CN107520407A - 一种超薄壳精密铸造用减压式组合棒芯 - Google Patents

一种超薄壳精密铸造用减压式组合棒芯 Download PDF

Info

Publication number
CN107520407A
CN107520407A CN201710903217.7A CN201710903217A CN107520407A CN 107520407 A CN107520407 A CN 107520407A CN 201710903217 A CN201710903217 A CN 201710903217A CN 107520407 A CN107520407 A CN 107520407A
Authority
CN
China
Prior art keywords
core
sleeve
shell
wax
ultra
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201710903217.7A
Other languages
English (en)
Other versions
CN107520407B (zh
Inventor
马波
李霞
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
DONGFENG INVESTMENT CASTING Co Ltd
Original Assignee
DONGFENG INVESTMENT CASTING Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by DONGFENG INVESTMENT CASTING Co Ltd filed Critical DONGFENG INVESTMENT CASTING Co Ltd
Priority to CN201710903217.7A priority Critical patent/CN107520407B/zh
Publication of CN107520407A publication Critical patent/CN107520407A/zh
Application granted granted Critical
Publication of CN107520407B publication Critical patent/CN107520407B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

一种超薄壳精密铸造用减压式组合棒芯,棒芯由套筒和套芯构成,套筒的工作端周面上均布有多个减压孔,套芯的工作端插入至套筒的工作端内,套芯外周面与套筒内周面之间设有间隙。在脱蜡过程中,蜡模受热膨胀至慢慢融化,因型壳阻碍,蜡料/蜡膏会通过减压孔流入套筒内,继而减小蜡模的膨胀压力对型壳的冲击,均布的减压孔能使型壳受力均匀,有效地避免了型壳破裂的问题。

