CN107574397A
CN107574397A CN201710995835.9A CN201710995835A CN107574397A CN 107574397 A CN107574397 A CN 107574397A CN 201710995835 A CN201710995835 A CN 201710995835A CN 107574397 A CN107574397 A CN 107574397A
Authority
CN
China
Prior art keywords
roller
ring flange
connecting bushing
axially extending
extending bore
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Withdrawn
Application number
CN201710995835.9A
Other languages
English (en)
Inventor
沈炳辉
贲启轩
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Jiangsu Asia-Pacific Special Cast Steel Plant Co Ltd
Original Assignee
Jiangsu Asia-Pacific Special Cast Steel Plant Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Jiangsu Asia-Pacific Special Cast Steel Plant Co Ltd filed Critical Jiangsu Asia-Pacific Special Cast Steel Plant Co Ltd
Priority to CN201710995835.9A priority Critical patent/CN107574397A/zh
Publication of CN107574397A publication Critical patent/CN107574397A/zh
Withdrawn legal-status Critical Current

Links

Landscapes

  • Rolls And Other Rotary Bodies (AREA)

Abstract

本发明公开了一种高强度耐腐蚀沉没辊,包括辊筒、辊轴、两个连接轴套;连接轴套为阶梯式结构,大端为法兰盘;辊筒两端的止口孔套装在连接轴套法兰盘上,并固定连接;辊轴为轴向贯穿两个连接轴套内孔的整体式结构,与两个连接轴套固定连接;连接轴套法兰盘上均布若干周向布置、与辊筒内腔连通的轴向通孔;两端连接轴套法兰盘上轴向通孔在辊筒中心轴线的圆周方向上错开布置;进一步改进在于:两端连接轴套法兰盘上轴向通孔在辊筒中心轴线的圆周方向上错开的角度为每个连接轴套法兰盘上相邻轴向通孔夹角的一半;辊筒外壁套装钴基合金辊套。本发明结构强度、刚性高,使用时锌液从辊筒内腔中流通时能形成均匀旋流。

Description

高强度耐腐蚀沉没辊
技术领域
本发明涉及热镀锌技术领域,尤其是一种热镀锌装置上沉没辊。
背景技术
现有热镀锌装置上的沉没辊一般包括辊筒、两个辊轴、两个连接轴套,连接轴套为阶梯式结构,大端为法兰盘,辊筒两端止口孔套装在连接轴套法兰盘上,并固定连接;连接轴套小端套装在辊轴一端,并固定连接,这种沉没辊的主要缺陷在于:一是结构强度、刚性差;二是锌液如何从辊筒内腔中流通时形成旋流。
发明内容
本发明针对现有技术的不足,提供一种能显著提高结构强度、刚性,使用时锌液从辊筒内腔中流通时能形成旋流的高强度耐腐蚀沉没辊。
本发明通过下述技术方案实现技术目标。
高强度耐腐蚀沉没辊,包括辊筒、辊轴、两个连接轴套;所述连接轴套为阶梯式结构,大端为法兰盘;所述辊筒两端的止口孔套装在连接轴套法兰盘上,并固定连接;其改进之处在于:所述辊轴为轴向贯穿两个连接轴套内孔的整体式结构,与两个连接轴套固定连接;所述连接轴套法兰盘上均布若干周向布置、与辊筒内腔连通的轴向通孔;两端连接轴套法兰盘上轴向通孔在辊筒中心轴线的圆周方向上错开布置。
上述结构中,两端连接轴套法兰盘上轴向通孔在辊筒中心轴线的圆周方向上错开的角度为每个连接轴套法兰盘上相邻轴向通孔夹角的一半。
上述结构中,所述辊筒外壁套装钴基合金辊套。
本发明与现有技术相比,具有以下积极效果:
1、辊轴为轴向贯穿两个连接轴套内孔的整体式结构,显著提高本发明强度和刚性。
2、两端连接轴套法兰盘上轴向通孔在辊筒中心轴线的圆周方向上错开布置,使用时锌液从辊筒内腔中流通时能形成旋流。
3、两端连接轴套法兰盘上轴向通孔在辊筒中心轴线的圆周方向上错开的角度为每个连接轴套法兰盘上相邻轴向通孔夹角的一半,使用时锌液从辊筒内腔中流通时能形成均匀旋流。
4、辊筒外壁套装钴基合金辊套,在显著提高耐腐蚀性、耐磨损性的同时,显著提高耐热耐高温性能,减少粘渣,延长本发明使用寿命。
附图说明
图1为本发明结构示意图。
图2为图1的A-A剖面图。
图3为图1的B-B剖面图。
具体实施方式
下面根据附图并结合实施例对本发明作进一步说明。
附图所示的高强度耐腐蚀沉没辊,包括辊筒1、辊轴2、两个连接轴套3;连接轴套3为阶梯式结构,大端为法兰盘;辊筒1两端的止口孔套装在连接轴套3法兰盘上,并固定连接;辊轴2为轴向贯穿两个连接轴套3内孔的整体式结构,与两个连接轴套固定连接;连接轴套3法兰盘上均布若干(本实施例为6个)周向布置、与辊筒1内腔连通的轴向通孔3.1,两端连接轴套3法兰盘上轴向通孔3.1在辊筒中心轴线的圆周方向上错开布置 ,错开的角度为每个连接轴套3法兰盘上相邻轴向通孔3.1夹角的一半(本实施例为30°)。
辊筒1外壁套装钴基合金辊套4。

