also increase
The comfort level of client's dress, competitiveness greatly enhance.
Specific implementation mode
For the technology contents of technical solution, construction feature, the objects and the effects are described in detail, below in conjunction with specific reality
Example is applied to be explained in detail.
Embodiment 1
A kind of weaving of warp knit lace, the weaving of wherein spacer screen include the following steps:
Braiding:It is woven using multi-bar warp knitting machine, the sley bar includes that ground comb, jacquard comb and spandex are combed, describedly
The spandex that comb and jacquard comb are twisted using 700 coats nylon, and spandex comb uses 210D spandexs;The spandex covered yarn twist is set as 600
It twists -800 to twist, the twist is excessively high, and spandex is exposed very little, and bonding is few, and the twist is too low, and yarn and spandex obvolvent are poor, cause finished product flash.
The spandex comb and jacquard comb band yarn in the same direction;It in order to make combs, jacquard comb, spandex are combed three kinds of yarn materials and closely connect
Touch, weaving debugging web frame compacts direction tune, upper secret degree be arranged 20 rows/centimetre, adjustment direction is tightly to comb to send the Jacquard to be
Preferably;Make spacer screen even closer, constraint is a little big, and net bottom structure is not easy to slip;In order to meet sufficiently resilient demand, finished product density
Be arranged 40 rows/centimetre, ensure that finished product has enough elasticity;While in order to meet into the requirement of quality sense softness, spandex comb side
It is in the same direction to same jacquard comb direction.
Oil removing;Machine is washed with water in woven warp knit lace spacer screen semi-finished product and carries out washing oil removing, washing temperature 100
DEG C, speed is 25 yards/minute, washing time 3 minutes;
Pre-setting:Warp knit lace spacer screen semi-finished product are subjected to pre-setting with forming machine, forming machine speed is set as 26 yards/point
Clock, temperature setting are 185 DEG C;Combed in the step, jacquard comb charging spandex covered yarn in spandex can with spandex comb in
Spandex is melt bonded, and the relative position of yarn is fixed, and warp knit lace spacer screen is cut out to the rabbet after version, not in the case of overseam,
It is deformed in deformation or water-washing process even if pullling in use, since there is spandex restorative and yarn relative position to have consolidated
It is fixed, reset condition can be returned to after loosening.
Sizing:The warp knit lace spacer screen semi-finished product of pre-setting are carried out shaping with forming machine, forming machine speed is set as 26
Code/minute, temperature setting are 170 DEG C, obtain warp knit lace spacer screen.
It is compound:Spacer screen and lace surface layer is compound, complete the weaving of warp knit lace fabric.
For 1 obtained warp knit lace spacer screen of embodiment after cutting apart with a knife or scissors, detecting by an unaided eye, it is smooth at rabbet to find, is not in
It shrinks, the metaboly of curling;It will not deform, decoherence after stretching or washing 100 times, it is durable.
Embodiment 2
A kind of weaving of warp knit lace, the weaving of wherein spacer screen include the following steps:
Braiding:It is woven using multi-bar warp knitting machine, the sley bar includes that ground comb, jacquard comb and spandex are combed, describedly
The spandex that comb is twisted using 600 coats nylon, and jacquard comb uses 800 spandex covered yarns twisted, spandex comb to use 210D spandexs;Ground
Comb, Jacquard raw material use spandex covered yarn, the spandex covered yarn twist to be set as 600 twirls -800 twirl, and the twist is excessively high, and spandex is exposed too
Few, bonding is few, and the twist is too low, and yarn and spandex obvolvent are poor, cause finished product flash.
The spandex comb and jacquard comb band yarn in the same direction;It in order to make combs, jacquard comb, spandex are combed three kinds of yarn materials and closely connect
Touch, weaving debugging web frame compacts direction tune, upper secret degree be arranged 23 rows/centimetre, adjustment direction is tightly to comb to send the Jacquard to be
Preferably;In order to meet sufficiently resilient demand, finished product density be arranged 45 rows/centimetre, ensure that finished product has enough elasticity;While in order to
Meet into the requirement of quality sense softness, it is in the same direction that spandex, which combs direction with jacquard comb direction,.
