CN108047846B - Tile surface layer coating for maintenance and preparation method thereof - Google Patents
Tile surface layer coating for maintenance and preparation method thereof Download PDFInfo
- Publication number
- CN108047846B CN108047846B CN201711459088.3A CN201711459088A CN108047846B CN 108047846 B CN108047846 B CN 108047846B CN 201711459088 A CN201711459088 A CN 201711459088A CN 108047846 B CN108047846 B CN 108047846B
- Authority
- CN
- China
- Prior art keywords
- maintenance
- daub
- tile surface
- surface layer
- layer coating
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
The invention discloses a tile surface coating for maintenance, which comprises the following components in parts by weight: 80-90 parts of white base material, 10-20 parts of daub, 0-1 part of pigment and 0-5 parts of brightener. The tile surface layer coating for maintenance disclosed by the invention is simple in formula, good in mixing compatibility among raw materials, good in adhesion, not easy to fall off and fade, capable of repairing slight cracks and making up for the defects of conventional coatings, safe and environment-friendly. The invention also discloses a preparation method of the tile surface layer coating for maintenance, which comprises the following specific steps: adding the brightener into the white base material, stirring uniformly, adding the daub, stirring uniformly until no agglomeration exists, standing for 3-5 min, stirring again for 3-5 min, finally adding the pigment for uniform dispersion, and standing to obtain the tile surface layer coating for maintenance. The daub is dispersed by secondary stirring, so that the dispersion uniformity is better, no caking is caused, and the daub is uniform in dispersion of all raw materials, free of bubbles, not easy to settle and good in construction performance.
Description
Technical Field
The invention relates to a maintenance tile surface layer coating, in particular to a maintenance tile surface layer coating and a preparation method thereof.
Background
The roof (surface) is positioned at the uppermost part of the building, plays roles of protection, obstruction and beauty, and is an indispensable important component in the house building in terms of both material function and artistic effect. The tile roof is a common style of roof, and mainly refers to a green tile roof, a simple tile roof, a flat tile (clay or cement) roof, a slope asbestos cement tile roof and a sheet iron roof. As the name implies, the roofing material (also called roofing material) on a tile roofing is a variety of roofing tiles.
The roof tile is eroded by wind, wind and rain for a long time, so that the colored paint on the roof tile falls off or fades, even the roof tile generates fine cracks to cause water leakage, and therefore, the roof tile needs to be refreshed and recoated by regular maintenance.
However, various coatings used on the existing roof tiles can fall off or fade after being used for a long time, and fine cracks cannot be repaired, so that a novel coating which can effectively solve the problem that the existing tile surface coatings fall off or fade after being used for a long time and can repair the fine cracks is urgently needed to be developed on the basis of the existing tile coatings.
Disclosure of Invention
The invention aims to solve the problems of the tile coating in the prior art, and provides the maintenance tile surface coating which is simple in formula, good in adhesion, not easy to fall off and fade, and capable of repairing slight cracks.
The invention also provides a preparation method of the tile surface layer coating for maintenance, which has the advantages of simple process steps, no special requirements on equipment and strong operability.
In order to achieve the purpose, the invention adopts the following technical scheme:
the invention relates to a maintenance tile surface coating which comprises the following components in parts by weight: 80-90 parts of white base material, 10-20 parts of daub, 0-1 part of pigment and 0-5 parts of brightener. The invention provides a new formula of a tile surface layer coating for maintenance, all raw materials are directly purchased in the market, the formula is simple, the cost is low, the tile surface layer coating can be directly prepared according to construction colors on a construction site (namely, color mixing can be completed on the site), a white base material is a basic coating, and the best white base color can be prepared into various colors; the pigment can be powder or various color pastes, and is selectively added according to actual requirements; the daub can improve the waterproof performance of the invention, can be filled in the slight crack on the tile surface to repair the slight crack, can improve the viscosity of the invention at the same time, can not produce the sagging phenomenon when coating; the brightener is added according to the requirements of tile smooth surfaces or matte surfaces. The invention has simple formula, good mixing compatibility among raw materials, good adhesion, difficult shedding and fading, capability of repairing slight cracks and making up the defects of the conventional coating, safety and environmental protection.
