CN105983593A - 一种重卷机组钢卷头尾搭接分卷方法 - Google Patents
一种重卷机组钢卷头尾搭接分卷方法 Download PDFInfo
- Publication number
- CN105983593A CN105983593A CN201510087556.3A CN201510087556A CN105983593A CN 105983593 A CN105983593 A CN 105983593A CN 201510087556 A CN201510087556 A CN 201510087556A CN 105983593 A CN105983593 A CN 105983593A
- Authority
- CN
- China
- Prior art keywords
- coil
- previous
- volume
- steel
- tail
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
本发明提供一种重卷机组钢卷头尾搭接分卷方法,按正常操作标准将前一卷钢卷带尾卷入卷取机,助卷器皮带保持抱紧状态;当卷取机停止转动时,将前一卷钢卷带尾置于钟表表盘12点到2点得位置上;将后一卷钢卷的带头插入到前一卷钢卷的带尾与卷体之间,助卷器皮带保持抱紧状态,并开始运转;当后一卷钢卷的带头缺陷部分全部卷入前一卷钢卷内以后,机组进行剪切分卷、卸卷。本发明不仅可减少一道卸卷操作过程,缩短分卷时间,提高重卷机组作业率;而且可减少钢卷头尾切除量,降低剪切损失1/3,从而极大提高冷轧板的成材率,增加企业经济效益。
Description
技术领域
本发明属于轧钢工艺技术领域,尤其涉及一种冷轧重卷机组钢卷头尾搭接分卷方法。
背景技术
重卷机组是冷轧生产线重要的一道工序,其主要功能包括剪边、涂油、质量检查和分卷。对于每一卷钢卷来说,头尾会或多或少地存在一些比较严重的缺陷,这些缺陷在重卷机组需要全部切除,为此,严格控制切除量是重卷机组的一个重要任务。
由于在重卷机组生产过程中,需要将钢卷头尾有缺陷的部分切除。目前,国内冷轧厂大多采用每个钢卷带头与带尾单独分卷的方法,由于考虑散卷,因此带头和带尾分别至少需要卷8圈,带头加上带尾共卷有30米,不仅降低了机组作业率,而且增加了头尾切除量,直接降低了成材率。
发明内容
本发明提供一种重卷机组钢卷头尾搭接分卷方法,其目的旨在减少一道卸卷操作过程,并减少钢卷头尾切除量,提高成材率和机组作业率。
为此,本发明所采取的解决方案是:
一种重卷机组钢卷头尾搭接分卷方法,其特征在于,前一卷钢卷的带尾下蛋卷(即按照产品标准,将钢卷头尾带有缺陷部分切除,切除后把带有缺陷的带钢通过卷取机卷成一个小卷,现场称之为下蛋卷)卷取完成后不卸卷,后一卷钢卷的带头继续卷在前一卷钢卷上,其具体方法和步骤为:
(1)按正常操作标准将前一卷钢卷带尾卷入卷取机,助卷器皮带保持抱紧状态;
(2)当卷取机停止转动时,将前一卷钢卷带尾置于钟表表盘12点到2点得位置上;
(3)将后一卷钢卷的带头插入到前一卷钢卷的带尾与卷体之间,助卷器皮带保持抱紧状态,并开始运转;
(4)当后一卷钢卷的带头缺陷部分全部卷入前一卷钢卷内以后,机组进行剪切分卷、卸卷。
本发明的有益效果为:
由于本发明采取钢卷头尾搭接的分卷方法,不仅可减少一道卸卷操作过程,缩短分卷时间,提高重卷机组作业率;而且可减少钢卷头尾切除量,使带头和带尾的切除量由30米减少至20米,降低剪切损失1/3,从而极大提高冷轧板的成材率,增加企业经济效益。
具体实施方式
本发明重卷机组钢卷头尾搭接分卷方法,主要是采取前一卷钢卷的带尾下蛋卷卷取完成后不卸卷,后一卷钢卷的带头继续卷在前一卷钢卷上。其具体方法和步骤为:
1、按正常操作标准将前一卷钢卷带尾卷入卷取机,助卷器皮带保持抱紧状态。
2、当卷取机停止转动时,将前一卷钢卷带尾置于钟表表盘12点到2点得位置上。
3、将后一卷钢卷的带头插入到前一卷钢卷的带尾与卷体之间,助卷器皮带保持抱紧状态,并开始运转。
4、当后一卷钢卷的带头缺陷部分全部卷入前一卷钢卷内以后,机组再进行剪切分卷和卸卷,从而减少了一道卸卷操作过程。
Claims (1)
1.一种重卷机组钢卷头尾搭接分卷方法,其特征在于,前一卷钢卷的带尾下蛋卷卷取完成后不卸卷,后一卷钢卷的带头继续卷在前一卷钢卷上,其具体方法和步骤为:
(1)按正常操作标准将前一卷钢卷带尾卷入卷取机,助卷器皮带保持抱紧状态;
(2)当卷取机停止转动时,将前一卷钢卷带尾置于钟表表盘12点到2点得位置上;
(3)将后一卷钢卷的带头插入到前一卷钢卷的带尾与卷体之间,助卷器皮带保持抱紧状态,并开始运转;
(4)当后一卷钢卷的带头缺陷部分全部卷入前一卷钢卷内以后,机组进行剪切分卷、卸卷。