CN105155784A - 一种屋面防水涂料的施工方法 - Google Patents

一种屋面防水涂料的施工方法 Download PDF

Info

Publication number
CN105155784A
CN105155784A CN201510709218.9A CN201510709218A CN105155784A CN 105155784 A CN105155784 A CN 105155784A CN 201510709218 A CN201510709218 A CN 201510709218A CN 105155784 A CN105155784 A CN 105155784A
Authority
CN
China
Prior art keywords
construction method
roof
waterproof
roofing
waterproofing course
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201510709218.9A
Other languages
English (en)
Inventor
吴佩金
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SUZHOU AOLAIXIN BUILDING MATERIAL Co Ltd
Original Assignee
SUZHOU AOLAIXIN BUILDING MATERIAL Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SUZHOU AOLAIXIN BUILDING MATERIAL Co Ltd filed Critical SUZHOU AOLAIXIN BUILDING MATERIAL Co Ltd
Priority to CN201510709218.9A priority Critical patent/CN105155784A/zh
Publication of CN105155784A publication Critical patent/CN105155784A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种屋面防水涂料的施工方法,包括以下步骤:a、使用扫帚打扫干净屋面上的灰尘,用铲刀削平残留的砂浆块或突起物;b、将硅石灰粉、沥青、异氰酸酯、增稠剂、消泡剂以及银浆粉按照质量百分比配置防水涂料;c、将上述配置好的防水涂料铺在屋面上,并用压辊进行压平形成防水层;d、在防水层的表面包覆一层塑料膜,0.5-1.5天后至防水层干燥后撕去塑料膜,形成屋面防水层。本发明提供的屋面防水涂料的施工方法,常温下即可施工,操作简便,用于屋面工程可以起到很好的防水效果,能克服基层开裂带来的渗漏。