Preferably, the white base material is Nippon QB-659 exterior wall elastic finishing paint. The white base material is Nippon QB-659 external wall elastic finishing paint which has the functions of water resistance, crack resistance, good stain resistance and the like, has good comprehensive use performance and can be directly purchased in the market.
Preferably, the mastic is a tile mastic.
Preferably, the gloss enhancer is an aqueous gloss enhancer. The use of the water-based brightener is more environment-friendly.
A preparation method of a tile surface layer coating for maintenance comprises the following specific steps: adding the brightener into the white base material, stirring uniformly, adding the daub, stirring uniformly until no agglomeration exists, standing for 3-5 min, stirring again for 3-5 min, finally adding the pigment for uniform dispersion, and standing to obtain the tile surface layer coating for maintenance. The daub is dispersed by secondary stirring, so that the dispersion uniformity is better, no caking is caused, and the daub is uniform in dispersion of all raw materials, free of bubbles, not easy to settle and good in construction performance.
Therefore, the invention has the following beneficial effects:
(1) the tile surface layer coating for maintenance is provided, has a simple formula, good mixing compatibility among raw materials, good adhesion, difficult shedding and fading, capability of repairing slight cracks and making up the defects of conventional coatings, safety and environmental protection;
(2) the preparation method of the tile surface layer coating for maintenance is simple in process steps, free of special requirements for equipment, high in operability, uniform in dispersion of raw materials, free of bubbles, not prone to sedimentation and good in construction performance.
Detailed Description
The raw materials in the following examples are commercially available, and therefore, are not described in detail in the examples.
Example 1
Weighing the raw materials according to the mass ratio of 9kg of white base material (Nippon QB-659 external wall elastic finish), 2kg of daub (Lee brother tile daub), 0.1kg of pigment (black powder material) and 0.5kg of brightener (GH-1101, Van Hao trade Co., Ltd., Guangzhou), adding the brightener into the white base material, uniformly stirring, adding the daub, uniformly stirring until no caking exists, standing for 5min, stirring again for 5min, finally adding the pigment, uniformly dispersing, and standing to obtain the tile surface layer coating for the maintenance.
Example 2
Weighing raw materials according to the mass ratio of 8kg of white base material (Nippon QB-659 external wall elastic finish), 1kg of daub (Rayleigh brother tile daub) and 0.2kg of brightener (GH-1101, Guangzhou Sanskohao trade Co., Ltd.), adding the brightener into the white base material, uniformly stirring, adding the daub, uniformly stirring until no caking exists, standing for 3min, stirring again for 3min, finally adding pigment, uniformly dispersing, and standing to obtain the tile surface layer coating for maintenance.
Example 3
Weighing the raw materials according to the mass ratio of 8.5kg of white base material (Nippon QB-659 external wall elastic finish), 1.5kg of daub (Leeb brother tile daub) and 0.05kg of pigment (red color paste), adding the brightener into the white base material, uniformly stirring, adding the daub, uniformly stirring until no agglomeration exists, standing for 4min, stirring again for 4min, finally adding the pigment, uniformly dispersing, and standing to obtain the tile surface coating for maintenance.
The tile surface layer coating for maintenance, disclosed by the invention, is simple in formula, good in mixing compatibility among raw materials, good in adhesion, difficult to fall off and fade, capable of repairing slight cracks and making up for the defects of conventional coatings, safe and environment-friendly.
The above-described embodiments are only preferred embodiments of the present invention, and are not intended to limit the present invention in any way, and other variations and modifications may be made without departing from the spirit of the invention as set forth in the claims.
Claims (2)
1. The tile surface coating for maintenance is characterized by comprising the following components in parts by weight: 80-90 parts of white base material, 10-20 parts of daub, 0-1 part of pigment and 0-5 parts of brightener; the white base material is Nippon QB-659 external wall elastic finish paint; the daub is ceramic tile daub; the brightener is an aqueous brightener.
2. The preparation method of the maintenance tile surface layer coating as claimed in claim 1, which comprises the following specific steps: adding the brightener into the white base material, stirring uniformly, adding the daub, stirring uniformly until no agglomeration exists, standing for 3-5 min, stirring again for 3-5 min, finally adding the pigment for uniform dispersion, and standing to obtain the tile surface layer coating for maintenance.