Description

一种超薄壳精密铸造用减压式组合棒芯
技术领域
本发明涉及薄壳精密铸造领域,尤其是一种超薄壳精密铸造用减压式组合棒芯。
背景技术
熔模精密铸造常见两种工艺:水玻璃型壳工艺和硅溶胶型壳工艺。两种工艺的特点是:1.水玻璃型壳工艺成本低、周期短,但有环保风险;2.硅溶胶型壳工艺成本高、周期长,但产品质量好,环境风险小。东风精密铸造有限公司为解决硅溶胶型壳工艺存在制壳周期长、成本高的问题,研究应用了超薄壳硅溶胶型壳工艺,型壳厚度由原来的10-12毫米,减少到6-8毫米,同时解决了成本问题、周期问题、环保问题。不管是传统型壳,还是超薄型壳,虽然焙烧后的高温强度很高,但湿强度却不高。尤其是转运、脱蜡过程中,受物理碰撞、蜡模膨胀挤压容易产生型壳破裂,轻则铸件表面出现沟纹,重则浇注破裂跑火。
发明内容
本发明提供一种超薄壳精密铸造用减压式组合棒芯,解决了脱蜡过程中蜡模因受热膨胀而对型壳产生挤压力、避免了型壳破裂的问题。
为了解决上述技术问题,本发明的技术方案是:一种超薄壳精密铸造用减压式组合棒芯,其特征在于:棒芯由套筒和套芯构成,套筒的工作端周面上均布有多个减压孔,套芯的工作端插入至套筒的工作端内,套芯外周面与套筒内周面之间设有间隙。
对上述技术方案进一步地限定,所述棒芯上的减压孔直径为:4-5毫米。
对上述技术方案进一步地限定,所述套芯与套筒之间的间隙为0.4-0.6毫米。
有益效果:在脱蜡过程中,蜡模受热膨胀至慢慢融化,因型壳阻碍,蜡料/蜡膏会通过减压孔流入套筒内,继而减小蜡模的膨胀压力对型壳的冲击,均布的减压孔能使型壳受力均匀,有效地避免了型壳破裂的问题。
附图说明
图1是本发明的结构示意图。
图2是本发明中的套筒结构示意图。
图3是本发明中的套芯结构示意图。
图4是本发明使用状态图。
图5是图4的左视图。
具体实施方式
最佳实施例1:如图1所示,一种超薄壳精密铸造用减压式组合棒芯,棒芯由套筒1和套芯2构成,套筒的工作端周面上均布有多个减压孔3,每个减压孔的直径为4.5毫米,套芯的工作端插入至套筒的工作端内,套芯外周面与套筒内周面之间设有0.5毫米的间隙。采用4.5毫米的减压孔和0.5毫米的间隙,具有以下效果:1.在压蜡时蜡膏不易进入套筒内;2.减压效果能达到最佳状态;3. 制棒后套芯易取出。
实施例2:如图1所示,一种超薄壳精密铸造用减压式组合棒芯,棒芯由套筒和套芯构成,套筒的工作端周面上均布有多个减压孔,每个减压孔的直径为4毫米,套芯的工作端插入至套筒的工作端内,套芯外周面与套筒内周面之间设有0.4毫米的间隙。
实施例3:如图1所示,一种超薄壳精密铸造用减压式组合棒芯,棒芯由套筒和套芯构成,套筒的工作端周面上均布有多个减压孔,每个减压孔的直径为5毫米,套芯的工作端插入至套筒的工作端内,套芯外周面与套筒内周面之间设有0.6毫米的间隙。
如图2所示,所述套筒1由第一筒体101、第二筒体102、盖板103及固定杆104构成,第一筒体的左端为筒口端、第一筒体的右端为封闭端、第一筒体的周面上分布有多个减压孔3,第二筒体的左右两端贯通,第一筒体通过环形盖板与第二筒体焊接为一体式结构,第一筒体和第二筒体的筒腔相通,以盖板为界,第一筒体的长度大于第二筒体的长度,固定杆呈对称状固定在第二筒体上、连接方式为焊接。盖板嵌入蜡棒中,可以防止蜡棒脱落;固定杆用于悬挂模组。
如图3所示,所述套芯2由芯杆201和手柄202构成,手柄的中部与芯杆的左端固定连接,连接方式为焊接。
棒芯制作说明:L1定义为套筒长度;L2定义为套芯长度,L2=L1+10,方便工人抽取;ф1定义为减压孔直径值;ф2定义为套筒内径值,ф2=4×ф1;ф3定义为套杆直径值,ф3=ф2减去套芯与套筒之间的间隙值,保证压蜡时不漏蜡,也方便抽插套芯。
使用方法:如图4和5所示,在制蜡棒过程中,先将套筒放置在棒模模具4型腔内的相应位置处,再将套芯中的芯杆从套筒筒口处插入至套筒内,合模后射蜡,射蜡时保证套筒和套芯呈竖直状,经过保压、冷却后取出蜡棒,握手套芯中的手柄抽出芯杆。蜡棒经正常组树、制壳工序后进入脱蜡环节,脱蜡过程中,蜡模受热膨胀至慢慢融化,因型壳阻碍,蜡料/蜡膏会向空隙方向渗出,继而减小膨胀压力对型壳的冲击。
效益说明:1、本发明可减少模壳脱蜡破损:破损比例(5%)×产量(吨)×制壳成本(2500元/吨),年效益约125万元(比照2016年产量10000吨);2、本发明保障了薄壳技术顺利推广应用:薄壳项目效益(220元/吨)×产量(吨)=220万元(非直接效益);预计三年期效益:125×3=375万元。

Claims (3)

1.一种超薄壳精密铸造用减压式组合棒芯,其特征在于:棒芯由套筒和套芯构成,套筒的工作端周面上均布有多个减压孔,套芯的工作端插入至套筒的工作端内,套芯外周面与套筒内周面之间设有间隙。
2.根据权利要求1所述一种超薄壳精密铸造用减压式组合棒芯,其特征在于:所述棒芯上的减压孔直径为4-5毫米。
3.根据权利要求1或2所述一种超薄壳精密铸造用减压式组合棒芯,其特征在于:所述套芯与套筒之间的间隙为0.4-0.6毫米。
CN201710903217.7A 2017-09-29 2017-09-29 一种超薄壳精密铸造用减压式组合棒芯 Active CN107520407B (zh)