Description

一种屋面防水涂料的施工方法
技术领域
本发明涉及工程建设的领域,特别是涉及一种屋面防水涂料的施工方法。
背景技术
涂料又称油漆。指涂布于物体表面在一定的条件下能形成薄膜而起保护、装潢或其他特殊功能(绝缘、防锈、防霉、耐热等)的一类液体或固体材料。因早期的涂料大多以植物油为主要原料,故又称作油漆。现在合成树脂已大部分或全部取代了植物油,故称为涂料。
建筑防水涂料是在常温下呈无固定形状的粘稠液态高分子合成材料。经涂布后,通过溶剂的挥发或水分的蒸发或反应固化后在基层面上形成坚韧的防水膜的材料的总称。
目前,国内广泛使用的涂料种类繁多,而用于建筑物表面,如屋顶、外墙等仍然使用三油二毡防水材料,施工时费时费工,而且使用范围受到了很大的局限。特别是这种方法五反光降温性能,每到夏天由于三油二毡得吸热作用,使得顶楼或者冷库、粮库的温度升高,要保持温度适宜,耗能较大。
发明内容
本发明主要解决的技术问题是提供一种屋面防水涂料的施工方法,常温下即可施工,操作简便,用于屋面工程可以起到很好的防水效果,能克服基层开裂带来的渗漏。
为解决上述技术问题,本发明采用的一个技术方案是:提供了一种屋面防水涂料的施工方法,包括以下步骤:
a、使用扫帚打扫干净屋面上的灰尘,用铲刀削平残留的砂浆块或突起物;
b、将硅石灰粉、沥青、异氰酸酯、增稠剂、消泡剂以及银浆粉按照质量百分比配置防水涂料;
c、将上述配置好的防水涂料铺在屋面上,并用压辊进行压平形成防水层;
d、在防水层的表面包覆一层塑料膜,0.5-1.5天后至防水层干燥后撕去塑料膜,形成屋面防水层。
在本发明一个较佳实施例中,所述的步骤b中的原料以及质量百分比为:
硅石灰粉30-60%;
沥青15-25%;
异氰酸酯10-15%;
增稠剂8-16%;
消泡剂2-4%;
银浆粉5-10%。
在本发明一个较佳实施例中,所述的防水层的厚度为10-30mm。
在本发明一个较佳实施例中,所述的塑料膜的厚度为1-2mm。
本发明的有益效果是:本发明的屋面防水涂料的施工方法,常温下即可施工,操作简便,用于屋面工程可以起到很好的防水效果,能克服基层开裂带来的渗漏。
附图说明
为了更清楚地说明本发明实施例中的技术方案,下面将对实施例描述中所需要使用的附图作简单地介绍,显而易见地,下面描述中的附图仅仅是本发明的一些实施例,对于本领域普通技术人员来讲,在不付出创造性劳动的前提下,还可以根据这些附图获得其它的附图,其中:
图1是本发明的屋面防水涂料的施工方法一较佳实施例的流程图。
具体实施方式
下面将对本发明实施例中的技术方案进行清楚、完整地描述,显然,所描述的实施例仅是本发明的一部分实施例,而不是全部的实施例。基于本发明中的实施例,本领域普通技术人员在没有做出创造性劳动前提下所获得的所有其它实施例,都属于本发明保护的范围。
如图1所示,本发明实施例包括:
一种屋面防水涂料的施工方法,包括以下步骤:
a、使用扫帚打扫干净屋面上的灰尘,用铲刀削平残留的砂浆块或突起物;
b、将硅石灰粉、沥青、异氰酸酯、增稠剂、消泡剂以及银浆粉按照质量百分比配置防水涂料;
c、将上述配置好的防水涂料铺在屋面上,并用压辊进行压平形成防水层;
d、在防水层的表面包覆一层塑料膜,0.5-1.5天后至防水层干燥后撕去塑料膜,形成屋面防水层。
上述中,所述的步骤b中的原料以及质量百分比为:
硅石灰粉30-60%;
沥青15-25%;
异氰酸酯10-15%;
增稠剂8-16%
消泡剂2-4%;
银浆粉5-10%。
进一步的,所述的防水层的厚度为10-30mm,达到了很好的防水效果;所述的塑料膜的厚度为1-2mm,方便风干防水层,同时又阻挡的灰尘粘结在防水层上面。
本发明揭示的屋面防水涂料的施工方法,常温下即可施工,操作简便,用于屋面工程可以起到很好的防水效果,能克服基层开裂带来的渗漏。
以上所述仅为本发明的实施例,并非因此限制本发明的专利范围,凡是利用本发明说明书内容所作的等效结构或等效流程变换,或直接或间接运用在其它相关的技术领域,均同理包括在本发明的专利保护范围内。

Claims (4)

1.一种屋面防水涂料的施工方法,其特征在于,包括以下步骤:
a、使用扫帚打扫干净屋面上的灰尘,用铲刀削平残留的砂浆块或突起物;
b、将硅石灰粉、沥青、异氰酸酯、增稠剂、消泡剂以及银浆粉按照质量百分比配置防水涂料;
c、将上述配置好的防水涂料铺在屋面上,并用压辊进行压平形成防水层;
d、在防水层的表面包覆一层塑料膜,0.5-1.5天后至防水层干燥后撕去塑料膜,形成屋面防水层。
2.根据权利要求1所述的屋面防水涂料的施工方法,其特征在于,所述的步骤b中的原料以及质量百分比为:
硅石灰粉30-60%;
沥青15-25%;
异氰酸酯10-15%;
增稠剂8-16%
消泡剂2-4%;
银浆粉5-10%。
3.根据权利要求1所述的屋面防水涂料的施工方法,其特征在于,所述的防水层的厚度为10-30mm。
4.根据权利要求1所述的屋面防水涂料的施工方法,其特征在于,所述的塑料膜的厚度为1-2mm。
CN201510709218.9A 2015-10-28 2015-10-28 一种屋面防水涂料的施工方法 Pending CN105155784A (zh)