CN1075158A - 水解氢离子固体燃料及工艺流程 - Google Patents

水解氢离子固体燃料及工艺流程 Download PDF

Info

Publication number
CN1075158A
CN1075158A CN 93110590 CN93110590A CN1075158A CN 1075158 A CN1075158 A CN 1075158A CN 93110590 CN93110590 CN 93110590 CN 93110590 A CN93110590 A CN 93110590A CN 1075158 A CN1075158 A CN 1075158A
Authority
CN
China
Prior art keywords
mix
methyl alcohol
ethanol
solid fuel
hydrogen ion
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 93110590
Other languages
English (en)
Inventor
傅汝杰
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN 93110590 priority Critical patent/CN1075158A/zh
Publication of CN1075158A publication Critical patent/CN1075158A/zh
Pending legal-status Critical Current

Abstract

本发明提出的是一种水解氢离子固体燃料及生 产工艺流程。它的成分配比(生产1kg燃料计):甲 醇0.6—0.70464,水0.2147—0.31934,乙醇0.03543, 硬脂酸0.02349,氢氧化钠0.00744丙烯酸(或硝酸) 0.018,硫酸铜0.0006(上述单位kg)。生产工艺:配 制变性剂(丙烯酸、硫酸铜混合),将其与甲醇混合成 混合甲醇,先用50%乙醇与硬脂酸混合搅拌加温,再 用50%乙醇与氢氧化钠混合搅拌加温,然后与混合 甲醇混合,冷却成型。测试证明其效果达4000— 6000大卡,燃烧时温度可达700℃左右,材料成本在 1.5元/1kg。

Description

本发明提出的是一种水解氢离子固体燃料及其生产工艺。属化合物固体燃料技术领域。
现有技术如一种化合物固体燃料。它由三部分物质混合而成,(1)工业乙醇和液碱、(2)硬脂酸、(3)水和工业乙醇。前二者的配比1∶1∶1,第三部分水与工业乙醇配比26∶17。其制造方法是三个部分分别装在三个反应罐中,然后将三个罐中的物质在50-75℃温度下混合,然后入容器冷却。其主要缺陷是效果不够理想,生产成本不够低。
本发明的目的在于针对上述存在的问题,提出一种水解氢离子固体燃料,它可使效果达到4000-6000大卡,燃烧时温度达700℃左右,成本低,材料成本只有1.5元/1Kg。
本发明的技术解决方案:它的成份配比是(以生产1Kg燃料甲醇0.6-0.70464,水0.2147-0.31934,催化剂0.06636,其催化剂是由乙醇:0.03543和硬脂酸:0.02349和氢氧化钠:0.00744组成,变性剂0.0186,其变性剂是由丙烯酸(或硝酸):0.018和硫酸铜:0.0006组成,(上述单位为Kg)。水解氢离子固体燃料的生产工艺流程是,(1)按上述成份比例备好,(2)变性剂中的丙烯酸(或硝酸)、硫酸铜分别倒入甲醇中静置24-48小时,然后加水,加温至74-76℃成混合甲醇,(3)取50%的乙醇与硬脂酸混合加温至76-78℃搅拌,(4)取50%的乙醇和氢氧化钠加温至76-78℃,(5)将上述的(3)、(4)混合,然后倒入(2)已配制的混合甲醇中搅拌3-5分钟,(6)自然降温至65℃左右时,流放入成型模具中冷凝成固体型。
经测试:固体燃料燃烧效果在4000-6000大卡,燃烧时的温度可达700℃左右,成本低,其中材料成本在1.5元/1Kg。

Claims (2)

1、水解氢离子固体燃料,其特征是它的成份配比是(以生产1Kg燃料计),甲醇0.6-0.70464,水0.2147-0.31934,催化剂0.06636,其催化剂是由乙醇:0.03543和硬脂酸:0.02349和氢氧化钠:0.00744组成,变性剂0.0186,其变性剂是由丙烯酸(或硝酸):0.018和硫酸铜:0.0006组成,(上述单位为Kg)。
2、水解氢离子固体燃料的生产工艺流程:其特征是,(1)按上述成份比例备好,(2)变性剂中的丙烯酸(或硝酸)、硫酸铜分别倒入甲醇中静置24-48小时,然后加水,加温至74-76℃成混合甲醇,(3)取50%的乙醇与硬脂酸混合加温至76-78℃搅拌,(4)取50%的乙醇和氢氧化钠加温至76-78℃,(5)将上述的(3)、(4)混合,然后倒入(2)已配制的混合甲醇中搅拌3-5分钟,(6)自然降温至65℃左右时,流放入成型模具中冷凝成固体型。
CN 93110590 1993-03-03 1993-03-03 水解氢离子固体燃料及工艺流程 Pending CN1075158A (zh)