CN107461008A - 一种屋面防水施工工艺 - Google Patents
一种屋面防水施工工艺 Download PDFInfo
- Publication number
- CN107461008A CN107461008A CN201610381393.4A CN201610381393A CN107461008A CN 107461008 A CN107461008 A CN 107461008A CN 201610381393 A CN201610381393 A CN 201610381393A CN 107461008 A CN107461008 A CN 107461008A
- Authority
- CN
- China
- Prior art keywords
- construction
- roofing
- glass fiber
- mentioned steps
- techniques
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种屋面防水施工工艺,施工工艺包括如下步骤:①清除屋面;②对屋面表层进行修补和平整;③在上述步骤的屋面表层滚涂基丙稀酸乙酯胶后,平铺一层玻纤网格布;④将改性碳酸钙粉、聚氨酯防水涂料和丙酮稀释调配均匀后,用塑料刮板平行涂刮在玻纤网格布表面;⑤再按上述步骤对涂层表面进行第二遍垂直涂刮;⑥待第二遍涂刮层固化后,再用有机硅抗老化剂对其表面进行喷洒,干燥,即可。采用该工艺的施工层和屋面不存在施工气泡,粘结更为牢固;该施工层热胀冷缩率小,不易起鼓、不易翘皮。
Description
技术领域
本发明涉及建筑防水工程领域,特别涉及一种屋面防水施
工工艺。
背景技术
建筑物屋面渗透问题是建筑物较为普遍的质量通病,也是用户反映最为强烈的问题。许多住户在使用后经常会出现屋面渗水、漏水、内墙面粉刷层大面积剥落等现象,时间一长渗漏潮湿的墙面还会发生霉变,直接影响住户的身体健康,而办公室、机房、车间等工作场所如长期渗漏更会严重损坏办公设施、精密仪器、机床设备等,甚至引起电器设备的短路,由此可见良好的防水工程在建筑工程中占有十分重要的地位。
目前我国建筑物屋面防水处理方法,已从七八十年代的油毡纸、焦油沥青铺设法逐步向改性沥青防水卷材、三元乙丙高分子防水卷材铺设法进行转变,但仍存在下列问题:1、耐高低温性能差,遇高温沥青容易融化,遇低温沥青则容易开裂;2、易起鼓、易翘皮,油毡纸以及防水卷材吸热高,尤其是在夏季高温和强紫外线照射后,易出现热胀冷缩现象,导致翘皮和起鼓;3、易老化、易燃;4、施工复杂、施工周期长。
发明内容
本发明的目的是针对现有技术的不足,提供一种屋面防水
施工工艺。
为实现上述目的,本发明提供一种屋面防水施工工艺,施工工艺包括如下步骤:
① 清除屋面表层的浮尘、杂物以及明水;
② 对屋面表层的裂缝、凹凸部分用水灰进行修补和平整;
③ 在上述步骤的屋面表层滚涂基丙稀酸乙酯胶后,平铺一层玻纤网格布;
④ 将改性碳酸钙粉、聚氨酯防水涂料和丙酮稀释调配均匀后,用塑料刮板平行涂刮在玻纤网格布表面;
⑤ 待上述步骤的涂层固化后,再按上述步骤对涂层表面进行第二遍垂直涂刮,涂刮厚度均匀一致;
⑥待第二遍涂刮层固化后,再用有机硅抗老化剂对其表面进行喷洒,干燥,即可。
进一步,所述步骤③中,平铺一层玻纤网格布后,用压辊对粘结面进行往返滚压3次。
进一步,所述步骤④中,改性碳酸钙粉、聚氨酯防水涂料和丙酮的重量比为:(20~40):(60~70):(10~15) 。
本发明相对现有技术具有突出的优点和积极效果,具体地说,采用该工艺的施工层和屋面不存在施工气泡,粘结更为牢固;该施工层热胀冷缩率小,不易起鼓、不易翘皮;该施工层抗老化、阻燃、使用年限长;该施工工艺简单科学、施工周期短。
具体实施方式
下面通过具体实施方式,对本发明的技术方案做进一步的详细描述。
一种屋面防水施工工艺,施工工艺包括如下具体步骤:
① 清除屋面表层的浮尘、杂物以及明水;
② 对屋面表层的裂缝、凹凸部分用水灰进行修补和平整;
③ 在上述步骤的屋面表层滚涂基丙稀酸乙酯胶后,平铺一层玻纤网格布后,用压辊对粘结面进行往返滚压3次,以排出粘结层内多余的空气;
④ 将改性碳酸钙粉、聚氨酯防水涂料和丙酮稀释调配均匀后,用塑料刮板平行涂刮在玻纤网格布表面,所述改性碳酸钙粉、聚氨酯防水涂料和丙酮的重量比为:25:64:11 ;
⑤ 待上述步骤的涂层固化后,再按上述步骤对涂层表面进行第二遍垂直涂刮,涂刮厚度均匀一致;
⑥待第二遍涂刮层固化后,再用有机硅抗老化剂对其表面进行喷洒,干燥,即可。
Claims (3)
1.一种屋面防水施工工艺,其特征在于,该施工工艺包括如下步骤:
① 清除屋面表层的浮尘、杂物以及明水;
② 对屋面表层的裂缝、凹凸部分用水灰进行修补和平整;
③ 在上述步骤的屋面表层滚涂基丙稀酸乙酯胶后,平铺一层玻纤网格布;
④ 将改性碳酸钙粉、聚氨酯防水涂料和丙酮稀释调配均匀后,用塑料刮板平行涂刮在玻纤网格布表面;
⑤ 待上述步骤的涂层固化后,再按上述步骤对涂层表面进行第二遍垂直涂刮,涂刮厚度均匀一致;
⑥待第二遍涂刮层固化后,再用有机硅抗老化剂对其表面进行喷洒,干燥,即可。
2.根据权利要求1所述的一种屋面防水施工工艺,其特征在于:所述步骤③中,平铺一层玻纤网格布后,用压辊对粘结面进行往返滚压3次。
3.根据权利要求1所述的一种屋面防水施工工艺,其特征在于:所述步骤④中,改性碳酸钙粉、聚氨酯防水涂料和丙酮的重量比为:(20~40):(60~70):(10~15) 。