Oil removing;Machine is washed with water in woven warp knit lace spacer screen semi-finished product and carries out washing oil removing, washing temperature 101
DEG C, speed is 24 yards/minute, washing time 5 minutes;
Pre-setting:Warp knit lace spacer screen semi-finished product are subjected to pre-setting with forming machine, forming machine speed is set as 28 yards/point
Clock, temperature setting are 190 DEG C;Combed in the step, jacquard comb charging spandex covered yarn in spandex can with spandex comb in
Spandex is melt bonded, and the relative position of yarn is fixed, and warp knit lace spacer screen is cut out to the rabbet after version, not in the case of overseam,
It is deformed in deformation or water-washing process even if pullling in use, since there is spandex restorative and yarn relative position to have consolidated
It is fixed, reset condition can be returned to after loosening.
Sizing:The warp knit lace spacer screen semi-finished product of pre-setting are carried out shaping with forming machine, forming machine speed is set as 25
Code/minute, temperature setting are 160 DEG C, obtain warp knit lace spacer screen.
It is compound:Spacer screen and lace surface layer is compound, complete the weaving of warp knit lace fabric.
With 2 obtained warp knit lace spacer screen of embodiment after cutting apart with a knife or scissors, detecting by an unaided eye, it is smooth at rabbet to find, will not go out
The metaboly for now shrinking, crimping will not deform after stretching or washing 100 times, decoherence, durable.
Embodiment 3
A kind of method for weaving of warp knit lace spacer screen, the weaving of wherein spacer screen include the following steps:
Braiding:It is woven using multi-bar warp knitting machine, the sley bar includes that ground comb, jacquard comb and spandex are combed, describedly
The spandex covered yarn that comb is twisted using 800, jacquard comb use 700 spandex covered yarns twisted, spandex comb to use 210D spandexs;Spandex packet
It covers twist per unit and is set as 600 twirls -800 twirl, the twist is excessively high, and spandex is exposed very little, and bonding is few, and the twist is too low, and yarn and spandex are embraced
It is poor to close, and causes finished product flash.
The spandex comb and jacquard comb band yarn in the same direction;It in order to make combs, jacquard comb, spandex are combed three kinds of yarn materials and closely connect
Touch, weaving debugging web frame compacts direction tune, upper secret degree be arranged 15 rows/centimetre, adjustment direction is tightly to comb to send the Jacquard to be
Preferably;In order to meet sufficiently resilient demand, finished product density be arranged 38 rows/centimetre, ensure that finished product has enough elasticity and texture
Softness, it is in the same direction that spandex, which combs direction with jacquard comb direction,.
Oil removing;Machine is washed with water in woven warp knit lace spacer screen semi-finished product and carries out washing oil removing, washing temperature is 99 DEG C,
Speed is 26 yards/minute, washing time 2 minutes;
Pre-setting:Warp knit lace spacer screen semi-finished product are subjected to pre-setting with forming machine, forming machine speed is set as 28 yards/point
Clock, temperature setting are 187 DEG C;Combed in the step, jacquard comb charging spandex covered yarn in spandex can with spandex comb in
Spandex is melt bonded, and the relative position of yarn is fixed, and warp knit lace finished product is cut out to the rabbet after version, not in the case of overseam,
It is deformed in deformation or water-washing process even if pullling in use, since there is spandex restorative and yarn relative position to have consolidated
It is fixed, reset condition can be returned to after loosening.
Sizing:The warp knit lace spacer screen semi-finished product of pre-setting are carried out shaping with forming machine, forming machine speed is set as 28
Code/minute, temperature setting are 180 DEG C, obtain warp knit lace spacer screen finished product.
It is compound:Spacer screen and lace surface layer is compound, complete the weaving of warp knit lace fabric.
With 3 obtained warp knit lace spacer screen of embodiment after cutting apart with a knife or scissors, detecting by an unaided eye, it is smooth at rabbet to find, will not go out
The metaboly for now shrinking, crimping will not deform after stretching or washing 100 times, decoherence, durable.