Claims (3)

1.一种高强度耐腐蚀沉没辊,包括辊筒(1)、辊轴(2)、两个连接轴套(3);所述连接轴套(3)为阶梯式结构,大端为法兰盘;所述辊筒(1)两端的止口孔套装在连接轴套(3)法兰盘上,并固定连接;其特征在于:所述辊轴(2)为轴向贯穿两个连接轴套(3)内孔的整体式结构,与两个连接轴套固定连接;所述连接轴套(3)法兰盘上均布若干周向布置、与辊筒(1)内腔连通的轴向通孔(3.1);两端连接轴套(3)法兰盘上轴向通孔(3.1)在辊筒中心轴线的圆周方向上错开布置。
2.根据权利要求1所述的高强度耐腐蚀沉没辊,其特征在于:两端连接轴套(3)法兰盘上轴向通孔(3.1)在辊筒中心轴线的圆周方向上错开的角度为每个连接轴套(3)法兰盘上相邻轴向通孔(3.1)夹角的一半。
3.根据权利要求2所述的高强度耐腐蚀沉没辊,其特征在于:所述辊筒(1)外壁套装钴基合金辊套(4)。
CN201710995835.9A 2017-10-24 2017-10-24 高强度耐腐蚀沉没辊 Withdrawn CN107574397A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201710995835.9A CN107574397A (zh) 2017-10-24 2017-10-24 高强度耐腐蚀沉没辊

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201710995835.9A CN107574397A (zh) 2017-10-24 2017-10-24 高强度耐腐蚀沉没辊

Publications (1)

Publication Number Publication Date
CN107574397A true CN107574397A (zh) 2018-01-12

Family

ID=61038489

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201710995835.9A Withdrawn CN107574397A (zh) 2017-10-24 2017-10-24 高强度耐腐蚀沉没辊

Country Status (1)

Country Link
CN (1) CN107574397A (zh)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN116638256A (zh) * 2023-07-16 2023-08-25 江苏亚太特种铸钢厂有限公司 一种具有机械安全保护结构的稳定辊加工工艺

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN116638256A (zh) * 2023-07-16 2023-08-25 江苏亚太特种铸钢厂有限公司 一种具有机械安全保护结构的稳定辊加工工艺
CN116638256B (zh) * 2023-07-16 2024-05-10 江苏亚太特种铸钢厂有限公司 一种具有机械安全保护结构的稳定辊加工工艺

Similar Documents

Publication Publication Date Title
CN107604294A (zh) 抗疲劳耐高温沉没辊
CN107574397A (zh) 高强度耐腐蚀沉没辊
CN107630178A (zh) 螺纹连接增强型沉没辊
CN108265255A (zh) 耐高温组合式沉没辊
CN207261483U (zh) 一种船用抗变形轴承座
CN206655919U (zh) 一种球形端面圆柱滚子
CN104196903A (zh) 一种带花键副的十字轴式万向联轴器
CN109910423B (zh) 热涨式铝导辊
CN107587091A (zh) 设有螺旋槽的分体辊轴式沉没辊
CN209272132U (zh) 一种连轧机双金属轧辊
CN205708602U (zh) 一种新型铸钢齿辊
CN107630179A (zh) 抗腐蚀、高耐磨沉没辊
CN108165914A (zh) 设有通流孔的沉没辊
CN107619918A (zh) 耐高温耐磨型炉底辊
CN107420309B (zh) 旋转压缩机用活塞及其制备方法
CN206846186U (zh) 一种能够消除焊接影响的单层耐磨直管
CN107893157A (zh) 高强度耐高温炉底辊
CN107604288A (zh) 焊接式增强型沉没辊
CN203091413U (zh) 加热极片轧辊
CN107604293A (zh) 设有防松结构的焊接式沉没辊
CN209662665U (zh) 一种传动辊及萃取设备
CN108165913A (zh) 加强型焊接式沉没辊
CN214767802U (zh) 一种pqf连轧辊组合结构
CN108193157A (zh) 螺纹连接式耐腐蚀沉没辊
CN207619468U (zh) 一种高强度炉辊

Legal Events

Date Code Title Description
PB01 Publication
PB01 Publication
SE01 Entry into force of request for substantive examination
SE01 Entry into force of request for substantive examination
WW01 Invention patent application withdrawn after publication
WW01 Invention patent application withdrawn after publication

Application publication date: 20180112