4 rabbet sliding test of embodiment:
By the woven warp knit lace spacer screens of embodiment 1-3 and commercially available lace spacer screen, 10cm × 3.5cm is intercepted, is placed on
On tensiometer rabbet sliding test is done with different pulling force.See below table with conventional test result:
Pulling force kilogram | 0.5kg | 1kg | 1.5kg | 2kg | 2.5kg |
Commercially available lace spacer screen | Start to slide | Skid off 0.3cm | Skid off 0.5 centimetre | ||
Embodiment 1 | It is intact | It is intact | It is intact | Start to slide | Skid off 0.2 centimetre |
Embodiment 2 | It is intact | It is intact | It is intact | It is intact | Sliding |
Embodiment 3 | It is intact | It is intact | Start to slide | Skid off 0.2 centimetre | Skid off 0.4 centimetre |
Normal condition, because fat or thin, movement radian problem, cloth cover stretch the tractive force generated and be in human body wearing process
1.2kg following.The lace spacer screen produced by technical solution of the present invention, resistant slide power are more than commercially available lace spacer screen, can meet big
The demand of wearing of groups of people.
It should be noted that herein, relational terms such as first and second and the like are used merely to a reality
Body or operation are distinguished with another entity or operation, are deposited without necessarily requiring or implying between these entities or operation
In any actual relationship or order or sequence.Moreover, the terms "include", "comprise" or its any other variant are intended to
Non-exclusive inclusion, so that process, method, article or terminal device including a series of elements include not only those
Element, but also include other elements that are not explicitly listed, or further include for this process, method, article or end
The intrinsic element of end equipment.In the absence of more restrictions, being limited by sentence " including ... " or " including ... "
Element, it is not excluded that there is also other elements in process, method, article or the terminal device including the element.This
Outside, herein, " being more than ", " being less than ", " being more than " etc. are interpreted as not including this number;" more than ", " following ", " within " etc. understandings
It includes this number to be.
It should be noted that although the various embodiments described above have been described herein, it is not intended to limit
The scope of patent protection of the present invention.Therefore, based on the present invention innovative idea, to embodiment described herein carry out change and repair
Change or the equivalent structure or equivalent process transformation made by using the contents of the present specification, directly or indirectly by the above technology
Scheme is used in other related technical areas, is included within the scope of patent protection of the present invention.
Claims (5)
1. a kind of method for weaving of warp knit lace, which is characterized in that the weaving of the warp knit lace spacer screen includes the following steps:
Braiding:It is woven using multi-bar warp knitting machine, the multi-bar warp knitting machine includes that ground comb, jacquard comb and spandex are combed, institute
It is spandex covered yarn to comb with stating with the feed yarn of jacquard comb, and the spandex comb and jacquard comb band yarn in the same direction obtain warp knit lace
Spacer screen semi-finished product;
Pre-setting:Warp knit lace spacer screen semi-finished product are put into forming machine and carry out pre-setting, forming machine speed is 25-28 codes/minute,
Temperature is 180-190 DEG C;
Sizing:The warp knit lace spacer screen semi-finished product of pre-setting are carried out shaping with forming machine, forming machine speed is set as 25-28
Code/minute, temperature setting are 160-180 DEG C, obtain warp knit lace spacer screen.
2. method for weaving according to claim 1, which is characterized in that the weaving step of the warp knit lace spacer screen further includes
Oil removing;Machine is washed with water in woven warp knit lace spacer screen semi-finished product and carries out washing oil removing, washing temperature is 99-101 DEG C, speed
For 24-26 codes/minute, washing time 2-5 minutes;The deoiling step is after the braiding step, the pre-setting step
Before.
3. method for weaving according to claim 1, which is characterized in that in weaving step, the twirl of the spandex covered yarn
Degree is that 600-800 is twisted.
4. method for weaving according to claim 1, which is characterized in that in weaving step, the upper machine of the feed yarn
Density be 15-23 rows/centimetre, the density of the warp knit lace spacer screen semi-finished product be 38-45 rows/centimetre.
5. a kind of warp knit lace, which is characterized in that the warp knit lace is weaved by any method for weaving of claim 1-4
It forms.